Material Notes:
3M TMW Tubing is a semi-rigid translucent heat-shrinkable polyolefin tubing that is co-extruded and selectively cross-linked with an integral, meltable inner wall. When heated in excess of 135°C the adhesive inner wall of the tubing is softened and forced by the shrinking action of the outer wall into contact with all underlying surfaces and small voids. The adhesive forms a flexible bond with a wide variety of rubber, plastics and metals. Upon cooling, 3M TMW tubing provides a tough, protective and insulating barrier, highly resistant to penetration by moisture, chemicals and solvents. #M TMW tubing is rated for continuous operation at temperatures fro -55°C to 110°C and will withstand higher operating temperatures for brief periods. Adhesive reflow will occur at temperatures above 80°C.Information provided by 3M
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
Water Absorption 0.10 %
0.10 %
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 4.14 MPa
>= 600 psi
Gasoline Resistance
6.89 MPa
999 psi
Solvent Resistance
17.2 MPa
2490 psi
Elongation at Break 400 %
400 %
175 %

@Temperature 175 °C,
Time 1.21e+6 sec
175 %

@Temperature 347 °F,
Time 336 hour
Heat Aged
2% Secant Modulus 0.221 GPa
32.0 ksi
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
Dielectric Strength 15.7 kV/mm
400 kV/in
Solvent Resistance
23.6 kV/mm
600 kV/in
Fluid Resistance
35.4 kV/mm
900 kV/in