PolyOne Edgetek® AS-1000 SD Unreinforced ABS - Antistatic Protection  (discontinued **)

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® AS-1000 SD Unreinforced ABS - Antistatic Protection  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by PolyOne.
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0050 cm/cm

@Thickness 3.17 mm
0.0050 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 40.0 MPa
5800 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Tensile Modulus 2.40 GPa
348 ksi
ASTM D638
Izod Impact, Notched 1.33 J/cm

@Thickness 6.35 mm
2.49 ft-lb/in

@Thickness 0.250 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 93.0 °C
199 °F
ASTM D648
Electrical Properties Metric English Comments
Surface Resistance 1.00e+9 - 1.00e+13 ohm
1.00e+9 - 1.00e+13 ohm
ASTM D257
Processing Properties Metric English Comments
Melt Temperature 221 - 243 °C
430 - 469 °F
Stock
Mold Temperature 27.0 - 49.0 °C
80.6 - 120 °F
Drying Temperature 82.0 °C
180 °F