Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 185 - 243 °C | 365 - 469 °F | Average value: 218 °C Grade Count:8 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Glass Filled". Each property range of values reported is minimum .. |
|||
Melt Temperature | 210 - 243 °C | 410 - 469 °F | |
Ineos Nova Zylar® 220 High Performance Styrenic, Acrylic Copolymer
(discontinued **) Excellent moldability, High clarity, Extended toughness and elongation, meets USP XXI specification for Class VI Plastics, Property retention after gamma irradiationApplications: Display, medical de.. |
|||
Melt Temperature | 216 - 243 °C | 421 - 469 °F | Stock |
PolyOne Lubri-Tech™ AS-000/10T-2S ABS - 10% PTFE - 2% Silicone
(discontinued **) Data provided by PolyOne. |
|||
Melt Temperature | 221 - 243 °C | 430 - 469 °F | Stock |
PolyOne Edgetek® AS-1000 SD Unreinforced ABS - Antistatic Protection
(discontinued **) Data provided by PolyOne. |
|||
Melt Temperature | 221 - 243 °C | 430 - 469 °F | Stock |
PolyOne Stat-Tech™ AS-15GF/000 SD ABS - 15% Glass Fiber Reinforced - Antistatic Protection
(discontinued **)& Data provided by PolyOne. |
|||
Melt Temperature | 204 - 243 °C | 399 - 469 °F | |
Ineos ABS Centrex® 401 AES Extrusion
(discontinued **) Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with |
|||
Melt Temperature | 232 - 243 °C | 450 - 469 °F | Injection Molding |
Ineos ABS Lustran® 720 ABS, Molding Grade Lustran® ABS 720 resin is a black, virgin injection molding grade of ABS (acrylonitrile butadiene styrene). It is supplied as salt-and-pepper pellets with color concentrate 901802 black. Designed.. |
|||
Melt Temperature | 232 - 243 °C | 450 - 469 °F | Injection Molding |
Ineos ABS Lustran® 750 ABS, Molding Grade Lustran® 750 resin is a black, virgin injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It is designed for molded drain, waste, and vent (DWV) fittings. Lustran® 750 (901802 bl.. |
|||
Melt Temperature | 232 - 243 °C | 450 - 469 °F | Injection Molding |
Ineos ABS Lustran® ABS 241 ABS, Blending Grade Lustran® ABS 241 resin is a natural, stiffer-flow, virgin blending grade of ABS (acrylonitrile butadiene styrene). It is designed for use with other high-impact ABS resins for drain, waste, and v.. |
|||
Melt Temperature | 232 - 243 °C | 450 - 469 °F | Extrusion |
Ineos ABS Lustran® ABS 241 ABS, Blending Grade Lustran® ABS 241 resin is a natural, stiffer-flow, virgin blending grade of ABS (acrylonitrile butadiene styrene). It is designed for use with other high-impact ABS resins for drain, waste, and v.. |
|||
Melt Temperature | 221 - 243 °C | 430 - 469 °F | |
Ineos Nova Styrosun® 3600 Weather Resistant High Impact Styrenic Polymer Features: Outdoor weatherablePhysical property retention after UV exposurePaintable and printableExcellent toughness Can be injection molded or co-extruded Easy to process, no drying required Appli.. |
|||
Melt Temperature | 221 - 243 °C | 430 - 469 °F | |
Ineos Nova Styrosun® 6600 Weather Resistant High Impact Styrenic Polymer Features: Outdoor weatherablePhysical property retention after UV exposurePaintable and printableExcellent toughness Can be injection molded or co-extruded Easy to process, no drying required Appli.. |
|||
Melt Temperature | 232 - 243 °C | 450 - 469 °F | Injection Molding |
Ineos ABS Lustran® 261 ABS, High-Impact Blending Grade Lustran® ABS 261 resin is a natural, stiffer-flow, virgin blending grade of ABS (acrylonitrile butadiene styrene). It is designed for use with other high-impact ABS resins for drain, waste, and v.. |
