Polymer Property : Middle Barrel Temperature = 464 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Middle Barrel Temperature 230 - 240 °C
446 - 464 °F
NHEP Spectron™ E6046 Nylon 6, 15% Glass Fiber
Natural color. E6046 exhibits high rigidity and mechanical strength. It is suitable for wide range of applications. Property data measured at room temperature, 50% RH.Information provided by Bieglo..
Middle Barrel Temperature 210 - 240 °C
410 - 464 °F
Start Point: 225°C
Kingfa HR-528 Modified ABS
Features:UL94 HB @ 1.5-3.2mmExcellent heat resistanceApplications:Automobile partsAutomobile audioDashboard, interior trimAutomobile lamp, mirrorInformation Provided by Kingfa Sci. & Tech. Co., Ltd...
Middle Barrel Temperature 220 - 240 °C
428 - 464 °F
Start Point: 235°C
Kingfa MAC-601 DY Modified 60/40 PC/ABS Alloy
Features:Excellent balance propertiesHigh impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile instrument panelPower toolComputer and acce..
Middle Barrel Temperature 220 - 240 °C
428 - 464 °F
Injection Molding
LG Chemical KEYFLEX BT 2140D Ester Type TPE
Description: Injection Molding, TPC-ET, Specialty, Low ModulusApplication: Films & SheetsCAS: 37282-12-5Information provided by LG Chemical
Middle Barrel Temperature 220 - 240 °C
428 - 464 °F
LG Chemical LUMAX HF-5006F High Flow PBT, Weather Resistant, Flame Retardant
LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r..
Middle Barrel Temperature 220 - 240 °C
428 - 464 °F
LG Chemical LUMAX HF-5008 High Flow PBT, Dimensional Stability
LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r..
Middle Barrel Temperature 220 - 240 °C
428 - 464 °F
Injection Molding
LG Chemical LUPOS HR2207A ABS+GF20%, General Purpose, Heat Resistance
Feature: Injection Molding, ABS+GF20%, General Purpose, Heat ResistanceApplication: Electric & Electronic (Housing, Components)Information provided by LG Chemical
Middle Barrel Temperature 230 - 240 °C
446 - 464 °F
LG Chemical Lupox® SV-1120 General Purpose PBT, Unreinforced, High Molecular Weight, Extrusion
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
Middle Barrel Temperature 190 - 240 °C
374 - 464 °F
Injection
Inno-Comp INNOPOL® CS 2-2523 EP 16% Talc Filled, Elastomer Modified Polypropylene Copolymer
INNOPOL® CS 2-2523 EP is a 16% talc-filled, elastomer modified compound based on polypropylene block-copolymer. This grade is available in natural and custom colored form.INNOPOL® CS 2-2523 EP..
Middle Barrel Temperature 190 - 240 °C
374 - 464 °F
Injection
Inno-Comp INNOPOL® CS 2-3840 MO 40% Glass Filled Polypropylene Copolymer
INNOPOL® CS 2-3840 MO is a 40 % glass-fiber-filled polypropylene block-copolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 2-3840 MO is recommended for p..
Middle Barrel Temperature 220 - 240 °C
428 - 464 °F
Injection Molding
LG Chemical XR474 ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior HousingCAS No. 25120-20-1, 9003-56-9, 31621-07-5, and 9003-54-7Information provided by LG Chemical
Middle Barrel Temperature 220 - 240 °C
428 - 464 °F
Injection Molding
LG Chemical XR474F ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Automotives Exterior Housing (Lamp Housing Etc)CAS No. 25120-20-1, 9003-56-9, 31621-07-5, and 9003-54-7Information provided by LG Chemical
Middle Barrel Temperature 220 - 240 °C
428 - 464 °F
Injection Molding
LG Chemical XR490 ABS, Heat Resistance, Low Emission
Feature: Injection Molding, Heat Resistance, Low EmissionApplication: Automotives Interior Housing (Glove Box Etc)CAS No. 25120-20-1, 9003-56-9, 31621-07-5, and 9003-54-7Information provided by LG C..
Middle Barrel Temperature 220 - 240 °C
428 - 464 °F
Injection Molding
LG Chemical LUPOS GP2200 ABS+GF20%, General Purpose
Feature: Injection Molding, ABS+GF20%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7 and 65997-17-3Information provided by LG Chemical
Middle Barrel Temperature 220 - 240 °C
428 - 464 °F
Injection Molding
LG Chemical XR407D ABS
Feature: Electric & Electronic HousingApplication: Electric & Electronic HousingCAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Chemical
Middle Barrel Temperature 230 - 240 °C
446 - 464 °F
Solvay Technyl® C 216 Nylon 6, 30% Glass Fiber, EH50
Polyamide PA6, reinforced with 30% of glass fiber, for injection molding.It has good mechanical properties. It is used in all sectors of industry, offering an excellent combination between thermal ..
Middle Barrel Temperature 220 - 240 °C
428 - 464 °F
Samsung Cheil Industries Starex® SR-0300 Heat Resistant Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 220 - 240 °C
428 - 464 °F
Samsung Cheil Industries Starex® SR-0310 Heat Resistant Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 220 - 240 °C
428 - 464 °F
Samyang Tribit® 1503 Polybutylene Terephthalate
Characteristics:High flow & processabilityApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll information provid..
Middle Barrel Temperature 220 - 240 °C
428 - 464 °F
Samyang Tribit® 1503S Polybutylene Terephthalate
Characteristics:High impactApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll information provided by Samyang
Middle Barrel Temperature 200 - 240 °C
392 - 464 °F
Sumitomo Chemical ESPOLEX® 3255 Thermoplastic Elastomer
ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi..
Middle Barrel Temperature 220 - 240 °C
428 - 464 °F
Mid-2. Region Temperature
Tisan TISLAMID® 6 Flame Retardant (V0) Heat Stabilized Nylon 6
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
Middle Barrel Temperature 220 - 240 °C
428 - 464 °F
Mid-2. Region Temperature
Tisan TISLAMID® 6 Flame Retardant (V0). Halogen Free Heat Stabilized Nylon 6
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
Middle Barrel Temperature 230 - 240 °C
446 - 464 °F
Zone 2
Eurostar Staramide BST01 PA6, Impact Modified, Injection Molded
BST01 is an Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Middle Barrel Temperature 210 - 240 °C
410 - 464 °F
Tube Extrusion
Arkema Group KYNAR FLEX® 3120-15 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness..
Middle Barrel Temperature 210 - 240 °C
410 - 464 °F
Tube Extrusion
Arkema Group KYNAR® 710, 710 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Middle Barrel Temperature 210 - 240 °C
410 - 464 °F
Tube Extrusion
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a..
Middle Barrel Temperature 220 - 240 °C
428 - 464 °F
Pipe Extrusion
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a..
Middle Barrel Temperature 210 - 240 °C
410 - 464 °F
Tube Extrusion
Arkema Group KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..
Middle Barrel Temperature 210 - 240 °C
410 - 464 °F
Tube Extrusion
Arkema Group KYNAR FLEX® 2850-00 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..