Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ascend Performance Materials Vydyne® R513H Black Nylon 66, 13% Glass Reinforced, DAM

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 10% Glass Fiber Filled
Manufacturer Ascend Performance Materials (formerly Solutia)
Trade Name VYDYNE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ascend Performance Materials Vydyne® R513H Black Nylon 66, 13% Glass Reinforced, DAM.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Vydyne® R513H Black is general-purpose, 13% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is an injection-molding grade that is lubricated for machine feed, flow, and mold release. Glass-reinforced Vydyne resins provide a higher heat distortion temperature, better resistance to creep, high impact, and better dimensional stability when compared with unreinforced PA66. This product has good chemical resistance to a broad range of chemicals, including many aliphatic and aromatic hydrocarbons found in most solvents, gasoline, hydraulic fluids, greases and machine oils. Vydyne R513 Black has tensile strength and modulus properties just below aluminum and zinc and can replace these metals in numerous applications due to an excellent balance of properties. Reduction in production costs, energy consumption and part weight are key advantages of Vydyne glass-reinforced PA66 resins over aluminum and/or zinc die-cast parts. Vydyne R513 Black is heat-stabilized and formulated to minimize the oxidative and thermal degradation of the PA66 polymer when exposed to elevated temperatures for extended periods of time. Vydyne R513H Black provides improved retention of physical properties under exposure to long-term heat. The continuous operating use temperature is 275°F, with short-term peak temperatures as high as 475°F. Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 13% Filler by WeightAdditive:Heat StabilizerLubricant Features: Gasoline ResistanceGood Chemical ResistanceGood FlowGood Mold ReleaseGrease ResistantHeat StabilizedHigh RigidityHigh StrengthLubricatedOil ResistantSolvent ResistantUses: Automotive Under the Hood GearsHousings Power/Other ToolsAppearance: BlackForms: PelletsProcessing Method: Injection MoldingInformation provided by Ascend Performance Materials.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ISO 1183
Water Absorption 1.0 %

@Time 86400 sec
1.0 %

@Time 24.0 hour
ISO 62
Moisture Absorption at Equilibrium 2.2 %
2.2 %
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0050 cm/cm

@Diameter 2.00 mm
0.0050 in/in

@Diameter 0.0787 in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.010 cm/cm

@Diameter 2.00 mm
0.010 in/in

@Diameter 0.0787 in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 115 MPa
16700 psi
ISO 527-2
Elongation at Break 3.0 %
3.0 %
ISO 527-2
Tensile Modulus 6.20 GPa
899 ksi
ISO 527-2
Flexural Strength 165 MPa
23900 psi
ISO 178
Flexural Modulus 5.20 GPa
754 ksi
ISO 178
Poissons Ratio 0.40
0.40
ISO 527
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature -30.0 °C
2.38 ft-lb/in²

@Temperature -22.0 °F
ISO 180
5.10 kJ/m²

@Temperature 23.0 °C
2.43 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Charpy Impact Unnotched 3.10 J/cm²

@Temperature -30.0 °C
14.8 ft-lb/in²

@Temperature -22.0 °F
ISO 179
3.80 J/cm²

@Temperature 23.0 °C
18.1 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Charpy Impact, Notched 0.600 J/cm²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
ISO 179
0.600 J/cm²

@Temperature 23.0 °C
2.86 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 3.00 µm/m-°C

@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
1.67 µin/in-°F

@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
ISO 11359-2
CTE, linear, Transverse to Flow 11.0 µm/m-°C

@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
6.11 µin/in-°F

@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
ISO 11359-2
Melting Point 260 °C
500 °F
ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 258 °C
496 °F
Unannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 240 °C
464 °F
Unannealed; ISO 75-2/A
UL RTI, Electrical 140 °C

