Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
RTP Company RTP 1300 AR 15 TFE 10 Polyphenylene Sulfide (PPS) Aramid Fiber 15% - PTFE 10%
Aramid Fiber 15% - PTFE 10%Comments:Aramid FiberPTFE LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provi.. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
RTP Company RTP 1301 L Polyphenylene Sulfide (PPS) Glass Fiber 10% - Lubricated
(discontin Glass Fiber 10% - LubricatedComments:Glass FiberLubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided b.. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
PolyOne Lubri-Tech™ PS-000/15T-2S Polyester (PBT) - 15% PTFE Lubricated - 2% Silicone Lubricated
(discontinue Data provided by PolyOne. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
RTP Company RTP 2200 AR 35 Polyetheretherketone (PEEK) Aramid Fiber 35%
(discontinued **)& Aramid Fiber 35%Comments:Aramid FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data fo.. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Amodel® A-1115 HS Polyphthalamide (PPA) Resin, 15% Glass Reinforced, Dry As Molded
AMODEL A-1115 HS resin is a 15% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, and high tensile strength. Excellent cre.. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
RTP Company RTP 2200 LF Z Polyetheretherketone (PEEK) Low Flow - FDA Type
(discontinued ** Low Flow - FDA TypeComments:Low FlowFDA CompliantUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Com.. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
RTP Company RTP 2205 TFE 10 Polyetheretherketone (PEEK) Glass Fiber 30% - PTFE 10%
(discon Glass Fiber 30% - PTFE 10%Comments:Glass FiberPTFE LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provide.. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
RTP Company RTP 1110 Polyethylene Terephthalate (PET) Glass Fiber 55%
(discontinued **)< Glass Fiber 55%Comments:Glass FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for .. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
RTP Company RTP 1105 L Polyethylene Terephthalate (PET) Glass Fiber 30% - Lubricated
(disc Glass Fiber 30% - LubricatedComments:Glass FiberLubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided b.. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
RTP Company RTP 1400 A-100 Polyethersulfone (PES) Base Resin
(discontinued **) Base ResinComments:UnfilledUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for this pro.. |
|||
Electrical Resistivity | 1.00e+16 - 1.00e+17 ohm-cm | 1.00e+16 - 1.00e+17 ohm-cm | Average value: 5.50e+16 ohm-cm Grade Count:6 |
Overview of materials for ABS/Polyester Alloy + GF This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy + GF". Each property range of values reported is minimum and maximum values of appro.. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
Covestro Makrolon® SF-800 Polycarbonate, Structural Foam
(discontinued **) Properties based on foam density of 0.90 g/cc.Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially.. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
RTP Company RTP 2100 TFE 25 Polyetherimide (PEI) PTFE 25%
(discontinued **) PTFE 25%Comments:PTFE LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for thi.. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | |
Idemitsu Kosan Xarec® EA 537 SPS, 30% Glass Filled Crystalline Polymer, Glass Filled, Ignition Resistant, Impact Modified. Used in Electronic and Electrical applications |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
Borealis Borstar® HE6067 Black Bimodal HD Polyethylene Compound for Jacketing of Communication and Power Cables Borstar HE6067 is a black, bimodal, co-polymer high density polyethylene (HDPE) compound produced according to the bimodal Borstar process. It is characterized by its balanced properties important .. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | |
Goodfellow Polyhydroxybutyrate / Polyhydroxyvalerate (PHB 92/PHV 8) See also PHB. PHB/PHV copolymers are used in preference to PHB homopolymer for general purposes (e.g. molding containers) in order to obtain a better balance of stiffness and toughness. PHV contents.. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
Toyobo Vylopet® EMC120S Glass Reinforced Polyester, Standard Grade Key Feature: Flame retardant V-0 UL-94 classApplications: Electric and electronic componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strengt.. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
Toyobo Vylopet® EMC330K Glass Reinforced Polyester, Easy Molding Grade HB UL-94 classApplications: General and high rigidity componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and tracking resistance, c.. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
Borealis SuperTR™ LE4212 Scorch Retardant, Crosslinkable Polyethylene, Water Tree Retardant Insulation for Me Power Cables SuperTR LE4212 is a natural, crosslinkable low density polyethylene compound, which has water tree retardant and scorch retardant properties.SuperTR LE4212 has been specifically developed as a scorc.. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
Celanese Fortron® 1140 L7 Polyphenylene Sulfide (PPS), 40% Glass Fiber Excellent flow, fast cycleInformation provided by Celanese Corporation. |
|||
Electrical Resistivity | >= 1.00e+16 ohm-cm | >= 1.00e+16 ohm-cm | ASTM D257 |
Celanese Celanex® 5300 Polyester (PBT), 30% Glass-Fiber Good surface smoothnessInformation provided by Celanese Corporation. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
Borealis Visico™ LE4423/LE4460/LE4432 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Installation Visico LE4423/LE4460/LE4432 is a black, halogen-based flame retardant, moisture-induced crosslinking polyethylene compound that is designed for use as low wire insulation and jacketing. The combina.. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
Chevron Phillips Ryton® PR09-60 Polyphenylene Sulfide Compound
(discontinued **) Polyphenylene Sulfide CompoundRyton® PR09-60 is pelletized unfilled high molecular weight polyphenylene sulfide resin suitable for extrusion or injection molding.Comments: Test specimen molding con.. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
RTP Company RTP 1307 TFE 20 Polyphenylene Sulfide (PPS) Glass Fiber 40% - PTFE 20%
(discon Glass Fiber 40% - PTFE 20%Comments:Glass FiberPTFE LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provide.. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
RTP Company RTP 1405 B Polyethersulfone (PES) Glass Fiber 30%
(discontinued **) Glass Fiber 30%Comments:Glass FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for .. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
RTP Company RTP 1403 N Z Polyethersulfone (PES) Glass Fiber 20% - FDA Type - High Viscosity
&nbs Glass Fiber 20% - FDA Type - High ViscosityComments:Glass FiberFDA CompliantHigh ViscosityUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect p.. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
RTP Company RTP 1805A Polycarbonate/Acrylic Alloy (PC/PMMA) Glass Fiber 30%
(discontinued Glass Fiber 30%Comments:Glass FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for .. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
Celanese Fortron® 1140 L6 Polyphenylene Sulfide (PPS), 40% Glass Fiber Good flowInformation provided by Celanese Corporation. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
Celanese Fortron® 6165 A6 Polyphenylene Sulfide (PPS), 65% Mineral/Glass-Fiber Good flowInformation provided by Celanese Corporation. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | Average value: 1.00e+16 ohm-cm Grade Count:5 |
Overview of materials for Polypropylene with Glass Fiber + PTFE This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + PTFE". Each property range of values reported is minimum and maximum va.. |