Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 240 - 260 °C | 464 - 500 °F | |
Plastcom PLASTAMID® 66 BT B 27 TS PA66 heat stabilized Basic type PA66 for injection molding, heat stabilized, modified for general use, with excellent manufacturing properties. Use: automotive, engineering, electrical and consumer-goods industry - elec.. |
|||
Melt Temperature | 240 - 260 °C | 464 - 500 °F | |
Plastcom PLASTAMID® 66 BT SD PA66 Basic type PA66 for injection molding, modified for general use. PA66 contains TiO2 up to 0.5% wt. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fasteners,.. |
|||
Melt Temperature | 240 - 280 °C | 464 - 536 °F | |
Polykemi AB POLYblend 45FS PC/ABS-blend, Flame Retardant Information provided by Polykemi AB |
|||
Melt Temperature | 240 - 280 °C | 464 - 536 °F | |
Polykemi AB POLYblend 85FS GF10 PC/ABS-Blend, Glass Fiber reinforced Information provided by Polykemi AB |
|||
Melt Temperature | 240 - 260 °C | 464 - 500 °F | |
DuPont Performance Polymers Crastin® CE2055 NC010 PBT
(Unverified Data**) Crastin® CE2055 NC010 is an unreinforced, low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Melt Temperature | 240 - 260 °C | 464 - 500 °F | |
Plastcom SLOVAMID 6 LI/1 LS PA6, improved strength, light stability FeaturesPA 6 with the content of thermoplastic kaoutchouc. Impacted, for mouldings with high toughness either at minus temperatures, suitable for external use, eg. ski shoes, sports and safety helme.. |
|||
Melt Temperature | <= 240 °C | <= 464 °F | |
EVALCA EVAL® F100 Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 32 mol % Ethylene.Data provided by EVALCA. Applications: Melt phase forming. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a pa.. |
|||
Melt Temperature | 240 - 280 °C | 464 - 536 °F | |
BASF Capron® 8203C Nylon 6 (Conditioned)
(discontinued **) Capron 8203C is a high viscosity, nylon 6 extrusion compound, possessing a modified crystalline structure for increased property performance and faster set up for tubing and cable applications. It.. |
|||
Melt Temperature | 240 - 280 °C | 464 - 536 °F | |
BASF Capron® 8203C Nylon 6 (Dry)
(discontinued **) Capron 8203C is a high viscosity, nylon 6 extrusion compound, possessing a modified crystalline structure for increased property performance and faster set up for tubing and cable applications. It.. |
|||
Melt Temperature | 240 - 260 °C | 464 - 500 °F | |
LG Chemical Lupox® PBT-GP-2306F 30% GFR Flame Retardant PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Melt Temperature | 240 - 270 °C | 464 - 518 °F | Injection Molding |
LG Chemical LUPOY HR5007AE PC/ABS, High Impact Description: Injection Molding, PC/ABS, High Flow, High ImpactApplication: E&E (Housing)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical |
|||
Melt Temperature | 240 - 260 °C | 464 - 500 °F | Injection |
Inno-Comp INNOPOL® CS 1-7120 AP 20% Talc Filled Polypropylene Homopolymer INNOPOL® CS 1-7120 is a 20 % talc-filled polypropylene homopolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 1-7120 is recommended for extrusion of sheet.. |
|||
Melt Temperature | 240 °C | 464 °F | Injection Molding; ISO 294 |
Ineos ABS Lustran® ABS E112LG Pellets Lustran® ABS E112LG is extrusion grade for low gloss surfaces. It is used for the production of molded plastic articles. |
|||
Melt Temperature | 240 - 290 °C | 464 - 554 °F | |
LATI Kelon® B H CETG/300 PA 6, Glass/Mineral Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers / Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Melt Temperature | 240 - 260 °C | 464 - 500 °F | |
LATI Latamid 6 H2 G/20-V2HF PA 6, 20% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Euro.. |
