Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 8.50 kV/mm @Temperature 23.0 °C |
216 kV/in @Temperature 73.4 °F |
Method A (Short-Time); ASTM D149 |
PolyOne LubriOne™ NN-30GF/10T WHT Polyamide 66 (Nylon 66) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Dielectric Strength | 8.50 - 16.7 kV/mm | 216 - 424 kV/in | Average value: 12.0 kV/mm Grade Count:30 |
Overview of materials for Phenolic, Novolac, Woodflour Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Woodflour Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Dielectric Strength | 8.50 kV/mm | 216 kV/in | Step by Step; ASTM D149 |
Plenco 00755 Melamine-Phenolic, Granular, Compression Molded PLENCO 00755 is a melamine-phenolic copolymer molding compound offering excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 00755.. |
|||
Dielectric Strength | 8.50 kV/mm | 216 kV/in | Short Time; ASTM D149 |
Plenco 2000 Phenolic, Granular, Injection Molded PLENCO 02000 is a versatile general purpose, organic filled phenolic molding compound, offering optimum cure characteristics and an excellent balance of molding properties. UL recognized under compo.. |
|||
Dielectric Strength | 8.50 kV/mm | 216 kV/in | Step by Step; ASTM D149 |
Plenco 3509 Phenolic, Granular, Injection Molded PLENCO 03509 is a mineral and flock filled phenolic molding compound offering excellent electrical properties, dimensional stability, and improved heat resistance. UL recognized under component file.. |
|||
Dielectric Strength | 8.50 kV/mm | 216 kV/in | ASTM D149 |
Tipco Tipcolite® THD 321 Phenolic Compound, Wood Flour & Cellulose, having Soft Flow & High Strength Soft Flow Phenolic Compound, Reinforced with Wood Flour & CelluloseApplications: Switchgear, HRC FusesProcessing: Compression & TransferInformation provided by the Manufacturer, Tipco Industries Lt.. |
|||
Dielectric Strength | 8.50 kV/mm | 216 kV/in | ASTM D149 |
Tipco Tipcolite® TX 311 Phenolic Compound, Wood Flour & Minerals, having Soft Flow & High Strength Soft Flow Phenolic Compound, Reinforced with Wood Flour & MineralsApplications: Switchgear, HRC FusesProcessing: Injection MouldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
I.. |
|||
Dielectric Strength | 8.50 - 10.0 kV/mm @Temperature 90.0 °C |
216 - 254 kV/in @Temperature 194 °F |
IS 2584-1963 |
Amity Thermosets ATO 1510 Phenolic Molding Glass fiber Filler, Compression Molded Characteristics:Shock resistantElectrical low lossHigh mechanical strengthHeat stableHigh electrical insulationDimensional stabilityGood mechanical tension bearing strengthMedium copper adhesionColo.. |