@Thickness 0.750 mm
284 °F

@Thickness 0.0295 in
UL 746
140 °C

@Thickness 1.50 mm
284 °F

@Thickness 0.0591 in
UL 746
140 °C

@Thickness 3.00 mm
284 °F

@Thickness 0.118 in
UL 746
UL RTI, Mechanical with Impact 120 °C

@Thickness 0.750 mm
248 °F

@Thickness 0.0295 in
UL 746
120 °C

@Thickness 1.50 mm
248 °F

@Thickness 0.0591 in
UL 746
120 °C

@Thickness 3.00 mm
248 °F

@Thickness 0.118 in
UL 746
UL RTI, Mechanical without Impact 125 °C

@Thickness 0.750 mm
257 °F

@Thickness 0.0295 in
UL 746
140 °C

@Thickness 1.50 mm
284 °F

@Thickness 0.0591 in
UL 746
140 °C

@Thickness 3.00 mm
284 °F

@Thickness 0.118 in
UL 746
Flammability, UL94 HB

@Thickness 0.750 mm
HB

@Thickness 0.0295 in
HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Oxygen Index 25 %
25 %
ISO 4589-2
Glow Wire Test 675 °C

@Thickness 0.750 mm
1250 °F

@Thickness 0.0295 in
Flammability Index; IEC 60695-2-12
675 °C

@Thickness 1.50 mm
1250 °F

@Thickness 0.0591 in
Flammability Index; IEC 60695-2-12
675 °C

@Thickness 3.00 mm
1250 °F

@Thickness 0.118 in
Flammability Index; IEC 60695-2-12
700 °C

@Thickness 0.750 mm
1290 °F

@Thickness 0.0295 in
Ignition Temperature; IEC 60695-2-13
700 °C

@Thickness 1.50 mm
1290 °F

@Thickness 0.0591 in
Ignition Temperature; IEC 60695-2-13
700 °C

@Thickness 3.00 mm
1290 °F

@Thickness 0.118 in
Ignition Temperature; IEC 60695-2-13
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm

@Thickness 0.750 mm
1.00e+13 ohm-cm

@Thickness 0.0295 in
IEC 60093
Dielectric Strength 20.0 kV/mm

@Thickness 1.00 mm
508 kV/in

@Thickness 0.0394 in
IEC 60243
Arc Resistance 60 - 119 sec

@Thickness 3.00 mm
60 - 119 sec

@Thickness 0.118 in
ASTM D495
Comparative Tracking Index 250 - 399 V

@Thickness 3.00 mm
250 - 399 V

@Thickness 0.118 in
IEC 60112
Hot Wire Ignition, HWI 7.0 - 14 sec

@Thickness 0.750 mm
7.0 - 14 sec

@Thickness 0.0295 in
UL 746
7.0 - 14 sec

@Thickness 3.00 mm
7.0 - 14 sec

@Thickness 0.118 in
UL 746
15 - 29 sec

@Thickness 1.50 mm
15 - 29 sec

@Thickness 0.0591 in
UL 746
High Amp Arc Ignition, HAI >= 120 arcs

@Thickness 0.750 mm
>= 120 arcs

@Thickness 0.0295 in
UL 746
>= 120 arcs

@Thickness 1.50 mm
>= 120 arcs

@Thickness 0.0591 in
UL 746
>= 120 arcs

@Thickness 3.00 mm
>= 120 arcs

@Thickness 0.118 in
UL 746
High Voltage Arc-Tracking Rate, HVTR 10.1 - 25.4 mm/min
0.398 - 1.00 in/min
UL 746
Processing Properties Metric English Comments
Rear Barrel Temperature 280 - 310 °C
536 - 590 °F
Middle Barrel Temperature 280 - 310 °C
536 - 590 °F
Front Barrel Temperature 280 - 310 °C
536 - 590 °F
Nozzle Temperature 280 - 310 °C
536 - 590 °F
Melt Temperature 285 - 305 °C
545 - 581 °F
Mold Temperature 65.0 - 95.0 °C
149 - 203 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 4.00 hour
4.00 hour
Descriptive Properties Value Comments
Suggested Max Regrind 25 %