Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 288 - 316 °C | 550 - 601 °F | |
PolyOne LubriOne™ PC-000/05T-2S Polycarbonate (PC) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Melt Temperature | 288 - 316 °C | 550 - 601 °F | |
PolyOne LubriOne™ PC-000/10T Polycarbonate (PC) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Melt Temperature | 288 - 316 °C | 550 - 601 °F | |
PolyOne LubriOne™ PC-000/15T Polycarbonate (PC) Information provided by PolyOne |
|||
Melt Temperature | 288 - 316 °C | 550 - 601 °F | |
PolyOne LubriOne™ PC-000/20T Polycarbonate (PC) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Melt Temperature | 288 - 316 °C | 550 - 601 °F | |
PolyOne LubriOne™ PC-20GF/15T Polycarbonate (PC) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Melt Temperature | 299 - 316 °C | 570 - 601 °F | |
PolyOne Stat-Tech™ LC-20NCF/000 V3 Natural Liquid Crystal Polymer (LCP) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Melt Temperature | 288 - 316 °C | 550 - 601 °F | |
PolyOne Edgetek® PC-20GF/000 Polycarbonate (PC) Information provided by PolyOne |
|||
Melt Temperature | 288 - 316 °C | 550 - 601 °F | |
PolyOne LubriOne™ PC-10CF/15T Black Polycarbonate (PC) Information provided by PolyOne |
|||
Melt Temperature | 249 - 316 °C | 480 - 601 °F | Average value: 284 °C Grade Count:7 |
Overview of materials for Polyphenylene Ether, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, PTFE Filled". Each property range of values reported is minimum and maximum values .. |
|||
Melt Temperature | 288 - 316 °C | 550 - 601 °F | Average value: 303 °C Grade Count:3 |
Overview of materials for Polycarbonate, Carbon + Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon + Glass Fiber Reinforced". Each property range of values reported is minimum and m.. |
|||
Melt Temperature | 271 - 316 °C | 520 - 601 °F | |
Solvay Specialty Polymers Mindel® B-322 Polysulfone, Modified (PSU, Modified)
(discontinued **) Mindel B-322 is a glass filled, modified polysulfone developed specifically for molded electrical connector applications requiring excellent dimensional stability and resistance to warpage. This mat.. |
|||
Melt Temperature | 288 - 316 °C | 550 - 601 °F | Stock |
PolyOne Edgetek® LCP-15GF/000 Liquid Crystal Polymer - 15% Fiber Glass
(discontinued **) Data provided by PolyOne. |
|||
Melt Temperature | 288 - 316 °C | 550 - 601 °F | Stock |
PolyOne Edgetek® LCP-30CF/000 Liquid Crystal Polymer - 30% Carbon Fiber
(discontinued **) Data provided by PolyOne. |
|||
Melt Temperature | 288 - 316 °C | 550 - 601 °F | |
Styron EMERGEâ„¢ 4530-10 Polycarbonate EMERGEâ„¢ PC 4530-10 advanced resin is a general purpose polycarbonate resin offering ignition resistance, heat resistance and excellent toughness. Applications: Consumer Electronics and Inform.. |
|||
Melt Temperature | 288 - 316 °C | 550 - 601 °F | |
Styron EMERGEâ„¢ 4702-15 Polycarbonate EMERGEâ„¢ PC 4702-15 advanced resin is formulated with 20% glass fiber and a proprietary flame retardant package. It provides good ignition resistance, rigidity, dimension stability and heat res.. |
|||
Melt Temperature | 288 - 316 °C | 550 - 601 °F | |
Styron EMERGEâ„¢ 4702-8 Polycarbonate EMERGEâ„¢ PC 4702-8 advanced resin is formulated with 20% glass fiber and a proprietary flame retardant package. It provides good ignition resistance, rigidity, dimension stability and heat resi.. |
|||
Melt Temperature | 288 - 316 °C | 550 - 601 °F | |
Styron EMERGEâ„¢ 4731-13 Polycarbonate EMERGEâ„¢ PC 4731-13 advanced resin is formulated with 10% glass fiber and has an f1 rating by Underwriters Laboratories Inc. It provides good ignition resistance, rigidity, dimension stability .. |
|||
Melt Temperature | 288 - 316 °C | 550 - 601 °F | |
Styron EMERGEâ„¢ 4731-8 Polycarbonate EMERGEâ„¢ PC 4702-15 advanced resin is formulated with 10% glass fiber and has an f1 rating by Underwriters Laboratories Inc. It provides good ignition resistance, rigidity, dimension stability .. |
|||
Melt Temperature | 288 - 316 °C | 550 - 601 °F | |
Styron EMERGEâ„¢ 4800-10 Polycarbonate EMERGEâ„¢ 4800-10 advanced resin provides superior ignition resistance in opaque, injection molding applications. Physical properties and process-ability are outstanding for this class of polyca.. |
|||
Melt Temperature | 288 - 316 °C | 550 - 601 °F | |
Styron EMERGEâ„¢ 4850-10 Polycarbonate EMERGEâ„¢ 4850-10 advanced resin provides superior ignition resistance and ultraviolet light resistance in opaque applications. It has an f1 rating by Underwriters Laboratories Inc. Physical pr.. |
|||
Melt Temperature | 288 - 316 °C | 550 - 601 °F | |
Styron EMERGEâ„¢ 4510-10 Polycarbonate EMERGEâ„¢ PC 4510-10 advanced resin is a general purpose polycarbonate resin offering ignition resistance, heat resistance and excellent toughness. Applications: Consumer Electronics and Inform.. |
|||
Melt Temperature | 288 - 316 °C | 550 - 601 °F | |
Styron EMERGEâ„¢ 4701-13 Polycarbonate EMERGEâ„¢ PC 4701-13 advanced resin is formulated with 10% glass fiber and a proprietary flame retardant package. It provides good ignition resistance, rigidity, dimension stability and heat res.. |
|||
Melt Temperature | 260 - 316 °C | 500 - 601 °F | Average value: 284 °C Grade Count:9 |
Overview of materials for Polycarbonate, Glass Fiber & Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber & Bead Filled". Each property range of values reported is minimum and maximum.. |
|||
Melt Temperature | 288 - 316 °C | 550 - 601 °F | Stock |
PolyOne Lubri-Tech™ SF-000/40T Polyphenylene Sulfide - 40% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Melt Temperature | 288 - 316 °C | 550 - 601 °F | Stock |
PolyOne Lubri-Tech™ MP-000/10T Modified PPO - 10% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Melt Temperature | 288 - 316 °C | 550 - 601 °F | Stock |
PolyOne Lubri-Tech™ MP-000/15T Modified PPO - 15% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Melt Temperature | 293 - 316 °C | 559 - 601 °F | Stock |
PolyOne Stat-Tech™ MP-25NCF/000 Modified PPO - 25% Nickel Coated Graphite Fiber
(discontinued **) Data provided by PolyOne. |
|||
Melt Temperature | 277 - 316 °C | 531 - 601 °F | Stock |
PolyOne Lubri-Tech™ MP-30GF/15T Modified PPO - 30% Glass Fiber - 15% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Melt Temperature | 243 - 316 °C | 469 - 601 °F | Average value: 290 °C Grade Count:7 |
Overview of materials for Polystyrene + Polyphenylene Ether, Glass Filler This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass Filler". Each property range of values reported is minimum and .. |