Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Diallyl Phthalate (DAP), Cast, Mineral Filler

Category Polymer , Thermoset , Diallyl Phthalate (DAP) , Diallyl Phthalate (DAP), Cast, Mineral Filler
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Diallyl Phthalate (DAP), Cast, Mineral Filler.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP), Cast, Mineral Filler". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.66 - 1.86 g/cc
0.0600 - 0.0672 lb/in³
Average value: 1.77 g/cc Grade Count:12
Apparent Bulk Density 0.600 - 0.860 g/cc
0.0217 - 0.0311 lb/in³
Average value: 0.732 g/cc Grade Count:6
Water Absorption 0.250 - 0.650 %
0.250 - 0.650 %
Average value: 0.445 % Grade Count:10
Linear Mold Shrinkage 0.00100 - 0.0100 cm/cm
0.00100 - 0.0100 in/in
Average value: 0.00429 cm/cm Grade Count:12
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 41.0 - 55.2 MPa
5950 - 8010 psi
Average value: 49.6 MPa Grade Count:12
Flexural Yield Strength 76.0 - 110 MPa
11000 - 16000 psi
Average value: 93.0 MPa Grade Count:12
Flexural Modulus 6.90 - 11.7 GPa
1000 - 1700 ksi
Average value: 10.3 GPa Grade Count:8
Compressive Yield Strength 138 - 179 MPa
20000 - 26000 psi
Average value: 153 MPa Grade Count:12
Izod Impact, Notched 0.210 - 0.320 J/cm
0.393 - 0.599 ft-lb/in
Average value: 0.236 J/cm Grade Count:11
Thermal Properties Metric English Comments
CTE, linear 25.0 - 46.0 µm/m-°C
13.9 - 25.6 µin/in-°F
Average value: 34.3 µm/m-°C Grade Count:12
Maximum Service Temperature, Air 130 °C
266 °F
Average value: 130 °C Grade Count:5
Deflection Temperature at 1.8 MPa (264 psi) 149 - 274 °C
300 - 525 °F
Average value: 192 °C Grade Count:12
UL RTI, Electrical 130 °C
266 °F
Average value: 130 °C Grade Count:3
UL RTI, Mechanical with Impact 130 °C
266 °F
Average value: 130 °C Grade Count:3
UL RTI, Mechanical without Impact 130 °C
266 °F
Average value: 130 °C Grade Count:3
Flammability, UL94 HB - V-0
HB - V-0
Grade Count:5
Oxygen Index 23.0 - 30.0 %
23.0 - 30.0 %
Average value: 25.7 % Grade Count:6
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+17 ohm-cm
1.00e+17 ohm-cm
Average value: 1.00e+17 ohm-cm Grade Count:4
Surface Resistance 1.00e+17 ohm
1.00e+17 ohm
Average value: 1.00e+17 ohm Grade Count:4
Dielectric Constant 3.60 - 4.70
3.60 - 4.70
Average value: 4.25 Grade Count:12
Dielectric Strength 14.0 - 17.0 kV/mm
356 - 432 kV/in
Average value: 15.2 kV/mm Grade Count:12
Dissipation Factor 0.0100 - 0.0250
0.0100 - 0.0250
Average value: 0.0168 Grade Count:12
Arc Resistance 135 - 180 sec
135 - 180 sec
Average value: 144 sec Grade Count:12
Comparative Tracking Index 600 V
600 V
Average value: 600 V Grade Count:5
Processing Properties Metric English Comments
Processing Temperature 135 - 180 °C
275 - 356 °F
Average value: 162 °C Grade Count:10