Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
LG Chemical AF312A ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
LG Chemical ER460 ABS, Medium Heat Resistance, High Flowability Feature: Injection Molding, Medium Heat Resistance, High FlowabilityApplication: Automobile, Motor Cycle, Electric & Electronic GoodsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
LG Chemical FH380P ABS, High Flow Feature: Injection Molding, High Flow, Good PaintabilityApplication: Electric & Electronic Painting Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
LG Chemical HG173 ABS, High Surface Gloss Feature: Injection Molding, High Surface GlossApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
LG Chemical HI100X ABS, High Impact, Semi-Transparency, Flexible Feature: Injection Molding, High Impact, Semi-Transparency, FlexibleApplication: Artificial Nails, Miscellaneous Goods)CAS No. 9010-94-0Information provided by LG Chemical |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
LG Chemical HI110 ABS, High Impact, Chemical Resistance Feature: Injection Molding, High Impact, Chemical ResistanceApplication: Edge of Furniture ApplicationsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
LG Chemical HI121U ABS Feature: Injection Molding, Well Balanced Mechanical Properties, Good weatherabilityApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemic.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
LG Chemical LUCEL EC-610B Electrically Conductive POM, 10% Carbon Black Filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
LG Chemical LUCEL MR-310 Low Warpage POM, 10% Mineral Filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
Huntsman AVALON® 65 DEU Thermoplastic Polyurethane Introduction: AVALON 65 DEU is a high performance UV-stabilized polyester based thermoplastic polyurethane for injection molding. AVALON 65 DEU is part of the AVALON Perform Range and offers a premi.. |
|||
Front Barrel Temperature | 195 - 220 °C | 383 - 428 °F | Start Point: 210°C |
Kingfa NH-627 Flame Retardant ABS Features:UL 94 V-2 @ 1.6mmHalogen-free flame retardantHigh flowApplications:OA deviceDigital cameraVidiconInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
LG Chemical AF305HT ABS, Flame Retardant, Heat Resistance Feature: Injection Molding, Flame Retardant, Heat ResistanceApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 9001-96-2, 68928-70-1, and 1309-64-4Inf.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
LG Chemical XG569C MABS, Anti-Scratch, High Gloss Feature: Injection Molding, Anti-Scratch, High GlossApplication: LCD TV Front Cabinet, Bezel, Audio/Video HousingCSA No. 9011-14-7 and 9003-56-9Information provided by LG Chemical |
|||
Front Barrel Temperature | 210 - 220 °C | 410 - 428 °F | |
Solvay TECHNYL® C 442 Black V PA6, DRY Description: Unreinforced polyamide PA6, high viscosity, with high flexibility and very high impact resistance even at low temperature, for extrusion.Available in: Europe Product Applications: It ha.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
Stellarchem AB835EM TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
Stellarchem AB855LG TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
Stellarchem AB870EM TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
Stellarchem GP-945 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
Stellarchem GP-965B TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
Stellarchem LP-845 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
Stellarchem LP-880 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Extrusion |
Stellarchem SE/PA745B TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Front Barrel Temperature | 190 - 220 °C | 374 - 428 °F | Extrusion |
Samyang Triel® 5400 Thermoplastic Polyether Ester Elastomer TRIEL® resins offer superior mechanical properties, elasticities, heat and chemical resistance, which allow it to be widely used for electric/electronic equipments, automotive parts and outdoor r.. |
|||
Front Barrel Temperature | 180 - 220 °C | 356 - 428 °F | Injection |
Samyang Triel® 5407EF Thermoplastic Polyether Ester Elastomer TRIEL® resins offer superior mechanical properties, elasticities, heat and chemical resistance, which allow it to be widely used for electric/electronic equipments, automotive parts and outdoor r.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
Borealis Beta-PPR™ RA7050 Polypropylene-Random-Copolymer for Pressure Pipe Systems Beta-PPR RA7050 is a PP-RCT, a Polypropylene-Random-Copolymer with an enhanced Crystalline structure brought about by a special ß-nucleation and with an improved Temperature resistance. Proof of t.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
Borealis Borcoat™ BB108E-1199 White Polypropylene Block Copolymer for Steel Pipe Coating Borcoat BB108E-1199, a ready made white compound, is a highly molecular weight, low melt flow polypropylene block copolymer. As a top-coat in three component polypropylene systems, Borcoat BB108E-1.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
Borealis BorECO™ BEC5015 Polypropylene Block Copolymer for Non-Pressure Pipes BorECO BEC5015 is a high molecular weight, low melt flow rate polypropylene block copolymer with high stiffness and impact strength.BorECO BEC5015 is recommended for solid wall and structured wall n.. |
|||
Front Barrel Temperature | 190 - 220 °C | 374 - 428 °F | |
Unitika TERRAMAC HV-6250H Polylactic Acid (PLA) Foam, Extrusion, blow, and foam sheet grades. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Front Barrel Temperature | 180 - 220 °C | 356 - 428 °F | |
Unitika TERRAMAC TE-1030 Polylactic Acid (PLA) High-Impact grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Front Barrel Temperature | 180 - 220 °C | 356 - 428 °F | |
Unitika TERRAMAC TE-2000 Polylactic Acid (PLA) Basic grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |