Material Notes:
3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and adhesion to metal, fiberglass, aluminum, wood (plywood, OSB, etc.), concrete and masonry. It is a two component 1:1 by volume system with adhesion enhancement chemical complexes. The protective coating can be applied up to 500mil thick and offers an ultra-fast cure that speeds production in an OEM setting. This aromatic formulation displays excellent chemical and environmental resistance while reducing the moisture problem that causes bubbling. It also offers high elongation and flexibility the produces high impact resistance.Information provided by 3M
Physical Properties Metric English Comments
Density 1.01 - 1.08 g/cc
0.0365 - 0.0390 lb/in³
Solids Content 100 %
100 %
Water Absorption <= 1.78 %
<= 1.78 %
ASTM D570
Brookfield Viscosity 150 - 1250 cP
150 - 1250 cP
RVT Model, Spindle #3 @ 20 rpm
Mechanical Properties Metric English Comments
Hardness, Shore D 54 - 60
54 - 60
ASTM D2240
Tensile Strength at Break 12.4 - 15.2 MPa
1800 - 2200 psi
ASTM 638-01
Elongation at Break 93 %
93 %
ASTM 638-01
Tear Strength 49.9 - 58.6 kN/m
285 - 335 pli
ASTM D624
Taber Abrasion, mg/1000 Cycles 35 - 40
35 - 40
ASTM D40695
Tangent Modulus 110 - 124 MPa
16000 - 18000 psi
Tangent; ASTM 638-01
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.0 °C
199 °F
Minimum Service Temperature, Air -29.0 °C
-20.2 °F
Flash Point 93.0 °C
199 °F
Processing Properties Metric English Comments
Cure Time 60.0 - 120 min
1.00 - 2.00 hour
light use
1440 min
24.0 hour
heavy duty use
Shelf Life 12.0 Month

@Temperature 21.0 - 32.0 °C
12.0 Month

@Temperature 69.8 - 89.6 °F
Users viewing this material also viewed the following: