Polymer Property : Cure Time = 2.50 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 2.50 - 4.83 min
0.0417 - 0.0806 hour
Gelation time
Mitsui MILEXâ„¢ XL-225MB Phenol Aralkyl Resin, Standard Grade
The MILEXâ„¢ Family of products is widely featured in brake systems of automobiles made by automakers through Mitsui Chemicals'. The phenolic material is primarily used as binders in brake pad..
Cure Time 2.50 - 3.00 min

@Temperature 150 °C
0.0417 - 0.0500 hour

@Temperature 302 °F
Loctite® 3607 Pin Transfer
Surface Mount AdhesivesLoctite® Chipbonder® Surface Mount Adhesives (SMAs) maintain component positioning during wave solder and solder reflow processes. Loctite offers a variety of application te..
Cure Time 2.50 - 5.50 min
0.0417 - 0.0917 hour
ts2; ASTM D2084
ExxonMobil Exxon™ 4266 Star-Branched Butyl
Exxon SB Butyl is a copolymer of isobutylene and isoprene, including a styrene block copolymer branching agent.Information provided by ExxonMobil Chemical
Cure Time 2.50 - 7.50 min
0.0417 - 0.125 hour
ts2; ASTM D2084
ExxonMobil Exxon™ 6222 Brominated Star-Branched Butyl
Exxon SB Bromobutyl is a brominated copolymer of isobutylene and isoprene, including a styrene block copolymer branching agent.Information provided by ExxonMobil Chemical
Cure Time 2.50 min
0.0417 hour
Curelastmeter
Daikin DAI-EL G-801 Fluoroelastomer Copolymer, Peroxide Curable Grade, 66% Fluorine Content
Offers excellent chemical and steam resistance. Offers good mechanical characteristics.Features: Good low-temperature and elasticity characteristics.Information provided by Daikin Industries.
Cure Time 2.50 min
0.0417 hour
Set Time
3M Scotch-Weld™ TE230 Black Polyurethane Reactive Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as ..
Cure Time 2.50 min
0.0417 hour
Set Time
3M Scotch-Weld™ TS230 Polyurethane Reactive Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as ..
Cure Time 2.50 min
0.0417 hour
Set Time
3M Scotch-Weld™ EZ250150 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive (PUR) Easy 250 Wood Adhesive is 100% solid, warm temperature applied, moisture curing urethanes. This product bonds a wide variety of plastics and wood to th..
Cure Time 2.50 - 5.83 min
0.0417 - 0.0972 hour
Gelation time
Mitsui MILEX™ XL-1210MB Phenol Aralkyl Resin, Silicone Rubber Modified  (discontinued **)
The MILEX™ Family of products is widely featured in brake systems of automobiles made by the top automakers through Mitsui Chemicals' affiliation with leading brake manufacturers. The phenolic ..