Polymer Property : Front Barrel Temperature = 662 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Front Barrel Temperature 300 - 350 °C
572 - 662 °F
Hybrid Plastics PO6C81.01 Nanoreinforced® Polyphenylene Oxide (PPO)
PPO available on the market today is typically mixed with polystyrene or other polymers to make it processable. However, these resins degrade the excellent mechanical and flammability properties of ..
Front Barrel Temperature 300 - 350 °C
572 - 662 °F
LG Chemical LUCON PO-3000 Electrically Conductive Thermoplastic
LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin..
Front Barrel Temperature 300 - 350 °C
572 - 662 °F
LG Chemical LUCON PO-5300H Electrically Conductive Thermoplastic
LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin..
Front Barrel Temperature 300 - 350 °C
572 - 662 °F
LG Chemical LUCON PO-5300M Electrically Conductive Thermoplastic
LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin..
Front Barrel Temperature 330 - 350 °C
626 - 662 °F
Unitika P-3001S Engineering Plastic
P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra..
Front Barrel Temperature 330 - 350 °C
626 - 662 °F
Unitika PT-3020
Characteristics: Dimensional accuracy (planarity) Heat resistance Creep resistance and elasticity RigidityInformation provided by Unitika Ltd.
Front Barrel Temperature 330 - 350 °C
626 - 662 °F
Unitika P-3001 Engineering Plastic
P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra..