Teknor Apex APEX® 4101 Polyvinyl Chloride, Flexible

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade , PVC, Wire and Cable Grade
Manufacturer Teknor Apex Company
Trade Name APEX®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex APEX® 4101 Polyvinyl Chloride, Flexible.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molded Components Additional Information: Temperature Rating: 60°C Recognized Component, CSA C22.2 No. 0.6, CSA Flammability Classification: 0.6HB at 0.86mmInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.36 g/cc
1.36 g/cc
ASTM D792
Linear Mold Shrinkage 0.010 - 0.012 cm/cm
0.010 - 0.012 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 76
76
15 seconds; ASTM D2240
Tensile Strength at Break 11.0 MPa
1590 psi
ASTM D638
Elongation at Break 320 %
320 %
ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 60.0 °C
140 °F
Continuous Use; ASTM D794
Brittleness Temperature -43.0 °C
-45.4 °F
ASTM D746
UL RTI, Electrical 90.0 °C

@Thickness 0.810 mm
194 °F

@Thickness 0.0319 in
UL 746
90.0 °C

@Thickness 3.00 mm
194 °F

@Thickness 0.118 in
UL 746
UL RTI, Mechanical without Impact 90.0 °C

@Thickness 0.810 mm
194 °F

@Thickness 0.0319 in
UL 746
90.0 °C

@Thickness 3.00 mm
194 °F

@Thickness 0.118 in
UL 746
Flammability, UL94 V-2

@Thickness 0.810 mm
V-2

@Thickness 0.0319 in
V-2

@Thickness 3.00 mm
V-2

@Thickness 0.118 in
Oxygen Index 26 %
26 %
ASTM D2863
Electrical Properties Metric English Comments
Comparative Tracking Index >= 600 V

@Thickness 3.00 mm
>= 600 V

@Thickness 0.118 in
UL 746
Hot Wire Ignition, HWI 60 - 120 sec

@Thickness 3.00 mm
60 - 120 sec

@Thickness 0.118 in
UL 746
High Amp Arc Ignition, HAI 30 - 60 arcs

@Thickness 3.00 mm
30 - 60 arcs

@Thickness 0.118 in
UL 746
Processing Properties Metric English Comments
Melt Temperature 177 °C
350 °F
Processing Temperature
Descriptive Properties Value Comments
Appearance Opaque