Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 27.6 kV/mm | 700 kV/in | ASTM D149 |
Ravago Manufacturing Americas Hylon® N2000THL Nylon 6 (DAM) Information provided by Ravago. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | ASTM D149 |
Ravago Manufacturing Americas Hylon® N2033HL Nylon 6 (DAM) Information provided by Ravago. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | Short Term; ASTM D149 |
Quadrant EPP Duratron® PAI T5530 Compression Molded Glass Reinforced Polyamide-imide (ASTM Product Data Sheet) |
|||
Dielectric Strength | 27.6 kV/mm @Thickness 1.57 mm |
700 kV/in @Thickness 0.0620 in |
Cond A; ASTM D229 S.T. |
Industrial Laminates/Norplex NP615 Paper Base Laminate Description: Room temperature punching and shearing grade up to .125" thick. More flexible and lower mechanical properties than NP611. NP615 is produced with high resin content melamine impregnated .. |
|||
Dielectric Strength | 27.6 kV/mm @Thickness 1.57 mm |
700 kV/in @Thickness 0.0620 in |
Cond A; ASTM D229 S.T. |
Industrial Laminates/Norplex NP612 Paper Base Laminate Description: Room temperature punching and shearing grade up to .125" thick. More flexible and lower mechanical properties than NP611. Intended for applications where electrical and moisture require.. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill FR® PBT/ABS FR Availability: North AmericaForms: PelletsFeatures: Flame RetardantProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA4/6 GF30 HS BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedUL File Number: E157318Appearance: Bla.. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA4/6 GF50 HS BK 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: BlackUL File Number: E1573.. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA4/6 M/GF 20 HS 20% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 50% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | ASTM D-149 |
Saint-Gobain Norton® T-100 Virgin Skived PTFE Sheet (0.062" thick) T-100/T-200 Features/Benefits: Outstanding heat and chemical resistance; High dielectric strength; Anti-stick properties; Can be chemically etched for bondability; Applications include laminate rele.. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Plastiblend® PC/PET IM 1016 UV Availability: North AmericaForms: PelletsAdditive: Impact Modifier and UV StabilizerFeatures: Impact ModifiedInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA4/6 GF5 IM HS BK 5% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 5% Filler by WeightAdditive: Heat Stabilizer and Impact ModifierFeatures: Heat Stabilized and Impact Modifie.. |
|||
Dielectric Strength | >= 27.6 kV/mm | >= 700 kV/in | At 20 mils; ASTM D3755 |
Borealis Borcell™ HE1102 High Density Polyethylene Compound for Gas Injection of Cellular Communication Cable Insulation Borcell HE1102 is a high density polyethylene. A nucleating agent is incorporated for a uniform and closed cell structure. The components in the formulation are selected to give the lowest possibl.. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | In Oil; ASTM D149 |
Ensinger TECAPEI® 10% Glass Reinforced, made from Ultem® 2100 PEI TECAPEI™ is an amorphous thermoplastic polyetherimide (PEI) made from Sabic Innovative Plastics' Ultem® 1000 and 2000 series resins. The unreinforced 1000 series materials are translucent amber in.. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | ASTM D149 |
Arlon 28751R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1528 FiberglassSide 2: Uncured Silicone RubberInterleave 2: PolyethyleneAppearance: Red silicone gum o.. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | ASTM D149 |
Arlon 51141R015 Silicone Rubber/Fiberglass Laminate Interleave 1: 3 mil PE; Side 1: uncured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave 2: 3 mil PE |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | ASTM D149 |
Arlon 51866R015E 0.0150" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production material .. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | ASTM D149 |
Arlon 51106R020 Silicone Rubber/Fiberglass Laminate Side 1: cured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | ASTM D149 |
Arlon 51273R020 0.020" (0.508 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberInterleave: Polyethylene This data represents typical values for the production materia.. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | ASTM D149 |
Arlon 51276R020 Silicone Rubber/Fiberglass Laminate Side 1: cured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | |
Arlon 51279R020 0.020" (0.508 mm) Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass This data represents typical values for the production ma.. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | |
3M EPS-300 Heat Shrink Tubing 3M Heat Shrink tubing EPS-300 is a 3:1 thin-wall, flexible tubing offering the advantages of integral, adhesive-lined construction. The tubing is made from flame-retardant, flexible polyolefin with .. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | |
3M EPS-400 Heat Shrink Tubing 3M Heat Shrink tubing EPS-400 is a medium-wall, semi-rigid tubing offering the advantages of integral, adhesive-lined construction. The tubing is made from flame-retardant, flexible polyolefin with .. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | |
3M Scotch-Weld™ DP 3501 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP 3501 is a rapid room temperature curing, two-part epoxy adhesives for use in bonding many metals, wood, and a variety of plastics. Equal parts by volume are easi.. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | ASTM D149 |
Arlon R3792-920-10R##-P0 Silicone Rubber This self-fusible silicone tape is specially formulated to yield improved flexibility, elongation and elastic recovery at low operating temperature (-70°C to -100°C) where standard fusible silicon.. |
|||
Dielectric Strength | 27.6 kV/mm | 700 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA4/6 GF5 HS 5% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 5% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedInformation provided by TP Composites, .. |