Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
RTP Company RTP 1300 MG 50 SI 2 Polyphenylene Sulfide (PPS) Milled Glass 50% - Silicone 2%
  Milled Glass 50% - Silicone 2%Comments:Milled GlassSilicone LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Informatio.. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
RTP Company RTP 2200 LF Z Polyetheretherketone (PEEK) Low Flow - FDA Type
(discontinued ** Low Flow - FDA TypeComments:Low FlowFDA CompliantUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Com.. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
RTP Company RTP 3803 Polyaryletherketone (PAEK), Glass Fiber 20%
(discontinued **) Data is for injection molded specimens and was provided by the manufacturer, RTP Company.This product has been discontinued, please contact RTP Company regarding alternate grades. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
RTP Company RTP 3805 Polyaryletherketone (PAEK), Glass Fiber 30%
(discontinued **) Data is for injection molded specimens and was provided by the manufacturer, RTP Company.This product has been discontinued, please contact RTP Company regarding alternate grades. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
RTP Company RTP 1105 Polyethylene Terephthalate (PET) Glass Fiber 30%
(discontinued **)< Glass Fiber 30%Comments:Glass FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for .. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
RTP Company RTP 3807 Polyaryletherketone (PAEK), Glass Fiber 40%
(discontinued **) Data is for injection molded specimens and was provided by the manufacturer, RTP Company.This product has been discontinued, please contact RTP Company regarding alternate grades. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
RTP Company RTP 1107 Polyethylene Terephthalate (PET) Glass Fiber 40%
(discontinued **)< Glass Fiber 40%Comments:Glass FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for .. |
|||
Electrical Resistivity | 1e+05 - 1.00e+16 ohm-cm | 1e+05 - 1.00e+16 ohm-cm | Average value: 8.27e+15 ohm-cm Grade Count:53 |
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a.. |
|||
Electrical Resistivity | >= 1.00e+16 ohm-cm | >= 1.00e+16 ohm-cm | ASTM D257 |
Covestro Apec® DP9-9333 High-Heat Polycarbonate, General Purpose, UV-Stabilized
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Electrical Resistivity | >= 1.00e+16 ohm-cm | >= 1.00e+16 ohm-cm | ASTM D257 |
Covestro Apec® DP9-9343 High-Heat Polycarbonate, UV Stabilized
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Electrical Resistivity | >= 1.00e+16 ohm-cm | >= 1.00e+16 ohm-cm | ASTM D257 |
Covestro Apec® DP9-9354T High-Heat Polycarbonate, Transparent, Flame-Retardant
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
RTP Company RTP 2105 HF Polyetherimide (PEI) Glass Fiber 30% - High Flow
(discontinued **) Glass Fiber 30% - High FlowComments:Glass FiberHigh FlowUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by .. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
RTP Company RTP 2105 TFE 15 Z Polyetherimide (PEI) Glass Fiber 30% - PTFE 15% - FDA Type
( Glass Fiber 30% - PTFE 15% - FDA TypeComments:Glass FiberPTFE LubricatedFDA CompliantUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect proper.. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
RTP Company RTP 2101 Z Polyetherimide (PEI) Glass Fiber 10% - FDA Type
(discontinued **)&l Glass Fiber 10% - FDA TypeComments:Glass FiberFDA CompliantUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided .. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | Average value: 1.00e+16 ohm-cm Grade Count:9 |
Overview of materials for Polypropylene with 20% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are .. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
Borealis Borcell™ HE1102 High Density Polyethylene Compound for Gas Injection of Cellular Communication Cable Insulation Borcell HE1102 is a high density polyethylene. A nucleating agent is incorporated for a uniform and closed cell structure. The components in the formulation are selected to give the lowest possibl.. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
Borealis Borstar® HE6067 Black Bimodal HD Polyethylene Compound for Jacketing of Communication and Power Cables Borstar HE6067 is a black, bimodal, co-polymer high density polyethylene (HDPE) compound produced according to the bimodal Borstar process. It is characterized by its balanced properties important .. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
Borealis SuperTR™ LE4212 Scorch Retardant, Crosslinkable Polyethylene, Water Tree Retardant Insulation for Me Power Cables SuperTR LE4212 is a natural, crosslinkable low density polyethylene compound, which has water tree retardant and scorch retardant properties.SuperTR LE4212 has been specifically developed as a scorc.. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
Toyobo Vylopet® EMC415 PET/PBT Blend Key Feature: HB UL-94 ClassApplications: accessory componentsPET/PBT blends suggested for glossy surfaces. General features of Vylopet® include heat resistance, good mechanical properties, high di.. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | IEC 112 |
Covestro Bayblend® T 45 Polycarbonate/ABS Blend High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy, good platable.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was sep.. |
|||
Electrical Resistivity | >= 1.00e+16 ohm-cm | >= 1.00e+16 ohm-cm | ASTM D257 |
Celanese Celanex® 2000 Polyester (PBT) High melt flowInformation provided by Celanese Corporation. |
|||
Electrical Resistivity | >= 1.00e+16 ohm-cm | >= 1.00e+16 ohm-cm | ASTM D257 |
Celanese Celanex® 2003 Polyester (PBT) Higher flow than 2002Information provided by Celanese Corporation. |
|||
Electrical Resistivity | >= 1.00e+16 ohm-cm | >= 1.00e+16 ohm-cm | ASTM D257 |
Chang Chun Plastic PBT4130 Fire Retardant & 30% Glass Fiber Enforced Grade PBT Information provided by Dowell Trading Company Ltd. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
RTP Company RTP 2200 GB 30 Polyetheretherketone (PEEK) Glass Bead 30%
(discontinued **)< Glass Bead 30%Comments:Glass BeadUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for th.. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
RTP Company RTP 2740S-80A Unsaturated Styrenic Elastomer (SEBS) 80 Shore A - SEBS
(discont 80 Shore A - SEBSComments:80-A DurometerUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data.. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
Chevron Phillips Ryton® PR09-60 Polyphenylene Sulfide Compound
(discontinued **) Polyphenylene Sulfide CompoundRyton® PR09-60 is pelletized unfilled high molecular weight polyphenylene sulfide resin suitable for extrusion or injection molding.Comments: Test specimen molding con.. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
RTP Company RTP 1301 TFE 5 Polyphenylene Sulfide (PPS) Glass Fiber 10% - PTFE 5%
(disconti Glass Fiber 10% - PTFE 5%Comments:Glass FiberPTFE LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided.. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
Celanese Fortron® 1140 L6 Polyphenylene Sulfide (PPS), 40% Glass Fiber Good flowInformation provided by Celanese Corporation. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
RTP Company RTP 2740U-50A Saturated Styrenic Elastomer (SBS) 50 Shore A
(discontinued **)& 50 Shore AComments:50-A DurometerUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for th.. |
|||
Electrical Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
RTP Company RTP 2740S-60A Unsaturated Styrenic Elastomer (SEBS) 60 Shore A - SEBS
(discont 60 Shore A - SEBSComments:60-A DurometerUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data.. |