Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 180 kV/mm @Thickness 0.0500 mm |
4570 kV/in @Thickness 0.00197 in |
Amorphous Film; ASTM D149 |
Solvay Specialty Polymers AvaSpire® AV-848 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire® AV-848 is a high-temperature, polyaryletherketone (PAEK) that offers several key performance advantages over comparable grades of PEEK above 150°C, including better dimensional stability.. |
|||
Dielectric Strength | 180 kV/mm | 4570 kV/in | ASTM D149 |
Solvay Specialty Polymers Ajedium™ Films -- Veradel® PES 201 NT Polyethersulfone (PESU) Veradel® PES 201 NT polyethersulfone is a tough, high-strength thermoplastics that are suitable for continuous use up to 356°F (180°C). Veradel® film is resistant to oxidation and hydrol.. |
|||
Dielectric Strength | 180 kV/mm @Thickness 0.0600 mm |
4570 kV/in @Thickness 0.00236 in |
Amorphous Film; ASTM D149 |
Solvay Specialty Polymers AvaSpire® AV-630 Polyaryletherketone (PAEK) AvaSpire® AV-630 is an unreinforced polyaryletherketone (PAEK) developed as an alternative to low melt flow PEEK for the extrusion of ultra-thin films. Films with thicknesses as low as 0.2 mils (.. |
|||
Dielectric Strength | 180 kV/mm @Thickness 0.0500 mm |
4570 kV/in @Thickness 0.00197 in |
Amorphous Film; ASTM D149 |
Solvay Specialty Polymers AvaSpire® AV-848 Polyaryletherketone (PAEK) AvaSpire® AV-848 is a high-temperature, polyaryletherketone (PAEK) that offers several key performance advantages over comparable grades of PEEK above 150°C, including better dimensional stabi.. |
|||
Dielectric Strength | 180 kV/mm @Thickness 0.0600 mm |
4570 kV/in @Thickness 0.00236 in |
Amorphous Film; ASTM D149 |
Solvay Specialty Polymers AvaSpire® AV-630 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-630 is an unreinforced polyaryletherketone (PAEK) developed as an alternative to low melt flow PEEK for the extrusion of ultra-thin films. Films with thicknesses as low as 0.2 mils (5 mi.. |
|||
Dielectric Strength | >= 180 kV/mm | >= 4570 kV/in | |
CEN® Electronic Material CN Polyimide Film, 2 Mil Thickness CEN®CN polyimide film is typical general-purpose polyimide film and has been used successfully in applications at temperatures as low as -269°C (-452°F) and as high as 400°C (752°F). CN film ca.. |
|||
Dielectric Strength | >= 180 kV/mm | >= 4570 kV/in | ASTM D149 |
CEN® Electronic Material CV Polyimide Film, 2 Mil Thickness CEN®CV polyimide film keeps the same film properties as CEN®CN polyimide film, and has an excellent balance of physical, chemical, and electrical properties over a wide temperature range. With sup.. |