Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 320 - 340 °C | 608 - 644 °F | |
PolyOne OnForce™ LFT SF-40LCF/000 Black Polyphenylene Sulfide (PPS) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Melt Temperature | 320 - 340 °C | 608 - 644 °F | |
PolyOne OnForce™ LFT SF-40LGF/001 Natural Polyphenylene Sulfide (PPS) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Melt Temperature | 320 - 330 °C | 608 - 626 °F | DAM |
DuPont Performance Polymers Zytel® HTN 54G35HSLR NC010 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN54G35HSLR NC010 is a 35% glass reinforced, toughened, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polym.. |
|||
Melt Temperature | 320 - 330 °C | 608 - 626 °F | DAM |
DuPont Performance Polymers Zytel® HTN FG52G35HSL BK011 Polyphthalamide (PPA)
(Unverified Data**) Zytel®® HTNFG52G35HSL BK011 is a 35% glass reinforced, lubricated, heat stabilized high performance polyamide resin, developed for consideration into applications for the food industry. It is also.. |
|||
Melt Temperature | 320 - 350 °C | 608 - 662 °F | |
LATI LAPEX A Polyethersulfone (PES) (UL94 V-0)
(Unverified Data**) Description: Lapex A compounds are polyethersulfone (PES) products. They are high temperature compounds offering an interesting combination of properties. Lapex A provides outstanding thermal resist.. |
|||
Melt Temperature | 320 - 340 °C | 608 - 644 °F | |
PolyOne Edgetek® AM-35GF/000 FR NH Polyphthalamide (PPA) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Melt Temperature | 320 - 360 °C | 608 - 680 °F | |
LATI LAXTAR G/30 30% Glass Reinforced LCP
(discontinued **) Description: Laxtar products are liquid crystal polymers (LCP). They offer exceptional performance together with increasing cost-effectiveness. Due to the outstanding fluidity at high shear rates LC.. |
|||
Melt Temperature | 320 - 330 °C | 608 - 626 °F | |
Solvay Specialty Polymers Amodel® A-1625 HS Polyphthalamide (PPA), 25% GlassCarbon Fiber Amodel® A-1625 HS is a 25% carbon and glass-reinforced, heat-stabilized grade of polyphthalamide (PPA). It is formulated for applications requiring the dissipation of static charge. This material.. |
|||
Melt Temperature | 320 - 340 °C | 608 - 644 °F | |
Covestro Apec® 1695 Polycarbonate Easy flowingeasy to demoldsoftening temperature (VST/B 120)=158 °CPreprocessingMax. Water content |
|||
Melt Temperature | 320 - 340 °C | 608 - 644 °F | |
Covestro Apec® 1745 Polycarbonate Easy to demoldsuitable for superheated steam sterilization up to 143 °C as well as for pharmaceutical applications according to United States Pharmacopeia (USP) XXII Class VIsoftening temperature (.. |
|||
Melt Temperature | 320 - 340 °C | 608 - 644 °F | |
Covestro Apec® 1795 Polycarbonate Easy flowingeasy to demoldsoftening temperature (VST/B 120)=173°CPreprocessingMax. Water content |
|||
Melt Temperature | 320 - 330 °C | 608 - 626 °F | |
Covestro Apec® DP1-9354 Polycarbonate, Flame Retardant Grade Developmental productflame retardant: V-0/1,5mm (UL 94)V-0/3,0mm (UL 94)5VA/3mm (UL 94)softening temperature (VST/B 120)=185 °Conly opaque colors availablePreprocessingMax. Water content |
|||
Melt Temperature | 320 - 340 °C | 608 - 644 °F | |
Covestro Apec® DP1-9354/1 Polycarbonate, Flame Retardant Grade Developmental productflame retardant: V-0/3,2mm (UL 94)V-2/1,5mm (UL 94),softening temperature (VST/B 120)=185 °Calso available in transparent colorsPreprocessingMax. Water content |
|||
Melt Temperature | 320 - 330 °C | 608 - 626 °F | DAM |
DuPont Performance Polymers Zytel® HTN 51G35NOX BK420 Polyphthalamide (PPA) Zytel® HTN51G35NOX BK083 is a 35% glass reinforced high performance polyamide resin developed for Selective Catalytic Reduction applications that require exposure to water/urea solution. It is also.. |
|||
Melt Temperature | 320 °C | 608 °F | Optimal |
BASF Ultramid® KR 4355 G5 25% Glass Filled PA6/6T (Conditioned) Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Melt Temperature | 320 °C | 608 °F | Optimal |
BASF Ultramid® KR 4355 G7 BK 00564 35% Glass Filled PA6/6T (Dry) Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Melt Temperature | 320 °C | 608 °F | Optimal |
BASF Ultramid® KR 4357 G6 BK 00564 30% Glass Filled PA6/6T (Conditioned) Description: 30% glass-fiber reinforced, impact-modified product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechan.. |
|||
Melt Temperature | >= 320 °C | >= 608 °F | Optimal |
BASF Ultramid® KR 4365 G5 35% Glass Filled PA6/6T FR (Dry) Description: Partially aromatic polyamide; flame retardant based on red phosphorus; low water absorption, high melting point (295°C); low tendency to form deposits on electrical contacts, very resi.. |
|||
Melt Temperature | 320 - 330 °C | 608 - 626 °F | |
Solvay Specialty Polymers Primef® 4002 40% GF PPS, High Fluidity Grade
(discontinued **) Used for injection molding of high performance parts. |
|||
Melt Temperature | 320 - 330 °C | 608 - 626 °F | DAM |
DuPont Performance Polymers Zytel® HTN 51G45HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN51G45HSL BK083 is a 45% glass reinforced, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polymers |
|||
Melt Temperature | 320 - 325 °C | 608 - 617 °F | DAM |
DuPont Performance Polymers Zytel® HTN FR52G30NHF BK337 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFR52G30NHF BK337 is a 30% glass reinforced, flame retardant, lubricated high performance polyamide resin with improved flow. It is also a PPA resin and it uses a non-halogenated flame ret.. |
|||
Melt Temperature | 320 - 330 °C | 608 - 626 °F | DAM |
DuPont Performance Polymers Zytel® HTN FR52G45BL BK337 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFR52G45BL BK337 is a 45% glass reinforced, flame retardant, lubricated high performance polyamide resin that has been developed for connector applications.Information provided by DuPont .. |
|||
Melt Temperature | 320 - 330 °C | 608 - 626 °F | DAM |
DuPont Performance Polymers Zytel® HTN 51G35HSLR BK420J Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN51G35HSLR BK420J is a 35% glass reinforced, heat stabilized, lubricated high performance polyamide resin with improved hydrolysis resistance and surface appearance. It is also a PPA resin.. |
|||
Melt Temperature | 320 - 330 °C | 608 - 626 °F | |
Solvay Specialty Polymers Amodel® A-1625 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1625 HS is a 25% carbon and glass-reinforced, heat-stabilized grade of polyphthalamide (PPA). It is formulated for applications requiring the dissipation of static charge. This material is .. |