Processing Properties Metric English Comments
Front Barrel Temperature 330 - 360 °C
626 - 680 °F
LG Chemical LUCON SE-4200H Electrically Conductive Thermoplastic
LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin..
Front Barrel Temperature 330 - 350 °C
626 - 662 °F
Unitika P-3001S Engineering Plastic
P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra..
Front Barrel Temperature 330 - 350 °C
626 - 662 °F
Unitika PT-3020
Characteristics: Dimensional accuracy (planarity) Heat resistance Creep resistance and elasticity RigidityInformation provided by Unitika Ltd.
Front Barrel Temperature 330 - 350 °C
626 - 662 °F
Unitika P-3001 Engineering Plastic
P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra..