Electrical Properties Metric English Comments
Surface Resistance 5.00e+18 ohm
5.00e+18 ohm
ASTM D257
Solvay Specialty Polymers Torlon® 4200 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 4200 is an unreinforced, unpigmented grade of polyamide-imide (PAI) resin for extrusion. This grade is designed for applications in the semiconductor industry which cannot tolerate particulat..
Surface Resistance 5.00e+18 ohm
5.00e+18 ohm
ASTM D257
Solvay Specialty Polymers Torlon® 4203L Polyamide-imide (PAI)  (Unverified Data**)
Torlon 4203L is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin. It has the best impact resistance and greatest elongation of all the Torlon grades. Torlon PAI has the hi..
Surface Resistance 5.00e+18 ohm
5.00e+18 ohm
ASTM D257
Solvay Specialty Polymers Torlon® 4200 Polyamide-imide (PAI)
Torlon® 4200 is an unreinforced, unpigmented grade of polyamide-imide (PAI) resin for extrusion. This grade is designed for applications in the semiconductor industry which cannot tolerate partic..
Surface Resistance 5.00e+18 ohm
5.00e+18 ohm
ASTM D257
Solvay Specialty Polymers Torlon® 4203L Polyamide-imide (PAI)
Torlon® 4203L is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin. It has the best impact resistance and greatest elongation of all the Torlon® grades. Torlon® PA..
Surface Resistance 5.00e+18 ohm
5.00e+18 ohm
DIN 53 482
Hippe PAI Polyamide-imide
Particularly used where high strength in a wide range of temperature (-190°C…+260°C), high notched strength and very good dielectric properties are required. Features good chemical stability, fl..
Surface Resistance 5.00e+18 ohm
5.00e+18 ohm
ASTM D257
Solvay Specialty Polymers Torlon® 4203 Polyamide-imide (PAI)  (discontinued **)
Torlon 4203 is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin for extrusion. It has the best impact resistance and greatest elongation of all the Torlon grades. Torlon P..