Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 170 - 195 °C | 338 - 383 °F | |
Premix Thermoplastics PRE-ELEC® ESD 4300 PRE-ELEC ESD 4300 is a static dissipative thermoplastic compound based on PE-LD. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 4300 has been developed for mult.. |
|||
Melt Temperature | 180 - 195 °C | 356 - 383 °F | |
SABIC HP0322N Low Density Polyethylene for Blown Film Product Description: HP0322N is a Low Density Polyethylene grade suitable for producing heavy duty films and contains no slip or antiblock additives. It yields outstanding toughness and optical pr.. |
|||
Melt Temperature | 170 - 195 °C | 338 - 383 °F | Injection |
Huntsman IROGRAN® A 78 E 4506 TPU-Polyester Introduction: IROGRAN A 78 E 4506 is a thermoplastic polyester- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are excellent mechanical prop.. |
|||
Melt Temperature | 170 - 195 °C | 338 - 383 °F | Injection |
Huntsman IROGRAN® A 78 E 4723 Polyester-Based TPU-Injection Extrusion Grade Introduction: IROGRAN A 78 E 4723 is a thermoplastic polyester- polyurethane for injection moulding and extrusion applications. Additional characteristics of the product are flexibility and high mec.. |
|||
Melt Temperature | 170 - 195 °C | 338 - 383 °F | Injection |
Huntsman IROGRAN® A 78 P 4766 TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
Melt Temperature | 170 - 195 °C | 338 - 383 °F | Injection |
Huntsman IROGRAN® A 85 E 4607 E TPU-Polyester Introduction: IROGRAN A 85 E 4607 is a thermoplastic polyether- polyurethane intended for extrusion and injection molding applications. Additional characteristics of the product are excellent mechan.. |
|||
Melt Temperature | 170 - 195 °C | 338 - 383 °F | Injection |
Huntsman IROGRAN® A 85 H 4508 TPU-Polyester Introduction: IROGRAN A 85 H 4508 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are excellent mechanical properties and hig.. |
|||
Melt Temperature | 170 - 195 °C | 338 - 383 °F | Injection |
Huntsman IROGRAN® A 85 P 4350 TPU-Polyether Introduction: IROGRAN A 85 P 4350 is a flame-retardant, halogen-free, thermoplastic polyether-polyurethane intended for extrusion and injection molding applications. Additional characteristics of th.. |
|||
Melt Temperature | 170 - 195 °C | 338 - 383 °F | Injection |
Huntsman IROGRAN® A 85 P 4380 TPU-Polyether Introduction: IROGRAN A 85 P 4380 is a flame-retardant, halogen-free, thermoplastic polyether-polyurethane intended for extrusion and injection molding applications. Additional characteristics of th.. |
|||
Melt Temperature | 170 - 195 °C | 338 - 383 °F | Injection |
Huntsman IROGRAN® A 86 E 4486 Polyester-Based TPU-Injection Extrusion Grade Introduction: IROGRAN A 86 E 4486 is a thermoplastic polyester- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are excellent mechanical prop.. |
|||
Melt Temperature | 170 - 195 °C | 338 - 383 °F | Injection |
Huntsman IROGRAN® A 92 P 4637 TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
Melt Temperature | 170 - 195 °C | 338 - 383 °F | |
Huntsman IROGRAN® A 92 P 4851 Ether-Based TPU-For Cable Industry Introduction: IROGRAN A 92 P 4851 is a thermoplastic polyether- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are high extrudability and lo.. |
|||
Melt Temperature | 170 - 195 °C | 338 - 383 °F | Injection |
Huntsman IROGRAN® A 95 E 4813 Polyester-Based TPU-High Performance Grade Introduction: IROGRAN A 95 R 4813 is a thermoplastic polyester- polyurethane for injection moulding applications. Additional characteristics of the product are very short cycle times and high dimens.. |
|||
Melt Temperature | 170 - 195 °C | 338 - 383 °F | Injection |
Huntsman IROGRAN® A 80 H 4698 Polyester-Based TPU-Injection Molding Grade Introduction: IROGRAN A 80 H 4698 is a transparent thermoplastic polyester-polyurethane for injection molding applications. Additional characteristics of the product are good melt flow and easy demo.. |
|||
Melt Temperature | 170 - 195 °C | 338 - 383 °F | Injection |
Huntsman IROGRAN® A 92 E 4694 Polyester-Based TPU-Injection Extrusion Grade Introduction: IROGRAN A 92 E 4694 is a thermoplastic special- polyester-polyurethane for injection moulding and extrusion applications. Additional characteristics of the product are flexibility and .. |
|||
Melt Temperature | 170 - 195 °C | 338 - 383 °F | Injection |
Huntsman IROGRAN® A 92 E 4738 Polyester-Based TPU-Injection Extrusion Grade Introduction: IROGRAN A 92 E 4738 is a white-colored, thermoplastic special-polyester-polyurethane for injection molding applications. Additional characteristics of the product are flexibility and h.. |
|||
Melt Temperature | 170 - 195 °C | 338 - 383 °F | Injection |
Huntsman IROGRAN® A 92 H 4656 Polyester-Based TPU-Injection Molding Grade Introduction: IROGRAN A 92 H 4656 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and e.. |
|||
Melt Temperature | 170 - 195 °C | 338 - 383 °F | Blown Film Coextrusion |
DuPont™ Appeel® 45D747 Polyolefin Appeel® 45D747 is a modified polyolefin resin designed to provide easy peel functionality from polyethylene copolymers. Appeel® 45D747 is available in pellet form for use in conventional extrusion.. |
|||
Melt Temperature | 185 - 195 °C | 365 - 383 °F | |
Eurostar Starpylen HU 30BF4 PP, 30% Bamboo Fiber Filled, Injection Molding Starpylen HU30BF4 is a 30% Bamboo Fiber Reinforced Polypropylene Injection Molding Resin (also known as HU30BF4) (PRELIMINARY DATASHEET)Information provided by Eurostar. |