Polymer Property : Dielectric Strength = 180 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 180 kV/mm

@Thickness 0.0500 mm
4570 kV/in

@Thickness 0.00197 in
Amorphous Film; ASTM D149
Solvay Specialty Polymers AvaSpire® AV-848 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire® AV-848 is a high-temperature, polyaryletherketone (PAEK) that offers several key performance advantages over comparable grades of PEEK above 150°C, including better dimensional stability..
Dielectric Strength 180 kV/mm
4570 kV/in
ASTM D149
Solvay Specialty Polymers Ajedium™ Films -- Veradel® PES 201 NT Polyethersulfone (PESU)
Veradel® PES 201 NT polyethersulfone is a tough, high-strength thermoplastics that are suitable for continuous use up to 356°F (180°C). Veradel® film is resistant to oxidation and hydrol..
Dielectric Strength 180 kV/mm

@Thickness 0.0600 mm
4570 kV/in

@Thickness 0.00236 in
Amorphous Film; ASTM D149
Solvay Specialty Polymers AvaSpire® AV-630 Polyaryletherketone (PAEK)
AvaSpire® AV-630 is an unreinforced polyaryletherketone (PAEK) developed as an alternative to low melt flow PEEK for the extrusion of ultra-thin films. Films with thicknesses as low as 0.2 mils (..
Dielectric Strength 180 kV/mm

@Thickness 0.0500 mm
4570 kV/in

@Thickness 0.00197 in
Amorphous Film; ASTM D149
Solvay Specialty Polymers AvaSpire® AV-848 Polyaryletherketone (PAEK)
AvaSpire® AV-848 is a high-temperature, polyaryletherketone (PAEK) that offers several key performance advantages over comparable grades of PEEK above 150°C, including better dimensional stabi..
Dielectric Strength 180 kV/mm

@Thickness 0.0600 mm
4570 kV/in

@Thickness 0.00236 in
Amorphous Film; ASTM D149
Solvay Specialty Polymers AvaSpire® AV-630 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-630 is an unreinforced polyaryletherketone (PAEK) developed as an alternative to low melt flow PEEK for the extrusion of ultra-thin films. Films with thicknesses as low as 0.2 mils (5 mi..
Dielectric Strength >= 180 kV/mm
>= 4570 kV/in
CEN® Electronic Material CN Polyimide Film, 2 Mil Thickness
CEN®CN polyimide film is typical general-purpose polyimide film and has been used successfully in applications at temperatures as low as -269°C (-452°F) and as high as 400°C (752°F). CN film ca..
Dielectric Strength >= 180 kV/mm
>= 4570 kV/in
ASTM D149
CEN® Electronic Material CV Polyimide Film, 2 Mil Thickness
CEN®CV polyimide film keeps the same film properties as CEN®CN polyimide film, and has an excellent balance of physical, chemical, and electrical properties over a wide temperature range. With sup..