Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1.00e+9 ohm | 1.00e+9 ohm | Cond. A; IPC 2.5.17.1 |
Rogers Corporation RO3210 Woven-Glass Reinforced PTFE Laminate Features and Benefits:Woven glass reinforcement - Improves rigidity for easier handlingUniform electrical and mechanical performance - ideal for complex multi-layer high frequency structuresLow diel.. |
|||
Surface Resistance | <= 1.00e+9 ohm | <= 1.00e+9 ohm | Teil 30; IEC 60093 / VDE 0303 |
Okulen® 500 PE-HMW, AST OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel.. |
|||
Surface Resistance | <= 1.00e+9 ohm | <= 1.00e+9 ohm | Teil 30; IEC 60093 / VDE 0303 |
Okulen® 500 PE-HMW, UV - stabilized OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel.. |
|||
Surface Resistance | 1.00e+9 ohm | 1.00e+9 ohm | ISO IEC 61340-5-1 |
Premix Thermoplastics PRE-ELEC® ESD 2300 PRE-ELEC ESD 2300 is a static dissipative thermoplastic compound based on PE-HD. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 2300 has been developed for mult.. |
|||
Surface Resistance | 1.00e+9 ohm | 1.00e+9 ohm | ISO IEC 61340-5-1 |
Premix Thermoplastics PRE-ELEC® ESD 5510 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 5510 is a static dissipative thermoplastic compound based on polypropylene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 5510 can be injectio.. |
|||
Surface Resistance | >= 1.00e+9 ohm | >= 1.00e+9 ohm | |
Lehmann & Voss LUVOCOM® 1105-8000 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Surface Resistance | >= 1.00e+9 ohm | >= 1.00e+9 ohm | |
Lehmann & Voss LUVOCOM® 1105-8476 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precisio.. |
|||
Surface Resistance | <= 1.00e+9 ohm | <= 1.00e+9 ohm | |
Lehmann & Voss LUVOCOM® 20-8286 Polyphthalamide, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear.. |
|||
Surface Resistance | <= 1.00e+9 ohm | <= 1.00e+9 ohm | |
Lehmann & Voss LUVOCOM® 21-7928 Polyamide 6/6T, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear.. |
|||
Surface Resistance | <= 1.00e+9 ohm | <= 1.00e+9 ohm | |
Lehmann & Voss LUVOCOM® 50/CF/5/GF/10 Polycarbonate, with carbon fiber and glass fiber Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Surface Resistance | 1e+05 - 1.00e+9 ohm | 1e+05 - 1.00e+9 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON DD200C PC (Asia Pacific) PTFE free polycarbonate compounds with ESD safety and good lubricating perfomrance , suitable for Semiconductor and Hard Disk Drive (HDD) and semicon industry. Added features of this material includ.. |
|||
Surface Resistance | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | ASTM D 257 |
SABIC Innovative Plastics LNP Stat-loy 9X05426C PMMA (Asia Pacific) LNP* Stat-loy* 9X05426C is a compound based on PMMA resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Surface Resistance | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY A3000 ABS (Asia Pacific) LNP STAT-LOY A3000 is a compound based on Acrylonitrile butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistatic. Also known as: STAT-LOY A |
|||
Surface Resistance | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY K3000SZ Acetal Copoly (Asia Pacific) LNP* Stat-loy* K3000SZ is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat. |
|||
Surface Resistance | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY N30009 PC+ABS (Europe-Africa-Middle East) LNP* STATLOY* N30009 is a compound based on PC+ABS Blend resin containing Flame Retardant. Added features include: Permanent Antistatic, Flame Retardant. |
|||
Surface Resistance | 1.00e+9 ohm | 1.00e+9 ohm | ASTM D257 |
Tipco Tipcolite® TMS 311 Phenolic Compound, Cotton, Filler & Wood Flour, having Medium Flow & High Strength Medium Flow Phenolic Compound, Reinforced with Cotton, Filler & Wood FlourApplications: Industrial & AutomotivesProcessing: Compression MoldingInformation provided by the Manufacturer, Tipco Industr.. |
|||
Surface Resistance | 1.00e+9 - 3.16e+9 ohm | 1.00e+9 - 3.16e+9 ohm | IS 3396-1979 |
Amity Thermosets ATM 125 Phenolic Molding Organic Filler, Compression Molded Characteristics:Glossy surface free of filler marks Surface good & free of flaws Good mouldabilitySurface free of filler marks even after turningGood mechanical strengthColor-black, brownSoft/medium.. |
|||
Surface Resistance | 1.00e+9 ohm | 1.00e+9 ohm | IEC 60093 |
Hexion Bakelite™ PF 4010 Phenolic Formaldehyde Resin, Improved Electrical Properties, Low Shrinkage
(disconti Glass fiber reinforced and inorganically filled molding compound. High heat resistance, reduced molding shrinkage, good chemical resistance and mechanical properties.Application areas: Switch housi.. |
|||
Surface Resistance | <= 1.00e+9 ohm | <= 1.00e+9 ohm | IEC 60093 |
CENTROPLAST CENTROSOL LF Acrylonitrile butadiene Styrene copolymer conductive CENTROSOL LF ABS has high rigidity and hardness even at low temperatures. It is permanently conductive and is used in support components for the semi-conductor industry.Information provided by CENT.. |