Electrical Properties Metric English Comments
Arc Resistance 80 sec
80 sec
ASTM D495
Owens Corning Glass Fiber Reinforced Acrylonitrile Butadiene Styrene (ABS), 20 wt.% glass
ABS is highly resistant to weak acids and alkalis, and provides good resistance to most organic solvents. It is attacked by sulfuric and nitric acids, and is soluble in esters, ketones and ethylene ..
Arc Resistance 80 sec
80 sec
ASTM D495
Plenco 51045 PET, Pellet, Injection Molded, Black  (discontinued **)
PLENCO 51045 is an engineering grade glass reinforced polyethylene terephthalate resin designed for higher physical strength. It is It is UL listed and available in black only.Information supplied b..
Arc Resistance 80 sec
80 sec
ASTM D495
Samyang Tripet® 2550GN45 Polyethylene Terephthalate, 45% Glass Fiber Reinforced, Flame Retardant  (discontinue
TRIPET® has excellent heat resistance, good surface, chemical resistance and high electrical performance.Applications:Coil BobbinConnectorMotor HousingLamp HousingRelay BaseIron bodyAll information..
Arc Resistance 80 sec
80 sec
ASTM D495
Plenco 7300 Phenolic, Nodular, Transfer Molded  (discontinued **)
Two-Stage Phenolic. PLENCO 07300 is an organic fiber reinforced phenolic molding compound offering improved mechanical strength and excellent cosmetic properties. UL recognized under component file..
Arc Resistance 80 sec
80 sec
ASTM D495
LG Chemical LUMID GN1001AF PA6, Halogen Free Flame Retardant
Feature: Injection Molding, PA6, Halogen Free Flame RetardantApplication: Electrical & Electronic (Switch)CAS No. 25038-54-4 and 37640-57-6Information provided by LG Chemical
Arc Resistance 80 sec
80 sec
ASTM D495
LG Chemical Lupox® PBT-LW5303F 30% Glass Filled Low Warp Flame Retardant PBT
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Arc Resistance 80 sec
80 sec
ASTM D495
KYDEX® 100 Acrylic/PVC Thermoplastic Sheet
High impact fire rated sheetApplications: Housings for equipment such as photocopy machines, instrument panels, computers, keyboards, telephones. Hidden parts for equipment such as vending machines..
Arc Resistance 80 sec
80 sec
ASTM D495
Samyang Tripet® 2550GN30 Polyethylene Terephthalate, 30% Glass Fiber Reinforced, Flame Retardant
TRIPET® has excellent heat resistance, good surface, chemical resistance and high electrical performance.Applications:Coil BobbinConnectorMotor HousingLamp HousingRelay BaseIron bodyAll informati..
Arc Resistance 80 sec
80 sec
Dry; ASTM D495
Plastics Group Polifil® GFABS-10 10% Glass-Reinforced Acrylonitrile-Butadiene Styrene (ABS)
Polifil® GFABS series compounds combine the most desirable properties of both components - allowing for enhanced processability and toughness together with the stiffness of glass.Applications: Fire..
Arc Resistance 80 sec
80 sec
Dry; ASTM D495
Plastics Group Polifil® GFABS-20 20% Glass-Reinforced Acrylonitrile-Butadiene Styrene (ABS)
Polifil® GFABS series compounds combine the most desirable properties of both components - allowing for enhanced processability and toughness together with the stiffness of glass.Applications: Fire..
Arc Resistance 80 sec
80 sec
ASTM D495
Unitika AX-1500W Conditioned
Characteristics: A resin succeeding the advantages of AX1500 resin and containing titanium oxide at high concentration. Improved drastically in light reflection and blocking properties, aimed at dis..
Arc Resistance 80 sec
80 sec
ASTM D495
Unitika AXF-1500-05 Conditioned
Characteristics: Lubricant grade of AX1500, excellent in heat and chemical resistancesInformation provided by Unitika Ltd.
Arc Resistance 80 sec
80 sec
Tungsten electrode; ASTM D495
Toyobo VYLOPET® EMC133 Injection Molding Polyester Resin, Hydrolysis Resistant
Applications: Electric rice cooker partsBathroom appliancesFeatures: Good hydrolysis resistanceInformation provided by Toyobo.
Arc Resistance 80 sec
80 sec
ASTM D495
Toyobo Vylopet® EMC145 Glass Reinforced Polyester, Standard Grade
Key Feature: Flame retardant V-0 UL-94 classApplications: Ultra-precise componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and trac..
Arc Resistance 80 sec
80 sec
Unitika UNILATE® 1 NC PET
Flame resisting gradeUNILATE® products are plate materials prepared by using a polyethylene terephthalate (PET resin) as the main component, blending it with glass staple fiber, inorganic filler, a..
Arc Resistance 80 sec
80 sec
ASTM D495
Toyobo Vylopet® EMC605 PET/PBT Blend
Key Feature: Flame retardant V-0 UL 94 classApplications: glossy surface componentsPET/PBT blends suggested for glossy surfaces. General features of Vylopet® include heat resistance, good mechanic..
Arc Resistance 80 sec
80 sec
ASTM D495
Toyobo Vylopet® EMC615 PET/PBT Blend
Key Feature: Flame retardant V-0 UL 94 classApplications: electrical and electronic componentsPET/PBT blends suggested for glossy surfaces. General features of Vylopet® include heat resistance, go..
Arc Resistance 80 sec
80 sec
ASTM D495
Toyobo Vylopet® EMC630 PET/PBT Blend
Key Feature: Flame retardant V-0 UL 94 classApplications: general and high rigidity componentsPET/PBT blends suggested for glossy surfaces. General features of Vylopet® include heat resistance, go..
Arc Resistance 80 sec
80 sec
Tungsten; ASTM D495
Asahi Kasei Xyron® 140Z Modified Polyphenylene Ether
Flame RetardantInformation provided by Asahi Kasei
Arc Resistance 80 sec
80 sec
Tungsten; ASTM D495
Asahi Kasei Xyron® 220Z Modified Polyphenylene Ether
Flame RetardantInformation provided by Asahi Kasei
Arc Resistance 80 sec
80 sec
Tungsten; ASTM D495
Asahi Kasei Xyron® 240W Modified Polyphenylene Ether
Flame RetardantInformation provided by Asahi Kasei
Arc Resistance 80 sec
80 sec
Tungsten; ASTM D495
Asahi Kasei Xyron® 240Z Modified Polyphenylene Ether
Flame RetardantInformation provided by Asahi Kasei
Arc Resistance 80 sec
80 sec
Tungsten; ASTM D495
Asahi Kasei Xyron® SZ800 Modified Polyphenylene Ether
High-Heat ResistantInformation provided by Asahi Kasei
Arc Resistance 80 sec
80 sec
Tungsten; ASTM D495
Asahi Kasei Xyron® 600H Modified Polyphenylene Ether
Heat ResistantInformation provided by Asahi Kasei
Arc Resistance 80 sec
80 sec
Tungsten; ASTM D495
Asahi Kasei Xyron® X9102 Modified Polyphenylene Ether
High-Heat ResistantInformation provided by Asahi Kasei
Arc Resistance 80 sec
80 sec
ASTM D495
Gromax CCP PBT 6730-104F Glass/Mineral Filled
Product Description: PBT glass/mineral reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excellent w..
Copyright © lookpolymers.com All Rights Reserved