Polymer Property : Arc Resistance = 135 sec Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Arc Resistance 135 sec
135 sec
ASTM D495
Owens Corning Glass Fiber Reinforced Polyester (PBT), 30 wt.% glass
Thermoplastic Polyesters are resistant to most organic solvents, weak acids and alkalis. They are not recommended with strong acids and alkalis or for prolonged use in hot water. Data provided by t..
Arc Resistance 135 sec
135 sec
Pyrotek TS-235 Thermoset Electrical Insulation Product
Glass reinforcement, Polyester resin, Tan color. Highly flexible. High heat resistance.Information provided by Pyrotek.
Arc Resistance 135 - 180 sec
135 - 180 sec
Average value: 164 sec Grade Count:4
Overview of materials for Phenolic, Resole, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Glass Fiber Filled". Each property range of values reported is minimum and maximum val..
Arc Resistance 135 sec
135 sec
ASTM D495
Kolon KOPA® KN333G15 G/F Reinforced Nylon 66
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin..
Arc Resistance 135 sec
135 sec
ASTM D495
Kolon KOPA® KN333G15SIBL G/F Reinforced Nylon 66
High strength, high toughnessApplications Relay coversInformation provided by API-Kolon.
Arc Resistance 135 sec
135 sec
ASTM D495
Kolon KOPA® KN333G25CRBK G/F Reinforced Nylon 66
EG-resistant, high strength, dimensionally stableApplications Cooling water pipesInformation provided by API-Kolon.
Arc Resistance 135 sec
135 sec
ASTM D495
Kolon KOPA® KN333G30BL G/F Reinforced Nylon 66
G/F 30% reinforcedApplications Engine coversInformation provided by API-Kolon.
Arc Resistance 135 sec
135 sec
ASTM D495
Kolon KOPA® KN333G30CRN G/F Reinforced Nylon 66
Oil resistantApplications Surge tanksInformation provided by API-Kolon.
Arc Resistance 135 sec
135 sec
ASTM D495
Kolon KOPA® KN333G30HS G/F Reinforced Nylon 66
High thermal resistant, high strength, dimensionally stableApplications Transmission gear supportersInformation provided by API-Kolon.
Arc Resistance 135 sec
135 sec
ASTM D495
Kolon KOPA® KN333G33BL G/F Reinforced Nylon 66
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin..
Arc Resistance 135 sec
135 sec
ASTM D495
Kolon KOPA® KN333G33CR G/F Reinforced Nylon 66
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin..
Arc Resistance 135 sec
135 sec
ASTM D495
Kolon KOPA® KN333G35CRBK G/F Reinforced Nylon 66
EG-resistant, high strength, dimensionally stableApplications Coolant temperature control partsInformation provided by API-Kolon.
Arc Resistance 135 sec
135 sec
ASTM D495
Kolon KOPA® KN333G45 G/F Reinforced Nylon 66
G/F 45% reinforcedApplications Internal gearsInformation provided by API-Kolon.
Arc Resistance 135 sec
135 sec
ASTM D495
Kolon KOPA® KN333HB40HFBL Hybrid Nylon 66
High flow, dimensionally stableApplications Fans & ShroudsInformation provided by API-Kolon.
Arc Resistance 135 sec
135 sec
ASTM D495
Haysite H515 Polyester, High Temp Flex
H515 exhibits excellent flexibility and retention of electrical properties at elevated temperatures. For use in 220º C insulation systems in dry type transformers and where flexibility and high t..
Arc Resistance 135 sec
135 sec
ASTM D495
Kolon KOPA® KN178MT40 M/F Reinforced Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
Arc Resistance 135 sec
135 sec
ASTM D495
Sumitomo Bakelite North America 3-2-530 Short-Glass Reinforced Diallyl Phthalate
Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North A..
Arc Resistance 135 sec
135 sec
ASTM D495
Sumitomo Bakelite North America 51-01 CAFR-P Mineral Filled Diallyl Phthalate
Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Americ..
Arc Resistance 135 sec
135 sec
ASTM D495
Sumitomo Bakelite North America RX® 3-2-530-P Long-Glass Reinforced Diallyl Phthalate
Long glass fiber reinforced, flame retardant, diallyl meta-phthalate molding compound which meets the requirements of ASTM D5948 Type GII-30F.Information provided by Vyncolit, a Sumitomo Bak Group
Arc Resistance 135 sec
135 sec
ASTM D495
Sumitomo Bakelite North America RX® 630 Fiberglass Reinforced Phenolic
RXÂ 630 is a fiberglass reinforced phenolic molding compound, with good dimensional stability and good strength at elevated temperatures. Information supplied by Sumitomo Bak North America.
Arc Resistance 135 sec
135 sec
ASTM D495
Plenco 6582 Phenolic, Briquette, Injection Molded
PLENCO 06582 is a rubber modified phenolic molding compound, offering excellent heat resistant properties, along with improved mechanical strength at elevated temperatures. UL recognized under compo..
Arc Resistance 135 sec
135 sec
Cosmic Plastics 6120F Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Arc Resistance 135 - 180 sec
135 - 180 sec
Average value: 144 sec Grade Count:12
Overview of materials for Diallyl Phthalate (DAP), Cast, Mineral Filler
This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP), Cast, Mineral Filler". Each property range of values reported is minimum and ma..
Arc Resistance 135 sec
135 sec
ASTM D495
Kolon KOPA® KN135G33HI Multi Reinforced Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubric..
Arc Resistance 135 sec
135 sec
Cosmic Plastics 6160 Mineral Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Arc Resistance 135 sec
135 sec
Cosmic Plastics D44 Mineral Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Arc Resistance 135 - 140 sec
135 - 140 sec
ASTM D495
Hexion Bakelite™ PF 2836 Phenolic Formaldehyde Resin, Improved Electrical Properties, Low Shrinkage, UL Listed &nbs
Phenolic molding compound, inorganically/organically filled, increased heat resistance, increased tracking resistance, low shrinkage and post shrinkage, improved electrical properties, UL listed mol..