Surface Resistance 2.0 - 4.0 ohm
2.0 - 4.0 ohm
ASTM D 257
SABIC Innovative Plastics LNP Faradex ES003DE PEI
LNP* Faradex* ES003DE is a Polyetherimide resin containing stainless steel fibers. Characteristics of this grade are EMI/RFI Shielding.This data was supplied by SABIC-IP for the Americas region.
Surface Resistance 2.0 - 4.0 ohm
2.0 - 4.0 ohm
ASTM D257
SABIC Innovative Plastics LNP FARADEX ES003E PEI
LNP* FARADEX* ES003E is a Polyetherimide resin containing 15% Stainless Steel Fibers. Added feature of this grade is: EMI/RFI Shielding.
Surface Resistance 1.0 - 4.0 ohm
1.0 - 4.0 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON AE006 ABS
LNP* STAT-KON* AE006 is a compound based on ABS containing 30% Carbon Fiber. Added feature of this grade is: Electrically Conductive.
Surface Resistance 2.0 - 4.0 ohm
2.0 - 4.0 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON DD0009E PC
LNP* STAT-KON* DD0009E is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant, Easy Molding.
Surface Resistance 2.0 - 4.0 ohm
2.0 - 4.0 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON DE004ER PC
LNP* STAT-KON* DE004ER is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added featuresof this material include: Electrically Conductive, Easy Molding, Mold Release.
Surface Resistance 1.0 - 4.0 ohm
1.0 - 4.0 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON DE0069F PC
LNP* STAT-KON* DE0069F is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, Superior Molding.
Surface Resistance 1.0 - 4.0 ohm
1.0 - 4.0 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON DEL36 PC
LNP* STAT-KON* DEL36 is a compound based on Polycarbonate resin containing 30% Carbon Fiber, 15% PTFE. Added features include: Electrically Conductive, Wear Resistant.
Surface Resistance 2.0 - 4.0 ohm
2.0 - 4.0 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON FX98501 PE
LNP* STAT-KON* FX98501 is a compound based on Polyethylene resin containing Proprietary Fillers. Added feature of this material is: Electrically Conductive.
Surface Resistance 2.0 - 4.0 ohm
2.0 - 4.0 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON OEL13I PPS - Linear
LNP* STAT-KON* OEL13I is a compound based on PPS-Linear resin containing 15% Carbon Fiber, 5% PTFE. Added features of this grade include: High Impact, Wear Resistant, Electrically Conductive.
Surface Resistance 2.0 - 4.0 ohm
2.0 - 4.0 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON OEL32 PPS - Linear
LNP* STAT-KON* OCL32 is a compound based on PPS - Linear resin containing 10% Carbon Fiber, 15% PTFE. Added features of this grade include: Electrically Conductive, Wear Resistant.
Surface Resistance 1.0 - 4.0 ohm
1.0 - 4.0 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON REL33 PA 66
LNP STAT-KON* REL33 is a compound based on Nylon 66 resin containing 15% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Wear Resistant.
Surface Resistance 2.0 - 4.0 ohm
2.0 - 4.0 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON RX05489 PA 66
LNP* STAT-KON* RX05489 is a compound based on Nylon 66 resin containing 10% Carbon Fiber, 20% Glass Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear..
Surface Resistance 1.0 - 4.0 ohm
1.0 - 4.0 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON SD000 PA12
LNP* STAT-KON* SD000 is an unfilled Nylon 12 compound. Added feature of this grade is: Electrically Conductive.
Surface Resistance 2.0 - 4.0 ohm
2.0 - 4.0 ohm
ASTM D 257
SABIC Innovative Plastics LNP Stat-kon WEF42 PET/PBT
LNP Stat-Kon WCF-1006 is a compound based on PET/PBT resin containing carbon and glass fiber reinforcements.This data was supplied by SABIC-IP for the Americas region.
Surface Resistance 2.0 - 4.0 ohm
2.0 - 4.0 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON WS002I PBT
LNP* STAT-KON* WS002I is a compound based on PBT resin containing 10% Stainless Steel. Added features of this material include: Electrically Conductive, High Impact.
Surface Resistance 2.0 - 4.0 ohm
2.0 - 4.0 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON AE002 ABS
LNP* STAT-KON* AE002 is a compound based on ABS resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive.
Surface Resistance 1.0 - 4.0 ohm
1.0 - 4.0 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON DEL36 PC (Asia Pacific)
LNP* Stat-kon* DEL36 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, , Internally Lubricated.
Surface Resistance 1.0 - 4.0 ohm
1.0 - 4.0 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON RE0069S PA 66
LNP* STAT-KON* RE0069S is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, Heat Stabilized.
Surface Resistance 1.0 - 4.0 ohm
1.0 - 4.0 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON RE0069S PA 66 (Asia Pacific)
LNP* STAT-KON* RE0069S is a compound based on Nylon 66 resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, Heat Stabil..
Surface Resistance 1.0 - 4.0 ohm
1.0 - 4.0 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON REF42I PA 66
LNP* STAT-KON* REF42I is a compound based on Nylon 6/6 containing Proprietary Fillers. Added feature of this grade is: Electrically Conductive.
Surface Resistance 2.0 - 4.0 ohm
2.0 - 4.0 ohm
ASTM D 257
SABIC Innovative Plastics LNP Stat-kon MDM40 PP
LNP* Stat-Kon* MDM40 is a compound based on Polypropylene resin containing Mica and Carbon. Characteristics are Statically Conductive.This data was supplied by SABIC-IP for the Americas region.