Polymer Property : Melt Temperature = 325 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 315 - 325 °C
599 - 617 °F
Optimum adhesion is obtained at a draw span of about 10 cm. Treatment of the substrate or the use of primers will significantly enhance adhesion.
NOVA Chemicals Novapol® LC-0517-A LDPE Extrusion Resin
Excellent adhesion, High drawdown, Excellent sealabilityApplications: Dry soup pouches, Powdered drink pouches, Pharmaceutical packaging, Potato chip bags, Flexible and snack food packagingAdditives..
Melt Temperature 315 - 325 °C
599 - 617 °F
Optimum adhesion is obtained at a draw span of about 10 cm. Treatment of the substrate or the use of primers will significantly enhance adhesion.
NOVA Chemicals Novapol® LC-0522-A LDPE Extrusion Resin
Excellent sealability, High drawdown, High adhesion, Good barrier, High stiffness, Good abrasion resistanceApplications: Milk cartons, Paperboard containers, Liquid packaging, Woven fabrics, Lumber ..
Melt Temperature 315 - 325 °C
599 - 617 °F
Optimum adhesion is obtained at a draw span of about 10 cm. Treatment of the substrate or the use of primers will significantly enhance adhesion.
NOVA Chemicals Novapol® LC-0717-A LDPE Extrusion Resin
High speeds, Low coating weights, Excellent adhesion, Excellent drawdown, Excellent sealabilityApplications: Sugar pouch stock; Popsicle wrap, Multi-wall bags, High speed/low coating weight paper co..
Melt Temperature 315 - 325 °C
599 - 617 °F
Extrusion Coating
NOVA Chemicals Sclair® 61C Octene LLDPE Extrusion Resin  (discontinued **)
Features: Octene co-polymer, excellent sealability and toughness, high drawdown, high adhesion, good barrier, good abrasion resistance.Applications: Food packaging, milk cartons, paperboard containe..
Melt Temperature 300 - 325 °C
572 - 617 °F
LATI LAESTRA E01 G/30 30% Glass Fiber Reinforced, Elastomer Modified Syndiotactic Polystyrene (SPS)  (disconti
Description: Laestra compounds are syndiotactic polystyrene (SPS) products. SPS is a polymer offering a combination of properties unavailable with other materials. It exhibits a melting point of 270..
Melt Temperature 300 - 325 °C
572 - 617 °F
LATI LAESTRA G/30 30% Glass Fiber Reinforced Syndiotactic Polystyrene (SPS)  (discontinued **)
Description: Laestra compounds are syndiotactic polystyrene (SPS) products. SPS is a polymer offering a combination of properties unavailable with other materials. It exhibits a melting point of 270..
Melt Temperature 300 - 325 °C
572 - 617 °F
LATI LAESTRA G/30-V0CT1 30% Glass Fiber Reinforced, Elastomer Modified, Flame Retardant Syndiotactic Polystyrene (SPS)
Description: Laestra compounds are syndiotactic polystyrene (SPS) products. SPS is a polymer offering a combination of properties unavailable with other materials. It exhibits a melting point of 270..
Melt Temperature 315 - 325 °C
599 - 617 °F
NOVA Chemicals Novapol® LE-0520-AM LDPE Extrusion Resin  (discontinued **)
Features: easy processing, good dispersion.Applications: extrusion coating.Data provided by the manufacturer.
Melt Temperature 315 - 325 °C
599 - 617 °F
NOVA Chemicals Novapol® LM-1019-A LDPE Masterbatch Resin  (discontinued **)
Features: easy processing, good dispersion.Applications: masterbatch/compounding.Data provided by the manufacturer.
Melt Temperature 305 - 325 °C
581 - 617 °F
Covestro Apec® DP9-9331 High-Heat Polycarbonate, General Purpose  (discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
Melt Temperature 305 - 325 °C
581 - 617 °F
Covestro Apec® DP9-9333 High-Heat Polycarbonate, General Purpose, UV-Stabilized  (discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
Melt Temperature 70.0 - 325 °C
158 - 617 °F
Average value: 282 °C Grade Count:14
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl..
Melt Temperature 300 - 325 °C
572 - 617 °F
LATI LAESTRA G/40-V0CT1 40% Glass Fiber Reinforced, Elastomer Modified, Flame Retardant Syndiotactic Polystyrene (SPS)
Description: Laestra compounds are syndiotactic polystyrene (SPS) products. SPS is a polymer offering a combination of properties unavailable with other materials. It exhibits a melting point of 270..
Melt Temperature 320 - 325 °C
608 - 617 °F
DAM
DuPont Performance Polymers Zytel® HTN FR52G30NHF BK337 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTNFR52G30NHF BK337 is a 30% glass reinforced, flame retardant, lubricated high performance polyamide resin with improved flow. It is also a PPA resin and it uses a non-halogenated flame ret..
Melt Temperature 300 - 325 °C
572 - 617 °F
LATI LAESTRA G/40 40% Glass Fiber Reinforced Syndiotactic Polystyrene (SPS)  (discontinued **)
Description: Laestra compounds are syndiotactic polystyrene (SPS) products. SPS is a polymer offering a combination of properties unavailable with other materials. It exhibits a melting point of 270..