Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 10.0 - 150 kV/mm | 254 - 3810 kV/in | Average value: 42.4 kV/mm Grade Count:58 |
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m.. |
|||
Dielectric Strength | 17.0 - 150 kV/mm | 432 - 3810 kV/in | Breakdown; DIN 53 481, IEC-243, VDE 0303 Part 1 |
Hippe PVDF Better mechanical strength compared to other fluorinated polymers. Tough and hard. High-grade electrical feature. Good weathering stability. Physiologically safe. Not as good as fluorinated pol.. |