Electrical Properties | Metric | English | Comments |
---|---|---|---|
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness 3.00 mm |
15 - 30 sec @Thickness 0.118 in |
UL 746 |
Polymer Resources NY6-GP2-[color]-H General Purpose Nylon 6, Nucleated, Heat Stabilized General Purpose Nylon 6, Nucleated, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness 1.50 mm |
15 - 30 sec @Thickness 0.0591 in |
PLC 3 |
PTS Tristar® PC-10R-CL(6) 6 MFI Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=2.50 mm |
15 - 30 sec @Thickness >=0.0984 in |
|
LG Chemical AF312T ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=3.00 mm |
15 - 30 sec @Thickness >=0.118 in |
|
LG Chemical ER451 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior Housing (garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemica.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=3.00 mm |
15 - 30 sec @Thickness >=0.118 in |
|
LG Chemical GPPS 15NF(I) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: Food Container, Merchandise, Artificial Woods, Refrigerator Vegetable Box, PSP, Sheet, Film, etc.CAS: 9003-53-6-5In.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=1.50 mm |
15 - 30 sec @Thickness >=0.0591 in |
|
LG Chemical HF380I ABS, High Flow Feature: Injection Molding, High Flow, Good PaintabilityApplication: Painting Products of Motor Cycle)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=3.00 mm |
15 - 30 sec @Thickness >=0.118 in |
|
LG Chemical HI100K ABS, High Impact Feature: Injection Molding, High Impact, Good ProcessingApplication: Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=3.00 mm |
15 - 30 sec @Thickness >=0.118 in |
|
LG Chemical HIPS 403AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 21850-44-2 and 1309-64-4Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=1.50 mm |
15 - 30 sec @Thickness >=0.0591 in |
|
LG Chemical KEYFLEX BT 1040D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=1.50 mm |
15 - 30 sec @Thickness >=0.0591 in |
|
LG Chemical LUMID GP2130B(W) PA66+GF13%, General Purpose Feature: Injection Molding, PA66+GF13%, General PurposeApplication: Valve CoversCAS No. 32131-17-2, 65997-17-3 and 9010-79-9Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=3.00 mm |
15 - 30 sec @Thickness >=0.118 in |
|
LG Chemical LUMID GP2330B(W) PA66+GF33%, General Purpose Feature: Injection Molding, PA6+GF33%, General PurposeApplication: Automotive (Air Intake Manifold, Cylinder Head Cover)CAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=2.00 mm |
15 - 30 sec @Thickness >=0.0787 in |
|
LG Chemical Lupoy NF1005F 03R Polycarbonate Resin Description: LUPOY NF 1005F03R, eco-friendly UL94 V0/1.5 mm, is designed for extrusion products. It combines an excellent physical property balance of heat resistance, transparency and impact streng.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=2.00 mm |
15 - 30 sec @Thickness >=0.0787 in |
|
LG Chemical Lupoy NF1009F 08R Polycarbonate Resin Description: LUPOY NF 1009F08R, eco-friendly UL94 V0/2.0 mm, is designed for extrusion and injection molding products. It combines an excellent physical property balance of heat resistance, transpar.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=1.70 mm |
15 - 30 sec @Thickness >=0.0669 in |
|
LG Chemical LUSEP GP2400 PPS+GF40%, General Purpose Feature: Injection Molding, PPS+GF40%, General PurposeApplication: Pump Units, Motor Units, etc.CAS No. 25212-74-2 and 65997-17-3Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=3.00 mm |
15 - 30 sec @Thickness >=0.118 in |
|
LG Chemical MP211 ABS, Low Gloss, Metal Plating Feature: Injection Molding, High Flow, Metal PlatingApplication: Decorative Parts (Home Appliance Door Handle Etc)CAS No. 9003-56-9 and 9003-54-7Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=3.00 mm |
15 - 30 sec @Thickness >=0.118 in |
|
LG Chemical XR401T ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746A |
Ascend Performance Materials Vydyne® 21SPC Nylon 66, DAM Vydyne® 21SPC is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding fabrication. This resin offers a well balanced combination of engineering .. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 3.00 mm |
15 - 29 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 21SPF BLK Nylon 66, Conditioned Vydyne® 21SPF BLK is a, general-purpose PA66 resin used for extrusion-compounding. Available in black, it is designed principally for injection-molding fabrication. This grade offers a well-balance.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness 1.50 mm |
15 - 30 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 21SPF Nylon 66, General Purpose, High Productivity, DAM Vydyne® 21SPF is general-purpose PA66 resin. Available in natural, it is designed principally for injection-molding fabrication. This grade offers a well-balanced combination of engineering propert.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 3.00 mm |
15 - 29 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 47H BK0668 Nylon 66, Impact Modified, Heat Stabilized, DAM Vydyne® 47H BK0668 is a high-performance, medium-impact-modified, heat-stabilized grade of PA66 resin.Availability:Asia PacificEuropeNorth AmericaAdditive:Impact Modifier Features:Gasoline Resistan.. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness 3.00 mm |
15 - 30 sec @Thickness 0.118 in |
UL 746A |
Ascend Performance Materials Vydyne® ECO-315 Nylon 66/6, non-halogenated, ignition resistant, DAM Vydyne® ECO315 is non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and has an Underwriters Laboratories UL 94 fla.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R513H Black Nylon 66, 13% Glass Reinforced, DAM Vydyne® R513H Black is general-purpose, 13% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is an injection-molding grade that is lubricated for machine feed, flow, and m.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R515H Nylon 66, 15% Glass Reinforced, DAM Vydyne® R515H is general-purpose, heat-stabilized, hydrolysis-resistant, 15% glass-fiber reinforced PA66 resin. Available in natural it is specifically designed to maximize the retention of physica.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R530H BK0201 Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H BK0201 is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in black, it is specifically designed to maximize the retention of p.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R530H Black Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H Black is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. It is specifically designed to maximize the retention of physical properties wh.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R533H NT Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H NT is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties .. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746A |
Ascend Performance Materials Vydyne® 66B Nylon 66, General Purpose, high viscosity, DAM Vydyne® 66B is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66B resin offers high strength, .. |
|||
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness 1.50 mm |
15 - 30 sec @Thickness 0.0591 in |
UL 746B |
Ascend Performance Materials Vydyne® 50BWFS Nylon 66, Dry as Molded Vydyne® 50BWFS is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a highviscosity resin. This resin offers a well-balanced com.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R533H BK0201 Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H BK0201 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie.. |
|||
Hot Wire Ignition, HWI | 15 - 29 sec @Thickness 1.50 mm |
15 - 29 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 25WSP Nylon 66, Dry as Molded Vydyne® 25WSP is a black, weather-resistant injection-molding grade PA66 resin. This resin offers a well-balanced combination of engineering properties characterized by high strength, rigidity, goo.. |