Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Wire/Cable Grade
Manufacturer Borealis
Trade Name Visico™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Visico™ LE4423/LE4460/LE4437 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Installation.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Visico LE4423/LE4460/LE4437 is a natural, halogen-based, moisture-induced crosslinking polyethylene compound that is designed for use as low voltage wire insulation and jacketing. The combination of the Visico LE4423 base resin, along with the LE4460 brominated flame retardant masterbatch and the LE4437 tin catalyst masterbatch provides a highly scorch retardant compound with excellent thermal stability and good flame properties. LE4423/LE4460/LE4437 contains a patented scorch retardant additive (SRA) that increases the processing window for a moisture crosslinking compound and minimizes the tendency for premature crosslinking in the extruder, head or die. A finished compound that is composed of 75 parts LE4423 mixed with 20 parts of LE4460 and 5 parts of LE4437 is recognized by Underwriters Laboratories as Visico Horizontal.LE4422/LE4460/LE4437 is recommended for use as insulation for low voltage control cables and power cables up to 6 kV in rating.Information provided by the Manufacturer.
Physical Properties Metric English Comments
Density 0.923 g/cc
0.0333 lb/in³
LE 4423; ASTM D792
0.941 g/cc
0.0340 lb/in³
LE 4437; ASTM D792
2.00 g/cc
0.0723 lb/in³
LE 4460; ASTM D792
Melt Flow 0.90 g/10 min
0.90 g/10 min
LE 4423; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 14.58 MPa
>= 2115 psi
Heat Aging (7 days at 121°C); ASTM D412
16.2 MPa
2350 psi
ASTM D412
Elongation at Break <= 50 %
<= 50 %
Hot Creep Test (150°C, .2 MPa); ICEA T-28-562
270 %
270 %
Heat Aging (7 days at 121°C); ASTM D412
300 %
300 %
ASTM D412
Tensile Set <= 5.0 %
<= 5.0 %
Hot Creep Test (150°C,.2 MPa); ICE T-28-562
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Constant 2.3

@Frequency 60 Hz
2.3

@Frequency 60 Hz
ASTM D150
Dielectric Strength >= 21.7 kV/mm
>= 550 kV/in
ASTM D149
Dissipation Factor 0.00050

@Frequency 60 Hz
0.00050

@Frequency 60 Hz
ASTM D150
Processing Properties Metric English Comments
Middle Barrel Temperature >= 163 °C
>= 325 °F
Front Barrel Temperature >= 146 °C
>= 295 °F
Die Temperature >= 177 °C
>= 350 °F
Head Temperature >= 177 °C
>= 351 °F
Descriptive Properties Value Comments
Horizontal Flame Test Pass
14AWG-30mil, UL 1581