Electrical Properties Metric English Comments
Arc Resistance 160 sec
160 sec
IPC-TM-650.2.5.1
Park Electrochemical Nelco® N8000 Cyanate Ester Epoxy Laminate and Prepreg
The Nelco N8000 is a high-Tg cyanate ester laminate and prepreg system that provides superior performance and product integrity and is ideal for board designs with higher layer counts, finer lines a..
Arc Resistance 160 sec
160 sec
ASTM D495
Plenco 2424 Phenolic, Granular, Injection Molded  (discontinued **)
Two-stage Phenolic. PLENCO 02424 is a black, two stage, general purpose phenolic molding compound. It has a good balance of properties for a general purpose type material. It is used in electrical ..
Arc Resistance 160 sec
160 sec
ASTM D495
Plenco 4100 Phenolic, Granular, Injection Molded  (discontinued **)
Two-stage Phenolic. PLENCO 04100 is a black two stage, medium heat resistant phenolic molding compound. It has excellent moldability characteristics and molded finish. It is used in appliance and ..
Arc Resistance 160 sec
160 sec
ASTM D495
Plenco Valite 4100 Novolac Phenolic, Granular, Compression Molded  (discontinued **)
This Valite product has been replaced by Plenco 4100. Data provided by Plenco.VALITE 4100 is a black two stage, medium heat resistant phenolic molding compound. It has excellent moldability charac..
Arc Resistance 160 sec
160 sec
ASTM D495
LG Chemical LUMID GP2130A(W) PA6+GF13%, General Purpose
Feature: Injection Molding, PA6+GF13%, General PurposeApplication: Automotive PartsCAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical
Arc Resistance 160 sec
160 sec
ASTM D495
LG Chemical LUMID GP2130AE PA6+GF13%, General Purpose
Feature: Injection Molding, PA6+GF13%, General PurposeApplication: Industrial MaterialCAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical
Arc Resistance 160 sec
160 sec
ASTM D495
Sumitomo Bakelite North America RX® 640 Fiberglass Reinforced Phenolic Resole
RXÂ 640 is a fiberglass reinforced, ammonia-free, phenolic resole compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type GPI-5.Information supp..
Arc Resistance 160 sec
160 sec
Cosmic Plastics 6130F Long Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Arc Resistance 160 sec
160 sec
Tungsten electrode; ASTM D495
E-Polymers TEKAMID® TB120G15 , 15% Glass Fiber Reinforced PA6, DAM
15% Glass Fiber reinforced, Good surface Information provided by E-Polymers Co. Ltd.
Arc Resistance 160 sec
160 sec
IPC TM-650 2.5.1
Arlon 85NT Polyimide Nonwoven Aramid Laminate and Prepreg
85NT is a pure polyimide laminate and prepreg system (Tg = 250°C), reinforced with a non-woven aramid substrate. This system combines the high-reliability features of polyimide (improved PTH relia..
Arc Resistance 160 sec
160 sec
at 500 Volts; ASTM D495
Gharda Chemicals G-PAEK™ 1230GF Ultra High Performance PEK Polymer
Product Details: Ultra High Performance Thermoplastic material, 30% glass fiber reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection molding, standard flow, Beige ..
Arc Resistance 160 sec
160 sec
Cosmic Plastics 6130 Long Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Arc Resistance 160 sec
160 sec
ASTM D495
Plenco 7467 Phenolic, Nodular, Transfer Molded  (discontinued **)
Two-Stage Phenolic. PLENCO 07467 is an organic phenolic molding compound offering excellent dimensional stability under conditions of total water immersion. 07467 is formulated to provide improved ..