Electrical Properties Metric English Comments
Comparative Tracking Index 100 - 150 V
100 - 150 V
Average value: 117 V Grade Count:3
Overview of materials for Phenolic/Glass Fiber SMC
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic/Glass Fiber SMC". Each property range of values reported is minimum and maximum values of appro..
Comparative Tracking Index 125 - 150 V
125 - 150 V
Average value: 142 V Grade Count:3
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m..