Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 6.00e+14 ohm | 6.00e+14 ohm | |
Aardvark Polymers AARTEL® 2100UV Acetal Homopolymer Rotational Molding Resin Aartel 2100UV is a natural acetal homopolymer with UV stabilizers.Aartel 2100UV is a medium viscosity resin with excellent flow characteristics.Aartel 2100UV is available in natural white and may be.. |
|||
Surface Resistance | 6.00e+14 ohm | 6.00e+14 ohm | IEC 60093 |
Solvay TECHNYL® A 218 V25 Black 21 N PA66, 25% glass fiber, DRY Description: TECHNYL® A 218 V25 is a polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Surface Resistance | 6.00e+14 ohm | 6.00e+14 ohm | IEC 60093 |
Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 Black 34 NG is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p.. |
|||
Surface Resistance | 6.00e+14 ohm | 6.00e+14 ohm | IEC 60093 |
Solvay TECHNYL® A 218 V30 BK 34 NG-K PA66, 33% glass fiber, DRY Description: TECHNYL® A 218 V30 Black 34 NG-K is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color. Benefits: Thi.. |
|||
Surface Resistance | 6.00e+14 ohm | 6.00e+14 ohm | IEC 93 |
Solvay Technyl® A 218 V30 Nylon 66, 30% Glass Fiber, EH0 Polyamide PA66, reinforced with 30% of glass fiber, heat stabilized, for injection molding.Technyl A 218 V30 is used in all sectors of industry, offering an excellent combination between thermal and.. |
|||
Surface Resistance | 6.00e+14 ohm | 6.00e+14 ohm | IEC 60093 |
Solvay TECHNYL® A 218 V30 PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Surface Resistance | 6.00e+14 ohm | 6.00e+14 ohm | IEC 60093 |
Solvay TECHNYL® A 218 V35 Black 34 NG PA66, 35% glass fiber, DRY Description: TECHNYL® A 218 V35 Black 34 NG is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p.. |
|||
Surface Resistance | 6.00e+14 ohm | 6.00e+14 ohm | IEC 60093 |
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, DRY Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Surface Resistance | 6.00e+14 ohm | 6.00e+14 ohm | IEC 60093 |
Solvay TECHNYL® A 218 V50 PA66, 50% glass fiber, DRY Description: TECHNYL® A 218 V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Surface Resistance | 6.00e+14 ohm | 6.00e+14 ohm | IEC 60093 |
Solvay TECHNYL® A 216 V33 PA66, 33% glass fiber, DRY Description: TECHNYL® A 216 V33 is a polyamide 66, reinforced with 33% of glass fiber, for injection molding. This product is available in natural color.Benefits: The product offers an excellent .. |
|||
Surface Resistance | 6.00e+14 ohm | 6.00e+14 ohm | IEC 93 |
Solvay Technyl® A 218 V35 Nylon 66, 35% Glass Fiber, EH0 Polyamides PA66, reinforced with 35% of glass fiber, heat stabilized, for injection molding.Technyl A 218 V35 is used in all sectors of industry, offering an excellent combination between thermal an.. |
|||
Surface Resistance | 6.00e+14 ohm | 6.00e+14 ohm | IEC 93 |
Solvay Technyl® A 216 V30 Nylon 66, 30% Glass Fiber, EH0 Polyamide PA66, reinforced with 30% of glass fiber, for injection molding.Technyl A 216 V30 is used in all sectors of industry, offering an excellent combination between thermal and mechanical prope.. |
|||
Surface Resistance | 6.00e+14 ohm | 6.00e+14 ohm | IEC 60093 |
DuPont Performance Polymers Sorona® MT3401 NC010 Polytrimethylene Terephthalate (PTT) Unreinforced Renewably Sourced Polytrimethylene Terephthalate with Excellent Impact Resistance Sorona MT3401 NC010 is a medium toughened polytrimethylene terephthalate resin containing 29% renewably.. |
|||
Surface Resistance | 6.00e+14 ohm @Temperature 23.0 °C |
6.00e+14 ohm @Temperature 73.4 °F |
ASTM D257 |
DuPont Performance Polymers Delrin® 111P NC010 Acetal Homopolymer Delrin® 111P is a high viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, fewer voids). It has higher tensile strength and mod.. |
|||
Surface Resistance | 6.00e+14 ohm | 6.00e+14 ohm | ASTM D257 |
Adamas Adalon® 403 PTFE, 15% Polyimide Information provided by Adamas, HPM |
|||
Surface Resistance | 6.00e+14 ohm | 6.00e+14 ohm | C96/35/90; IPC TM-650 2.5.17.1 |
Arlon 85NT Polyimide Nonwoven Aramid Laminate and Prepreg 85NT is a pure polyimide laminate and prepreg system (Tg = 250°C), reinforced with a non-woven aramid substrate. This system combines the high-reliability features of polyimide (improved PTH relia.. |
|||
Surface Resistance | 6.00e+14 ohm @Temperature 23.0 °C |
6.00e+14 ohm @Temperature 73.4 °F |
IEC 60093 |
DuPont Performance Polymers Sorona® MT3401 NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**) Sorona® MT3401 NC010 is a medium toughened polytrimethylene terephthalate resin containing 29% renewably sourced ingredients by weight. It was initially coded SE38001.Information provided by DuPont.. |
|||
Surface Resistance | 1e+05 - 6.00e+14 ohm | 1e+05 - 6.00e+14 ohm | Average value: 1.96e+14 ohm Grade Count:12 |
Overview of materials for Polytrimethylene Terephthalate (PTT) This property data is a summary of similar materials in the MatWeb database for the category "Polytrimethylene Terephthalate (PTT)". Each property range of values reported is minimum and maximum val.. |