Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Toyobo Vylopet® EMC145 Glass Reinforced Polyester, Standard Grade

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant
Manufacturer Toyobo
Trade Name VYLOPET®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Toyobo Vylopet® EMC145 Glass Reinforced Polyester, Standard Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Feature: Flame retardant V-0 UL-94 classApplications: Ultra-precise componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and tracking resistance, chemical & weather resistance, and processability.Information provided by Toyobo Co., Ltd
Physical Properties Metric English Comments
Density 1.70 g/cc
0.0614 lb/in³
ASTM D792
Water Absorption 0.050 %
0.050 %
ASTM D570
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
0.0090 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell M 95
95
ASTM D785
Tensile Strength, Ultimate 172 MPa
24900 psi
ASTM D638
Elongation at Break 1.9 %
1.9 %
ASTM D638
Flexural Yield Strength 255 MPa
37000 psi
ASTM D790
Flexural Modulus 16.0 GPa
2320 ksi
ASTM D790
Compressive Yield Strength 128 MPa
18600 psi
ASTM D695
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
Taber Abrasion, mg/1000 Cycles 34
34
ASTM D1044
Thermal Properties Metric English Comments
Melting Point 255 °C
491 °F
DSC
Deflection Temperature at 0.46 MPa (66 psi) 245 °C
473 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 225 °C
437 °F
ASTM D648
UL RTI, Electrical 130 °C
266 °F
UL-746B
Flammability, UL94 V-0

@Thickness 0.7937 mm
V-0

@Thickness 0.03125 in
unregistered
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Strength 25.0 kV/mm

@Thickness 2.00 mm
635 kV/in

@Thickness 0.0787 in
ASTM D149
Arc Resistance 80 sec
80 sec
ASTM D495
Comparative Tracking Index 200 V
200 V
IEC test