CENTROPLAST CENTROSOL LF Acrylonitrile butadiene Styrene copolymer conductive

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Extruded
Manufacturer CENTROPLAST Engineering Plastics GMBH
Trade Name CENTROSOL
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CENTROPLAST CENTROSOL LF Acrylonitrile butadiene Styrene copolymer conductive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CENTROSOL LF ABS has high rigidity and hardness even at low temperatures. It is permanently conductive and is used in support components for the semi-conductor industry.Information provided by CENTROPLAST Engineering Plastics GMBH
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 35.0 MPa
5080 psi
v = 5 mm/min; ISO 527-2
Tensile Strength, Yield 27.0 MPa
3920 psi
v = 50 mm/min; ISO 527-2
Elongation at Break 28 %
28 %
ISO 527-2
Flexural Modulus 1.80 GPa
261 ksi
ISO 178
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+9 ohm-cm
1.00e+9 ohm-cm
IEC 60093
Surface Resistance <= 1.00e+9 ohm
<= 1.00e+9 ohm
IEC 60093