Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 190 - 220 °C | 374 - 428 °F | |
Panipol Oy DXH-PP Inherently Conductive Polymer Panipol DXH-PP composition is conductive masterbatch for melt processing mainly with polypropylene. It is based on conductive Polyaniline and resin. Main benefits of Panipol DXH-PP grade are contr.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
Huntsman AVALON® 60 DE Thermoplastic Polyurethane Introduction: AVALON 60 DE is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 60 DE is part of the AVALON Perform Range and offers a premium soling materi.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
LG Chemical AF312 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
LG Chemical ER460 ABS, Medium Heat Resistance, High Flowability Feature: Injection Molding, Medium Heat Resistance, High FlowabilityApplication: Automobile, Motor Cycle, Electric & Electronic GoodsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
LG Chemical HF380XC ABS, High Flow, High Surface Gloss Feature: Injection Molding, High Flow, High Surface GlossApplication: High melt flow index is suitable for injection molding of large and complicated part. High thermal stabilities enables to expres.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
LG Chemical KEYFLEX BT 1045D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
LG Chemical KEYFLEX BT 3028D Ester Type TPE Description: Injection Molding, TPC-ET, Functional, Fast Molding, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
LG Chemical LUCEL GB-325 Low Warpage POM, 25% Glass Bead Filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
LG Chemical PT270 ABS Feature: Injection Molding, Good PaintabilityApplication: Exterior Part of Automobile and Motor cycleCAS No. 9003-56-9Information provided by LG Chemical |
|||
Front Barrel Temperature | 180 - 220 °C | 356 - 428 °F | Extrusion |
Inno-Comp INNOPOL® CS 1-7120 AP 20% Talc Filled Polypropylene Homopolymer INNOPOL® CS 1-7120 is a 20 % talc-filled polypropylene homopolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 1-7120 is recommended for extrusion of sheet.. |
|||
Front Barrel Temperature | 180 - 220 °C | 356 - 428 °F | Extrusion |
Inno-Comp INNOPOL® CS 3-8000 FR Flame Retardant Polypropylene Blend INNOPOL® CS 3-8000 FR is a flame retarded polypropylene compound based on a specific blend of polypropylene homo polymer and copolymer. This grade is available in natural and custom colored form... |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
Huntsman AVALON® 65 DB Thermoplastic Polyurethane Introduction: AVALON 65 DB is a polyester based thermoplastic polyurethane for injection molding. AVALON 65 DB is part of the AVALON Perform Range and offers a premium soling material for sports foo.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
Huntsman AVALON® 65 DE Thermoplastic Polyurethane Introduction: AVALON 65 DE is a polyester based thermoplastic polyurethane for injection molding. AVALON 65 DE is part of the AVALON Perform Range and offers a premium soling material for sports foo.. |
|||
Front Barrel Temperature | 195 - 220 °C | 383 - 428 °F | Start Point: 210°C |
Kingfa NH-627 Flame Retardant ABS Features:UL 94 V-2 @ 1.6mmHalogen-free flame retardantHigh flowApplications:OA deviceDigital cameraVidiconInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
LG Chemical AF305HT ABS, Flame Retardant, Heat Resistance Feature: Injection Molding, Flame Retardant, Heat ResistanceApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 9001-96-2, 68928-70-1, and 1309-64-4Inf.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
LG Chemical AF308 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
LG Chemical MA221 ABS, High Impact, Low Gloss Feature: Injection Molding, Extrusion Molding, High Impact, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
LG Chemical XG568 MABS, Anti-Scratch, High Gloss Feature: Injection Molding, Anti-Scratch, High GlossApplication: LCD TV Front Cabinet, Bezel, Audio/Video HousingCSA No. 9011-14-7 and 9003-56-9Information provided by LG Chemical |
|||
Front Barrel Temperature | 210 - 220 °C | 410 - 428 °F | |
Solvay TECHNYL® C 442 Black V PA6, DRY Description: Unreinforced polyamide PA6, high viscosity, with high flexibility and very high impact resistance even at low temperature, for extrusion.Available in: Europe Product Applications: It ha.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
Stellarchem AB835EM TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
Stellarchem AB835EM-1 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed unconventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, completel.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
Stellarchem AB-860LG TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
Stellarchem GP-860 TPE Compound Product description : This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric poly.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
Stellarchem GP-860HD TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
Stellarchem MP-850 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
Stellarchem MP-950NC TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
Borealis BorECO™ BEC5015 Polypropylene Block Copolymer for Non-Pressure Pipes BorECO BEC5015 is a high molecular weight, low melt flow rate polypropylene block copolymer with high stiffness and impact strength.BorECO BEC5015 is recommended for solid wall and structured wall n.. |
|||
Front Barrel Temperature | 180 - 220 °C | 356 - 428 °F | |
Unitika TERRAMAC TE-1030 Polylactic Acid (PLA) High-Impact grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Front Barrel Temperature | 180 - 220 °C | 356 - 428 °F | |
Unitika TERRAMAC TE-1070 Polylactic Acid (PLA) High-Impact grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
LG Chemical MA201 ABS, Low Gloss Feature: Injection Molding, Extrusion Molding, General Purpose, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical |