Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 190 - 220 °C | 374 - 428 °F | |
Panipol Oy DXH-PP Inherently Conductive Polymer Panipol DXH-PP composition is conductive masterbatch for melt processing mainly with polypropylene. It is based on conductive Polyaniline and resin. Main benefits of Panipol DXH-PP grade are contr.. |
|||
Front Barrel Temperature | 190 - 215 °C | 374 - 419 °F | |
PTS POM-270 27.0 MFI Acetal Copolymer Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
LG Chemical AF342T ABS, Flame Retardant, High Impact Feature: Injection Molding, Flame Retardant, High ImpactApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provide.. |
|||
Front Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
LG Chemical ALPHALAC SH860 HIPS Description: Injection Molding, General Purpose, Good ProcessabilityApplication: Refrigerator Inner LinerCAS No. 9003-55-8Information provided by LG Chemical |
|||
Front Barrel Temperature | 190 - 200 °C | 374 - 392 °F | |
LG Chemical LUCEL FW-7005 Friction and Wear Resistant POM, Oil filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Front Barrel Temperature | 190 - 200 °C | 374 - 392 °F | |
LG Chemical LUCEL N109-HR Heat Resistant POM, Unreinforced, Standard Viscosity LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Front Barrel Temperature | 190 - 200 °C | 374 - 392 °F | Injection Molding |
LG Chemical LUCEL N109LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
Front Barrel Temperature | 190 - 200 °C | 374 - 392 °F | Injection Molding |
LG Chemical LUCEL N109LDS POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
Front Barrel Temperature | 190 - 200 °C | 374 - 392 °F | |
LG Chemical LUCEL N115 POM, Unreinforced, High Viscosity LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Front Barrel Temperature | 190 - 210 °C | 374 - 410 °F | |
Kolon Kocetal® K300 General Purpose Grade Acetal Copolymer Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Front Barrel Temperature | 190 - 210 °C | 374 - 410 °F | |
Kolon Kocetal® K700 General Purpose Grade Acetal Copolymer Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Front Barrel Temperature | 190 - 260 °C | 374 - 500 °F | Injection |
Inno-Comp INNOPOL® CS 3-8000 FR Flame Retardant Polypropylene Blend INNOPOL® CS 3-8000 FR is a flame retarded polypropylene compound based on a specific blend of polypropylene homo polymer and copolymer. This grade is available in natural and custom colored form... |
|||
Front Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
LG Chemical 82TR SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical |
|||
Front Barrel Temperature | 190 °C | 374 °F | Metering zone |
Taiwan PU Corporation TPU-EH95 High Hydrolysis Resistance, Extrusion Molding Polyether Base TPU Thermoplastic Polyurethane (TPU), High Hydrolysis Resistance, Polyether Base, Extrusion MoldingInformation provided by Taiwan PU Corporation. |
|||
Front Barrel Temperature | 190 °C | 374 °F | Metering zone |
Taiwan PU Corporation TPUI-E90 General Grade, Injection Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
Front Barrel Temperature | 190 - 230 °C | 374 - 446 °F | |
Borealis Beta (ß)-PP™ BE60-7032 Grey Polypropylene Homopolymer for Pressure Pipes, Fittings and Sheets Beta(ß)-PP BE60-7032 is a high molecular weight, low melt flow rate polypropylene homopolymer with fine grained ß-modification crystalline structure leading to excellent impact strength even at lo.. |
|||
Front Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Pre-3. Region Temperature |
Tisan TISAKRIL® Flame Retardant (V0) ABS TISAKRIL has a wide area of application in automotive, electronics, computer, construction, and furniture industries. General Specifications include: High surface luminosityEasy processabilityDimens.. |
|||
Front Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Pre-3. Region Temperature |
Tisan TISAKRIL® UNR ABS TISAKRIL has a wide area of application in automotive, electronics, computer, construction, and furniture industries. General Specifications include: High surface luminosityEasy processabilityDimens.. |
|||
Front Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Pre-3. Region Temperature |
Tisan TISOPLEN® 10% Calcite Filled Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Front Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Pre-3. Region Temperature |
Tisan TISOPLEN® 15% Mineral Filled Flame Retardant (V0). Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Front Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Pre-3. Region Temperature |
Tisan TISOPLEN® 40% Calcite Filled Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Front Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Pre-3. Region Temperature |
Tisan TISOPLEN® 40% Calcite Filled Heat Stabilized Homopolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Front Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Pre-3. Region Temperature |
Tisan TISOPLEN® Flame Retardant (V0). Heat Stabilized, Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Front Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Pre-3. Region Temperature |
Tisan TISOPLEN® 20% Calcite Filled Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Front Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Pre-3. Region Temperature |
Tisan TISOPLEN® 20% Talc Filled Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Front Barrel Temperature | 190 - 210 °C | 374 - 410 °F | H-1 |
Denka STYROL MW1 Polystyrene "DENKA SYTROL MW" is a well-balanced polystyrene (PS) resin, with a high tensile strength as well as good moldability. Overturning the traditional understanding that PS resin is "hard and brittle," .. |
|||
Front Barrel Temperature | 190 °C | 374 °F | Injection |
Alliance Polymers Viprene™ G80A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G80A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Front Barrel Temperature | 190 °C | 374 °F | Injection |
Alliance Polymers Viprene™ P85A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P85A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Front Barrel Temperature | 190 °C | 374 °F | Injection |
Alliance Polymers Viprene™ G85A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G85A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |