Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 320 - 340 °C | 608 - 644 °F | |
PolyOne OnForce™ LFT LF9200-5001 RS Natural Polyphenylene Sulfide (PPS) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Melt Temperature | 320 - 340 °C | 608 - 644 °F | |
PolyOne OnForce™ LFT SF-40LCF/000 Black Polyphenylene Sulfide (PPS) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Melt Temperature | 320 - 340 °C | 608 - 644 °F | |
PolyOne OnForce™ LFT SF-40LGF/001 Natural Polyphenylene Sulfide (PPS) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Melt Temperature | 320 - 330 °C | 608 - 626 °F | |
Solvay Specialty Polymers Primef® 4010 Polyphenylene Sulfide (PPS), 40% Glass Fiber Reinforcement
(discontinu Primef 4010 is a 40% glass fiber reinforced polyphenylene sulfide (PPS) that offers enhanced mechanical properties. In general, PPS offers an excellent balance of properties including high temperatu.. |
|||
Melt Temperature | 320 - 330 °C | 608 - 626 °F | |
Solvay Specialty Polymers Primef® 7002 Polyphenylene Sulfide (PPS), 65% GlassMineral
(discontinued **) Primef 7002 is a 65% mineral/glass fiber reinforced polyphenylene sulfide (PPS). This grade offers higher fluidity than Primef 7010 (also 65% mineral/glass fiber), but with somewhat lower mechanical.. |
|||
Melt Temperature | 320 - 330 °C | 608 - 626 °F | DAM |
DuPont Performance Polymers Zytel® HTN 51G15HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN51G15HSL BK083 is a 15% glass reinforced, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polymers |
|||
Melt Temperature | 320 - 330 °C | 608 - 626 °F | DAM |
DuPont Performance Polymers Zytel® HTN 52G35HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN52G35HSL BK083 is a 35% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds. It is also a PPA resin.Information provid.. |
|||
Melt Temperature | 320 - 330 °C | 608 - 626 °F | DAM |
DuPont Performance Polymers Zytel® HTN 54G35HSLR NC010 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN54G35HSLR NC010 is a 35% glass reinforced, toughened, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polym.. |
|||
Melt Temperature | 320 - 330 °C | 608 - 626 °F | DAM |
DuPont Performance Polymers Zytel® HTN FG52G35HSL BK011 Polyphthalamide (PPA)
(Unverified Data**) Zytel®® HTNFG52G35HSL BK011 is a 35% glass reinforced, lubricated, heat stabilized high performance polyamide resin, developed for consideration into applications for the food industry. It is also.. |
|||
Melt Temperature | 320 - 340 °C | 608 - 644 °F | |
PolyOne Edgetek® AM-35GF/000 FR NH Polyphthalamide (PPA) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Melt Temperature | 320 - 340 °C | 608 - 644 °F | |
LATI Latilub 57D-15T G/30 PPA, 30% Glass Fiber Reinforced Self-lubricating product based on Semi-aromatic polyamide (PPA). PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lat.. |
|||
Melt Temperature | 320 - 340 °C | 608 - 644 °F | |
LATI Latiohm 57-05 PD01 G/15 PPA, 15% Glass Fiber Reinforced Semiconductive/dissipative product based on Semi-aromatic polyamide (PPA). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by.. |
|||
Melt Temperature | 320 - 340 °C | 608 - 644 °F | |
Covestro Apec® 1703 Polycarbonate UV-stabilizedsoftening temperature (VST/B 120)=171 °CPreprocessingMax. Water content |
|||
Melt Temperature | 320 - 330 °C | 608 - 626 °F | |
Covestro Apec® DP1-9354 Polycarbonate, Flame Retardant Grade Developmental productflame retardant: V-0/1,5mm (UL 94)V-0/3,0mm (UL 94)5VA/3mm (UL 94)softening temperature (VST/B 120)=185 °Conly opaque colors availablePreprocessingMax. Water content |
|||
Melt Temperature | 320 °C | 608 °F | Optimal |
BASF Ultramid® KR 4355 G10 BK 23215 50% Glass Filled PA6/6T (Conditioned) Description: 50% glass-fiber reinforced product for injection molding; high toughness and rigidity; low water absorption, high melting point (285°C); mechanical properties remain constant up to 60°.. |
|||
Melt Temperature | 320 °C | 608 °F | Optimal |
BASF Ultramid® KR 4355 G10 BK 23215 50% Glass Filled PA6/6T (Dry) Description: 50% glass-fiber reinforced product for injection molding; high toughness and rigidity; low water absorption, high melting point (285°C); mechanical properties remain constant up to 60°.. |
|||
Melt Temperature | 320 °C | 608 °F | Optimal |
BASF Ultramid® KR 4355 G7 BK 00564 35% Glass Filled PA6/6T (Conditioned) Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Melt Temperature | 320 °C | 608 °F | Optimal |
BASF Ultramid® KR 4357 G6 BK 00564 30% Glass Filled PA6/6T (Dry) Description: 30% glass-fiber reinforced, impact-modified product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechan.. |
|||
Melt Temperature | >= 320 °C | >= 608 °F | Optimal |
BASF Ultramid® KR 4365 G5 35% Glass Filled PA6/6T FR (Dry) Description: Partially aromatic polyamide; flame retardant based on red phosphorus; low water absorption, high melting point (295°C); low tendency to form deposits on electrical contacts, very resi.. |
|||
Melt Temperature | >= 320 °C | >= 608 °F | Optimal |
BASF Ultramid® KR 4365 G5 BK 00100 35% Glass Filled PA6/6T FR (Conditioned) Description: Partially aromatic polyamide; flame retardant based on red phosphorus; low water absorption, high melting point (295°C); low tendency to form deposits on electrical contacts, very resi.. |
|||
Melt Temperature | >= 320 °C | >= 608 °F | Optimal |
BASF Ultramid® KR 4365 G5 BK 00100 35% Glass Filled PA6/6T FR (Dry) Description: Partially aromatic polyamide; flame retardant based on red phosphorus; low water absorption, high melting point (295°C); low tendency to form deposits on electrical contacts, very resi.. |
|||
Melt Temperature | 320 - 335 °C | 608 - 635 °F | |
Solvay Specialty Polymers Amodel® A-6135 NL Polyphthalamide (PPA), 35% Glass Fiber Reinforcement
(discontin Amodel A-6135 NL polyphthalamide (PPA), a 35% glass reinforced, high-glow, non-lubricated, hot-water moldable resin specially designed for laser welding. The black version is a laser absorber, and t.. |
|||
Melt Temperature | 320 - 330 °C | 608 - 626 °F | DAM |
DuPont Performance Polymers Zytel® HTN 51G35HSLR BK420J Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN51G35HSLR BK420J is a 35% glass reinforced, heat stabilized, lubricated high performance polyamide resin with improved hydrolysis resistance and surface appearance. It is also a PPA resin.. |
|||
Melt Temperature | 320 - 330 °C | 608 - 626 °F | DAM |
DuPont Performance Polymers Zytel® HTN FE8200 BK431 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFE8200 BK431 is an unreinforced, toughened, heat stabilized, lubricated high performance polyamide resin for injection molding. It is also a PPA resin.Information provided by DuPont Perfo.. |
|||
Melt Temperature | 320 - 330 °C | 608 - 626 °F | |
Solvay Specialty Polymers Amodel® A-1625 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1625 HS is a 25% carbon and glass-reinforced, heat-stabilized grade of polyphthalamide (PPA). It is formulated for applications requiring the dissipation of static charge. This material is .. |