3M Scotch-Weld™ DP-100NS Epoxy Adhesive

Category Polymer , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer 3M
Trade Name Scotch-Weld™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch-Weld™ DP-100NS Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Scotch-Weld™ Epoxy Adhesive DP-100NS is a two-part adhesives offering fast cure and machinability.Information provided by 3M
Physical Properties Metric English Comments
Brookfield Viscosity 50000 - 85000 cP
50000 - 85000 cP
Accelerator, RVF #6 spindle, 20 rpm @ 27°C
90000 - 150000 cP
90000 - 150000 cP
Base, RVF #6 spindle, 20 rpm @ 27°C
Mechanical Properties Metric English Comments
Hardness, Shore D 80 - 85
80 - 85
ASTM D2240
Thermal Properties Metric English Comments
CTE, linear 29.0 µm/m-°C

@Temperature -50.0 - 30.0 °C
16.1 µin/in-°F

@Temperature -58.0 - 86.0 °F
149 µm/m-°C

@Temperature 50.0 - 110 °C
82.8 µin/in-°F

@Temperature 122 - 230 °F
Thermal Conductivity 0.183 W/m-K

@Temperature 45.0 °C
1.27 BTU-in/hr-ft²-°F

@Temperature 113 °F
Glass Transition Temp, Tg 34.0 °C
93.2 °F
Electrical Properties Metric English Comments
Volume Resistivity 2.20e+14 ohm-cm
2.20e+14 ohm-cm
ASTM D257
Dielectric Strength 43.3 kV/mm
1100 kV/in
ASTM D257
Processing Properties Metric English Comments
Cure Time 1440 - 2880 min
24.0 - 48.0 hour
Descriptive Properties Value Comments
Appearance Translucent