Material Notes:
DescriptionPolypropylene PP 3487-01 is a special homopolymer polypropylene formulated with a long term heat aging resistance. This material has excellent resistance to chemicals and solvents. High performance in both wet and dry environments. ApplicationTypical applications of PP 3487-01 include large appliance and automotive parts. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Melt Flow 4.0 g/10 min
4.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ASTM D785
Tensile Strength, Yield 33.8 MPa
4900 psi
ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Flexural Modulus 1.45 GPa
210 ksi
ASTM D790
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
203 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 160 °C
320 °F