Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Torlon® 4203L Polyamide-imide (PAI)

Category Polymer , Thermoplastic , Polyamide-imide (PAI) , Polyamide-Imide, Extruded
Manufacturer Solvay Specialty Polymers
Trade Name Torlon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Torlon® 4203L Polyamide-imide (PAI).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Torlon® 4203L is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin. It has the best impact resistance and greatest elongation of all the Torlon® grades. Torlon® PAI has the highest strength and stiffness of any thermoplastic up to 275°C (525°F). It has outstanding resistance to wear, creep, and chemicals.Features: Ductile; Fatigue Resistant; Flame Retardant; Good Chemical Resistance; Good Creep Resistance; Good Electrical Properties; Good Wear Resistance; High Heat Resistance; High Temperature Strength; Low Temperature Toughness; Ultra High Impact ResistanceUses: Aircraft Applications; Automotive Applications; Bushings; Connectors; Electrical Parts; Electrical/Electronic Applications; Fasteners; Film; Machine/Mechanical Parts; Oil/Gas Applications; Semiconductor Molding Compounds; Thrust WasherAutomotive Specifications ASTM D4000 PAI000 R03 A56316 GA140 Z1Z2Z3Z4Z5Z6, Dwg YC3P-7E195-AA; CHRYSLER MS-DB-405 CPN3373 Color: NaturalInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ASTM D792
Water Absorption 0.33 %

@Time 86400 sec
0.33 %

@Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.0060 - 0.0085 cm/cm
0.0060 - 0.0085 in/in
Mechanical Properties Metric English Comments
Tensile Strength 152 MPa
22000 psi
ASTM D638
Tensile Stress 192 MPa
27800 psi
ASTM D1708
Elongation at Break 15 %
15 %
ASTM D638
Tensile Modulus 4.48 GPa
650 ksi
Type I; ASTM D638
Flexural Strength 118 MPa

@Temperature 232 °C
17100 psi

@Temperature 450 °F
ASTM D790
241 MPa

@Temperature 23.0 °C
35000 psi

@Temperature 73.4 °F
ASTM D790
Flexural Modulus 3.59 GPa

@Temperature 232 °C
521 ksi

@Temperature 450 °F
ASTM D790
5.03 GPa

@Temperature 23.0 °C
730 ksi

@Temperature 73.4 °F
ASTM D790
Compressive Strength 221 MPa
32100 psi
ASTM D695
Compressive Modulus 4.00 GPa
580 ksi
ASTM D695
Poissons Ratio 0.45
0.45
ASTM E132
Izod Impact, Notched 1.40 J/cm
2.62 ft-lb/in
ASTM D256
Izod Impact, Unnotched 11.0 J/cm
20.6 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 31.0 µm/m-°C
17.2 µin/in-°F
Thermal Conductivity 0.260 W/m-K
1.80 BTU-in/hr-ft²-°F
ASTM C177
Deflection Temperature at 1.8 MPa (264 psi) 278 °C
532 °F
Unannealed; ASTM D648
Glass Transition Temp, Tg 277 °C
531 °F
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+17 ohm-cm
2.00e+17 ohm-cm
ASTM D257
Surface Resistance 5.00e+18 ohm
5.00e+18 ohm
ASTM D257
Dielectric Constant 3.9

@Frequency 1.00e+6 Hz
3.9

@Frequency 1.00e+6 Hz
ASTM D150
4.2

@Frequency 60.0 Hz
4.2

@Frequency 60.0 Hz
ASTM D150
Dielectric Strength 23.0 kV/mm
584 kV/in
ASTM D149
Dissipation Factor 0.026

@Frequency 60.0 Hz
0.026

@Frequency 60.0 Hz
ASTM D150
0.031

@Frequency 1.00e+6 Hz
0.031

@Frequency 1.00e+6 Hz
ASTM D150
Processing Properties Metric English Comments
Rear Barrel Temperature 304 °C
579 °F
Nozzle Temperature 371 °C
700 °F
Mold Temperature 199 - 216 °C
390 - 421 °F
Drying Temperature 177 °C

@Time 10800 sec
351 °F

@Time 3.00 hour
Moisture Content <= 0.050 %
<= 0.050 %
Back Pressure 6.89 MPa
999 psi
Screw Speed 50 - 100 rpm
50 - 100 rpm
Descriptive Properties Value Comments
Additive PTFE Lubricant
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Form Pellets
Processing Technique Injection Molding; Machining; Profile Extrusion
RoHS Compliance RoHS Compliant
Screw L/D Ratio 18.0:1.0 to 24.0:1.0