Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | >= 1.00e+9 ohm | >= 1.00e+9 ohm | 50% rel. humidity; ASTM D257 |
Polikim EFALON® B-60 PTFE, 60% Bronze Filled Bronze-filled Efalon® (PTFE) has better heat insulation, less thermal expansion, higher wear resistance properties and less deformation under load compared to virgin Efalon®. Applications: bearing.. |
|||
Surface Resistance | 1.00e+9 ohm | 1.00e+9 ohm | Cond. A; IPC 2.5.17.1 |
Rogers Corporation RO3206 Woven-Glass Reinforced PTFE Laminate Features and Benefits:Woven glass reinforcement - Improves rigidity for easier handlingUniform electrical and mechanical performance - ideal for complex multi-layer high frequency structuresLow diel.. |
|||
Surface Resistance | <= 1.00e+9 ohm | <= 1.00e+9 ohm | Teil 30; IEC 60093 / VDE 0303 |
Okulen® 500 PE-HMW, AST OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel.. |
|||
Surface Resistance | <= 1.00e+9 ohm | <= 1.00e+9 ohm | Teil 30; IEC 60093 / VDE 0303 |
Okulen® 500 PE-HMW, UV - stabilized OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel.. |
|||
Surface Resistance | 1.00e+9 - 1.00e+12 ohm | 1.00e+9 - 1.00e+12 ohm | At 8-20% Dosing; ISO IEC 61340-5-1 |
Premix Thermoplastics PRE-ELEC® ESD 4000 Polyolefin Compatible Dissipative Masterbatch, IDP Additive PRE-ELEC® ESD 4000 is a polyolefin compatible dissipative masterbatch developed for PELD and PE-HD film, sheet, blow and injection moulded products. The active substance is an IDP (inherently dissi.. |
|||
Surface Resistance | 1.00e+9 - 1.00e+10 ohm | 1.00e+9 - 1.00e+10 ohm | ISO IEC 61340-5-1 |
Premix Thermoplastics PRE-ELEC® ESD 5300 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 5300 is a static dissipative thermoplastic compound based on polypropylene homopolymer. The dissipative property is permanent and built into the polymer chain. Surface resistance valu.. |
|||
Surface Resistance | <= 1.00e+9 ohm | <= 1.00e+9 ohm | Test specimen: 100mm x 100mm x 3mm molded plaque; ISO IEC 61340-5-1 |
Premix Thermoplastics PRE-ELEC® ESD 7140 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 7140 is a static dissipative thermoplastic masterbatch based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 7140 has been developed for.. |
|||
Surface Resistance | 1.00e+9 - 1.00e+16 ohm | 1.00e+9 - 1.00e+16 ohm | Average value: 1.03e+15 ohm Grade Count:24 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |
|||
Surface Resistance | >= 1.00e+9 ohm | >= 1.00e+9 ohm | |
Lehmann & Voss LUVOCOM® 19-7669 Polyamide 46, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Highly dimensionally stable at elevated temperatures.Gear parts for automot.. |
|||
Surface Resistance | <= 1.00e+9 ohm | <= 1.00e+9 ohm | |
Lehmann & Voss LUVOCOM® 20-8286 Polyphthalamide, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear.. |
|||
Surface Resistance | <= 1.00e+9 ohm | <= 1.00e+9 ohm | |
Lehmann & Voss LUVOCOM® 21-7928 Polyamide 6/6T, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear.. |
|||
Surface Resistance | >= 1.00e+9 ohm | >= 1.00e+9 ohm | |
Lehmann & Voss LUVOCOM® 6-7834 Polyamide 12, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Dynamic stressed parts.Low waterabsorbtion, for dimensional stable precision parts.Isotropic sh.. |
|||
Surface Resistance | >= 1.00e+9 ohm | >= 1.00e+9 ohm | |
Lehmann & Voss LUVOCOM® 6-8438-1 Polyamide 12, with glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Suitable for discharging of statically generated electricity.Dynamic stressed parts.Low waterab.. |
|||
Surface Resistance | <= 1.00e+9 ohm | <= 1.00e+9 ohm | |
Lehmann & Voss LUVOCOM® 1105-7106 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts,.. |
|||
Surface Resistance | 1.00e+9 - 1.00e+14 ohm | 1.00e+9 - 1.00e+14 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON KE004 Acetal Copoly (Asia Pacific) LNP* Stat-kon* KE004 is a compound based on Acetal Copolymer resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Surface Resistance | 1.00e+9 - 1.00e+12 ohm | 1.00e+9 - 1.00e+12 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY M3000 PP (Europe-Africa-Middle East) LNP* Stat-loy* M3000 is a compound based on Polypropylene resin. Added features of this material include: Antistat, High Impact. |
|||
Surface Resistance | 1.00e+9 ohm | 1.00e+9 ohm | ASTM D257 |
Techmer ES Statiblend® ABS E AS Availability: North AmericaForms: PelletsAdditive: AntistaticFeatures: AntistaticInformation provided by TP Composites, Inc. |
|||
Surface Resistance | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY KX96821 Acetal LNP STAT-LOY* KX96821 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Antistat. |
|||
Surface Resistance | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY NX13401 PC+ABS LNP* STAT-LOY* NX13401 is a compound based on PC+ABS blend. Added features of this material include: Antistat, Flame Retardant, Excellent Release. |