Arkema Group Pebax® 2533 SA 01 Polyether Block Amide (PEBA)

Category Polymer , Thermoplastic , Polyether Block Amide (PEBA)
Manufacturer Arkema
Trade Name Pebax®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Arkema Group Pebax® 2533 SA 01 Polyether Block Amide (PEBA).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Polyether block amide PEBAX® 2533 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema Group
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
ISO 1183
Water Absorption 1.2 %
<br>@Temperature 23.0 °C,<br> Time 86400 sec
1.2 %
<br>@Temperature 73.4 °F,<br> Time 24.0 hour
ISO 62
Moisture Absorption at Equilibrium 0.40 %
<br>@Temperature 20.0 °C
0.40 %
<br>@Temperature 68.0 °F
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0050 cm/cm
<br>@Thickness 4.00 mm,<br> Time 86400 sec
0.0050 in/in
<br>@Thickness 0.157 in,<br> Time 24.0 hour
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
<br>@Thickness 4.00 mm,<br> Time 86400 sec
0.0080 in/in
<br>@Thickness 0.157 in,<br> Time 24.0 hour
Mechanical Properties Metric English Comments
Hardness, Shore D 27
27
Instantaneous, Conditioned 15 days at 23°C - 50% RH; ISO 868
22
<br>@Time 15.0 sec
22
<br>@Time 0.00417 hour
Conditioned 15 days at 23°C - 50% RH; ISO 868
Tensile Strength at Break 32.0 MPa
4640 psi
Conditioned 15 days at 23°C - 50% RH; ASTM D638
Elongation at Break >= 750 %
>= 750 %
Conditioned 15 days at 23°C - 50% RH; ASTM D638
Flexural Modulus 0.0120 GPa
1.74 ksi
Conditioned 15 days at 23°C - 50% RH; ISO178
Charpy Impact Unnotched NB
<br>@Temperature 23.0 °C
NB
<br>@Temperature 73.4 °F
ISO 179
NB
<br>@Temperature -30.0 °C
NB
<br>@Temperature -22.0 °F
ISO 179
Charpy Impact, Notched NB
<br>@Temperature 23.0 °C
NB
<br>@Temperature 73.4 °F
ISO 179
NB
<br>@Temperature -30.0 °C
NB
<br>@Temperature -22.0 °F
ISO 179
Thermal Properties Metric English Comments
Melting Point 134 °C
273 °F
ISO 11357
Vicat Softening Point 58.0 °C
<br>@Load 1.02 kg
136 °F
<br>@Load 2.25 lb
ISO 306
Processing Properties Metric English Comments
Nozzle Temperature 210 °C
410 °F
Recommended
180 - 240 °C
356 - 464 °F
Mold Temperature 10.0 - 30.0 °C
50.0 - 86.0 °F
Drying Temperature 55.0 - 65.0 °C
131 - 149 °F
Dry Time 4.00 - 8.00 hour
4.00 - 8.00 hour