Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 27.9 kV/mm @Thickness 1.60 mm |
709 kV/in @Thickness 0.0630 in |
in oil; ASTM D 149 |
SABIC Innovative Plastics Ultem 1000FV PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact Compliant, NSF 51 Listing.This data wa.. |
|||
Dielectric Strength | 27.9 kV/mm @Thickness 1.60 mm |
709 kV/in @Thickness 0.0630 in |
in oil; ASTM D 149 |
SABIC Innovative Plastics Ultem 1000FV PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact Compliant, NSF 51 Listing.This data wa.. |
|||
Dielectric Strength | 27.9 kV/mm @Thickness 1.60 mm |
709 kV/in @Thickness 0.0630 in |
in oil; ASTM D 149 |
SABIC Innovative Plastics Ultem 1000FV PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact Compliant, NSF 51 Listing.This data wa.. |
|||
Dielectric Strength | 27.9 kV/mm @Thickness 1.60 mm |
709 kV/in @Thickness 0.0630 in |
in oil; ASTM D 149 |
SABIC Innovative Plastics Ultem 1000M PEI Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Dielectric Strength | 27.9 kV/mm @Thickness 1.60 mm |
709 kV/in @Thickness 0.0630 in |
in oil; ASTM D 149 |
SABIC Innovative Plastics Ultem 1000M PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Dielectric Strength | 27.9 kV/mm @Thickness 1.60 mm |
709 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics ULTEM 1000P PEI Standard flow Polyetherimide (Tg 217C) in 350 micron powder. ECO Conforming. |
|||
Dielectric Strength | 27.9 kV/mm @Thickness 1.60 mm |
709 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics ULTEM 1000P PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C) in 350 micron powder. ECO Conforming. |
|||
Dielectric Strength | 27.9 kV/mm @Thickness 1.60 mm |
709 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics ULTEM 1000RV PEI Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. |
|||
Dielectric Strength | 27.9 kV/mm @Thickness 1.60 mm |
709 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics ULTEM 1000RV PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. |
|||
Dielectric Strength | 27.9 kV/mm @Thickness 1.60 mm |
709 kV/in @Thickness 0.0630 in |
in oil; ASTM D 149 |
SABIC Innovative Plastics Ultem 1000RV PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Afr.. |
|||
Dielectric Strength | 27.9 kV/mm @Thickness 1.60 mm |
709 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics ULTEM 1010 PEI Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June 2007, this grade will no longer b.. |
|||
Dielectric Strength | 27.9 kV/mm @Thickness 1.60 mm |
709 kV/in @Thickness 0.0630 in |
in oil; ASTM D 149 |
SABIC Innovative Plastics Ultem 1010FV PEI Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contant compliant, NSF 51 listing.This data wa.. |
|||
Dielectric Strength | 27.9 kV/mm @Thickness 1.60 mm |
709 kV/in @Thickness 0.0630 in |
in oil; ASTM D 149 |
SABIC Innovative Plastics Ultem 1010FV PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contant compliant, NSF 51 listing.This data wa.. |
|||
Dielectric Strength | 27.9 kV/mm @Thickness 1.60 mm |
709 kV/in @Thickness 0.0630 in |
in oil; ASTM D 149 |
SABIC Innovative Plastics Ultem 1010FV PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contant compliant, NSF 51 listing.This data wa.. |
|||
Dielectric Strength | 27.9 kV/mm @Thickness 1.60 mm |
709 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics ULTEM 1010M PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. |
|||
Dielectric Strength | 27.9 kV/mm @Thickness 1.60 mm |
709 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics ULTEM 1010P PEI Enhanced flow Polyetherimide (Tg 217C) in 350 micron powder. ECO Conforming. |
|||
Dielectric Strength | 27.9 kV/mm @Thickness 1.60 mm |
709 kV/in @Thickness 0.0630 in |
in oil; ASTM D 149 |
SABIC Innovative Plastics Ultem 1010RV PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Americas r.. |
|||
Dielectric Strength | 27.9 kV/mm @Thickness 1.60 mm |
709 kV/in @Thickness 0.0630 in |
in oil; ASTM D 149 |
SABIC Innovative Plastics Ultem 1010RV PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Asia Pacif.. |
|||
Dielectric Strength | 27.9 kV/mm @Thickness 1.60 mm |
709 kV/in @Thickness 0.0630 in |
in oil; ASTM D 149 |
SABIC Innovative Plastics Ultem 1010RV PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Afr.. |
|||
Dielectric Strength | 27.9 kV/mm @Thickness 1.60 mm |
709 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics ULTEM 1010TC PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing. |
|||
Dielectric Strength | 27.9 kV/mm @Thickness 1.60 mm |
709 kV/in @Thickness 0.0630 in |
in oil; ASTM D 149 |
SABIC Innovative Plastics Ultem 1010V PEI Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.This data wa.. |
|||
Dielectric Strength | 27.9 kV/mm @Thickness 1.60 mm |
709 kV/in @Thickness 0.0630 in |
in oil; ASTM D 149 |
SABIC Innovative Plastics Ultem 1010V PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.This data wa.. |
|||
Dielectric Strength | 27.9 kV/mm @Thickness 1.60 mm |
709 kV/in @Thickness 0.0630 in |
in oil; ASTM D 149 |
SABIC Innovative Plastics Ultem 1010V PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.This data wa.. |
|||
Dielectric Strength | 27.9 kV/mm @Thickness 1.60 mm |
709 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics ULTEM 1010X PEI Enhanced flow Polyetherimide (Tg 217C) with low ionic contamination of less than 0.1 ppm each of leachable chloride and sulphates. ECO Conforming. Factory Mutual FM4910 compliant in recognized col.. |
|||
Dielectric Strength | 27.9 kV/mm @Thickness 1.60 mm |
709 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics ULTEM HU1000 PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
Dielectric Strength | 27.9 kV/mm @Thickness 1.60 mm |
709 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics ULTEM HU1000 PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
Dielectric Strength | 27.9 kV/mm @Thickness 1.60 mm |
709 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics ULTEM HU1000 PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
Dielectric Strength | 27.9 kV/mm @Thickness 1.60 mm |
709 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics ULTEM HU1010 PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI),.. |
|||
Dielectric Strength | 27.9 kV/mm @Thickness 1.60 mm |
709 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Xenoy® 6620 PBT+PC PBT+PC, Unreinforced, impact modified thermoplastic alloy. Outstanding impact at low temperature |
|||
Dielectric Strength | 27.9 kV/mm @Thickness 1.60 mm |
709 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics ULTEM 1000 PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing, compliant in natural color. Effective June, 20.. |