|||
Melt Temperature | 232 - 243 °C | 450 - 469 °F | Extrusion |
Ineos ABS Lustran® 261 ABS, High-Impact Blending Grade Lustran® ABS 261 resin is a natural, stiffer-flow, virgin blending grade of ABS (acrylonitrile butadiene styrene). It is designed for use with other high-impact ABS resins for drain, waste, and v.. |
|||
Melt Temperature | 210 - 243 °C | 410 - 469 °F | |
Styrolution NAS® 36 UV Stabilized Acrylic Copolymer Features:Sparkling clarity Excellent indoor light stability Styrenic processing advantages Scratch resistant Enhanced mold releaseApplications:Appliances Point-of -Purchase Displays Toys Office Acce.. |
|||
Melt Temperature | 210 - 243 °C | 410 - 469 °F | |
Styrolution NAS® 90 High Performance Styrenic NAS® 90 has sparkling clarity, improved toughness, and good scratch resistance. This easily processed copolymer blends well with clear impact modifiers. It meets USP XXIII Spec. of Class VI Pla.. |
|||
Melt Temperature | 221 - 243 °C | 430 - 469 °F | |
Lubrizol Isoplast® 2530 Engineering Thermoplastic Polyurethane Resin for Medical Applications Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Melt Temperature | 210 - 243 °C | 410 - 469 °F | |
Styrolution NAS® 21 Acrylic Copolymer Features:Sparkling clarity Scratch resistant Can be blended with K-Resin at any level to modify flexibility, surface hardness, heat distortion temperatures, etc. Styrenic processing advantages Gamma.. |
|||
Melt Temperature | 210 - 243 °C | 410 - 469 °F | |
Styrolution NAS® 30 Series High Performance Styrenic It has sparkling clarity and good scratch resistance. This easily processed copolymer blends well with K-Resin® to modify flexibility, surface hardness, and HDT. It meets USP XXIII Spec. of Class.. |
|||
Melt Temperature | 210 - 243 °C | 410 - 469 °F | |
Ineos Nova Zyntar® 7041 High Performance Flame Retardant Polystyrene
(discontinued **) Non-Decabromodiphenyl Oxide, High flow, Ease of processingApplications: Electronics, TelevisionsThis is an impact grade of polystyrene containing chemicals to increase resistance to ignition in labo.. |
|||
Melt Temperature | 221 - 243 °C | 430 - 469 °F | |
Ineos Nova Zyntar® 779 High Performance Flame Retardant Polystyrene
(discontinued **) Non-Decabromodiphenyl Oxide, Color stable, Custom colorsApplications: Injection molding, Alternative to flame retardant ABS, Copiers, Computer monitors, Office equipmentThis is an impact grade of po.. |
|||
Melt Temperature | 221 - 243 °C | 430 - 469 °F | |
Ineos Nova Zyntar® 702 High Performance Flame Retardant Polystyrene
(discontinued **) Custom ColorsApplications: Injection molding, Gas-assist injection moldingThis is an impact grade of polystyrene containing chemicals to increase resistance to ignition in laboratory flame tests. L.. |
|||
Melt Temperature | 221 - 243 °C | 430 - 469 °F | |
Ineos Nova Zyntar® 351 High Performance Flame Retardant Polystyrene
(discontinued **) High Vicat and heat reflection temperature, Custom colorsApplications: Injection molding, Gas-assist injection molding, Structural foam, TV cabinets, Electronic enclosuresThis is an impact grade of .. |
|||
Melt Temperature | 221 - 243 °C | 430 - 469 °F | |
Ineos Nova Zyntar® 707 High Performance Flame Retardant Polystyrene
(discontinued **) Non-Decabromodiphenyl Oxide, High flow, Ease of processingApplications: Electronics, TelevisionsThis is an impact grade of polystyrene containing chemicals to increase resistance to ignition in labo.. |