Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 16.7 kV/mm | 425 kV/in | |
Mykroy/Mycalex MM 561 Molding Grade Glass-bonded Mica Composite Synthetic mica filler. Does not burn. Good radiation resistance (3 x 10^10 Rads-Cobalt). ROHS CompliantThis ceramoplastic material is a versatile and efficient insulating material designed to meet.. |
|||
Dielectric Strength | 16.7 kV/mm | 425 kV/in | ASTM D149 |
Quantum Polysulfone Information provided by Quantum Advanced Engineering Plastics |
|||
Dielectric Strength | 16.7 - 25.0 kV/mm | 425 - 635 kV/in | Average value: 19.6 kV/mm Grade Count:7 |
Overview of materials for Polystyrene, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Glass Filled". Each property range of values reported is minimum and maximum values of appr.. |
|||
Dielectric Strength | 16.7 kV/mm | 425 kV/in | Short Term; ASTM D149 |
Quadrant EPP Quadrant LSG PSU, Extruded, Unfilled, Polysulfone (ASTM Product Data Sheet) |
|||
Dielectric Strength | 16.7 kV/mm @Thickness 1.57 mm |
425 kV/in @Thickness 0.0620 in |
Short time under oil; ASTM-D149 |
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (DAM) Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce.. |
|||
Dielectric Strength | 16.7 kV/mm @Thickness 1.59 mm |
425 kV/in @Thickness 0.0625 in |
Perpendicular, Short Time in Oil; ASTM D149 |
Haysite EMD Polyester, Glass Reinforced EMD is a glass mat reinforced polyester sheet designed primarily as a "slot wedge" material in large motors and generators. EMD has low weight loss at elevated temperatures and high flexural and sh.. |
|||
Dielectric Strength | 16.7 kV/mm | 425 kV/in | ASTM D149 |
Styron EMERGEâ„¢ 4610-10 Polycarbonate EMERGEâ„¢ PC 4610-10 advanced resin is formulated to deliver both outstanding clarity and enhanced ignition resistance while maintaining excellent physical properties and processability. Applica.. |
|||
Dielectric Strength | 16.7 kV/mm | 425 kV/in | ASTM D149 |
Styron EMERGEâ„¢ 4630-10 Polycarbonate EMERGEâ„¢ PC 4630-10 advanced resin is formulated to supply both excellent ultraviolet stability and enhanced ignition resistance while maintaining excellent physical properties and processabilit.. |
|||
Dielectric Strength | 16.7 kV/mm | 425 kV/in | ASTM D149 |
Styron EMERGEâ„¢ 4600-10 Polycarbonate EMERGEâ„¢ PC 4600-10 advanced resin is formulated to supply both clarity and enhanced ignition resistance while maintaining excellent physical properties. Applications: Information Technology E.. |
|||
Dielectric Strength | 16.7 kV/mm | 425 kV/in | |
Tra-Con Tra-Bond 5126 Medium Viscosity Aerospace-Grade Epoxy Adhesive TRA-BOND 5126 AEROSPACE-GRADE EPOXY ADHESIVE is a two-part, clear (amber), medium viscosity, aerospace-grade epoxy adhesive system recommended for bonding a wide variety of materials for structural .. |
|||
Dielectric Strength | 16.7 kV/mm | 425 kV/in | |
Tra-Con Tra-Cast 3101 Encapsulating Adhesive System TRA-CAST 3101 is an easy-to-use, room temperature cure, rigid, low viscosity, 100% solids (no solvents) epoxy resin and hardener system with excellent mechanical and electrical properties. It is rec.. |
|||
Dielectric Strength | 16.7 kV/mm | 425 kV/in | |
Trelleborg Emerson & Cuming Stycast® 1497 Two-Component Easy Mix Ratio Encapsulant Features and Typical ApplicationsPrimarily designed for ease of use in either meter mix or manual dispense operations. These products also offer a wide range of features including heat dissipation, .. |
|||
Dielectric Strength | 16.7 kV/mm | 425 kV/in | |
Trelleborg Emerson & Cuming Stycast® 2057FR/11 Two-Component Epoxy Flame Retardant Encapsulant Features and Typical ApplicationsProvide flame resistance down to 1/8 of an inch. These products also offer various other features such as thermal shock protection, low viscosity, and thermal conduc.. |
|||
Dielectric Strength | 16.7 kV/mm | 425 kV/in | ASTM D149 |
Ensinger TECASON™ S Polysulfone (PSU) TECASON™ S is a transparent engineering plastic known for its chemical resistance, rigidity, high-temperature performance, and its ability to operate in an autoclave environment. TECASON™ S is FD.. |
|||
Dielectric Strength | 16.7 kV/mm | 425 kV/in | ASTM D149 |
Arlon 55576R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Side 2: Uncured Silicone Rubber Interleave: LDPE This data represents typical values for the production material. T.. |
|||
Dielectric Strength | 16.7 kV/mm | 425 kV/in | ASTM D149 |
Arlon 55586R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave: PolyethyleneAppearance: Red silicone gum and rubber on fiberglass clothTh.. |
|||
Dielectric Strength | 16.7 kV/mm | 425 kV/in | Short Time |
Bulk Molding Compounds BMC 810 General Purpose Molding Compound BMC 810 is a general purpose, very high strength compound suitable for compression, transfer and stuffer injection molding. It is characterized by excellent flow and controlled reactivity and is wel.. |
|||
Dielectric Strength | 16.7 kV/mm | 425 kV/in | ASTM D149 |
Arlon R37879X034 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Layer 2: uncured silicone rubber; Layer 1: Cured silicone rubber; Substrate: 162 fiberglass |
|||
Dielectric Strength | 16.7 - 46.0 kV/mm | 425 - 1170 kV/in | Average value: 23.3 kV/mm Grade Count:5 |
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc.. |
|||
Dielectric Strength | 16.7 kV/mm | 425 kV/in | Short Term; ASTM D149 |
Quadrant EPP Quadrant PSU Estruded Unfilled Polysulfone (ASTM Product Data Sheet) |
|||
Dielectric Strength | 16.7 kV/mm | 425 kV/in | ASTM D149 |
Loctite® 5071 Silicone Encapsulant Conformal CoatingsConformal coatings are thin dielectric coatings that extend the longevity of circuit boards by protecting components and traces from corrosion, shorts, and mechanical damage. Locti.. |