|||
Melt Temperature | 240 - 250 °C | 464 - 482 °F | |
LATI Later 4 G/30 PBT, 30% Glass Fiber Reinforced Polybutylene Terephthalate (PBT) based compound. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast.. |
|||
Melt Temperature | 240 - 260 °C | 464 - 500 °F | |
LATI Latiblend 3675 G/10 ABS/PBT, 10% Glass Fiber Reinforced Blend based on Acrylonitrile-Butadiene-Styrene copolymer (ABS) / Polybutylene Terephthalate (PBT). Glass fibers. Good surface appearance.Availability: Africa & Middle East; Asia Pacific; Europe; Lat.. |
|||
Melt Temperature | 240 - 280 °C | 464 - 536 °F | |
LATI Latiohm 62-03 PD01 G/20 PPA, 20% Glass Fiber Reinforced Semiconductive/dissipative product based on Polyamide 6 (PA6). Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indust.. |
|||
Melt Temperature | 240 - 270 °C | 464 - 518 °F | ISO 294 |
Styrolution Novodur® E211 ABS Novodur E211 is a high heat extrusion grade and suitable for blow moldingInformation provided by Styrolution |
|||
Melt Temperature | 240 - 250 °C | 464 - 482 °F | |
Samyang Triloy® 130 PC/PBT alloy Characteristics:Impact resistantChemical resistantDimensional stabilityProcessabilityGood flowApplications:Automotive bumperAutomotive outdoor handleAll information provided by Samyang |
|||
Melt Temperature | 240 - 250 °C | 464 - 482 °F | |
Samyang Triloy® 210 PC/ABS alloy Characteristics:Impact resistantHeat resistantGood flowApplications:Camera partsExterior panelCluster fasciaWheel coverStructural applicationI/P. core panelHelmet shellGlove box doorCowl vent grillA.. |
|||
Melt Temperature | 240 - 275 °C | 464 - 527 °F | |
A. Schulman SCHULAMID® 6 MV5 Unreinforced Nylon 6 Information provided by A. Schulman. |
|||
Melt Temperature | 240 °C | 464 °F | Injection Molding; ISO 294 |
Covestro Bayblend® FR 3008 Polycarbonate + ABS, Flame Retardant Grade Injection molding gradeHDT/A = 85 °CVicat/B 120 temperature = 103 °CUL-listing 94 V-0 (1.5 mm)improved chemical and hydrolysis resistance antimony-, chlorine- and bromine-free flame retardant.. |
|||
Melt Temperature | 240 - 270 °C | 464 - 518 °F | |
Covestro Bayblend® FR 3021 Polycarbonate + ABS, Mineral Filled 15 % mineral filledinjection molding gradeincreased stiffnesstensile modulus = 4800 MPaVicat/B 120 temperature = 98 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame ret.. |
|||
Melt Temperature | 240 °C | 464 °F | Injection molding; ISO 294 |
Covestro Bayblend® FR3001 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Melt Temperature | 240 °C | 464 °F | Injection molding; ISO 294 |
Covestro Bayblend® FR3210 TV PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Melt Temperature | 240 °C | 464 °F | Injection molding; ISO 294 |
Covestro Bayblend® R-FR610 Polycarbonate Recyclate Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame retardantAs of 1 S.. |
|||
Melt Temperature | 240 - 270 °C | 464 - 518 °F | |
Eurostar Staramide PFB42U PA6, Glass Fiber/Bead Filled, Injection Molded Starflam PFB42U is an UV Stabilized, Glass Bead and Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Melt Temperature | 240 - 285 °C | 464 - 545 °F | |
BASF Ultramid® 8200 HS PA 6 (Dry) Description: Ultramid 8200 HS is a heat stabilized, medium viscosity, PA6 injection molding homopolymer, exhibiting resistance to sink-mark formation in thick sections, and improved toughness over c.. |
|||
Melt Temperature | 240 - 285 °C | 464 - 545 °F | |
BASF Ultramid® 8202 L Intermediate PA6 (Conditioned) Description: Ultramid 8202 L-Intermediate is an unreinforced, low viscosity, non-lubricated PA6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is avai.. |