Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ACC EP AEP EPI Engineered Polymers

Category Polymer , Thermoset , Epoxy
Manufacturer Amber Chemical Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ACC EP AEP EPI Engineered Polymers.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EP AEP is a new generation of Internetwork Polymers of polyurea and Epoxy, “Powered by Reactamine® Technology”. EP AEP was developed for a colorfast floor for both residential and industrial applications. Gel times are fast, around 15 minutes, and a tack free floor can be as fast as 45 minutes. A Broadcast or Trowl down floor can be easily made using EP AEP. EP AEP requires no primer and acts as its own top coat. EP AEP meet USDA and FDA indirect food contact. EP AEP is also available in antimicrobial formulas. Applications AIRCRAFT HANGAR FLOORS LOW TEMPERATURE FREEZERS MAINTENANCE FACILITIES FLOORS REQUIRING UV STABILITY UV-STABLE TOP COAT INDUSTRIAL SHOP FLOORS NON-CONDUCTIVE FLOORING FOOD PROCESSING FACILITIESPart of the Amber Chemical Group. Data provided by manufacturer.
Physical Properties Metric English Comments
Viscosity 1100 cP

@Temperature 75.0 °C
1100 cP

@Temperature 167 °F
A Side
1575 cP

@Temperature 75.0 °C
1575 cP

@Temperature 167 °F
B Side
Mechanical Properties Metric English Comments
Hardness, Shore D 45
45
ASTM 2240
Tensile Strength, Yield 24.8 MPa
3590 psi
ASTM D412
Elongation at Break 200 %
200 %
ASTM D412
Adhesive Bond Strength >= 1.72 MPa
>= 250 psi
Wood (no primer), Delamination; ASTM D4541 Elcometer
>= 2.07 MPa
>= 300 psi
Concrete (no primer) Concrete Failure; ASTM D4541 Elcometer
>= 2.07 MPa
>= 300 psi
Concrete (primer), Concrete Failure; ASTM D4541 Elcometer
>= 2.07 MPa
>= 300 psi
Concrete (epoxy), Concrete Failure; ASTM D4541 Elcometer
>= 6.21 MPa
>= 900 psi
Steel (no primer), Substrate Failure; ASTM D4541 Elcometer
>= 10.3 MPa
>= 1500 psi
Steel (epoxy primer), Primer Failure; ASTM D4541 Elcometer
Tear Strength 78.9 kN/m
450 pli
ASTM D412
Taber Abrasion, mg/1000 Cycles 45
45
CS17 WHEEL, 1kg per 1000 cycles; ASTM D4060
Thermal Properties Metric English Comments
Flash Point >= 93.3 °C
>= 200 °F
ASTM Pensky-Martin
Processing Properties Metric English Comments
Cure Time >= 45.0 min
>= 0.750 hour
Tack Free Time
Pot Life 15 min
15 min
Descriptive Properties Value Comments
Color All primary colors.
Flexibility Pass
ASTM D1737, 1/8"Mandrel
Resistance to 1,1,1-Trichlorethane Conditional
Resistance to Acetic Acid (100%) Conditional
Resistance to Acetone Conditional
Resistance to Ammonium Hydroxide (50%) Recommended Conditional
Resistance to Benzene Conditional
Resistance to Brine-Saturated H2O Recommended
Resistance to Brine-Saturated H<sub>2</sub>O (310g/l)
Resistance to Chlorinated H2O Recommended
Resistance to Clorox® (10%) H2O Recommended
Resistance to Diesel Fuel Recommended Conditional
Resistance to Gasoline Recommended Conditional
Resistance to Gasoline/ 5% Methanol Recommended Conditional
Resistance to Gasoline/5% MTBE Recommended Conditional
Resistance to H2O Recommended
Resistance to H2O (14 days at 82°C) Recommended Conditional
Resistance to Hydraulic Fluid (oil) Recommended Conditional
Resistance to Hydrochloric Acid (20%) Recommended
Resistance to Hydrofluoric Acid(10%) Not Recommended
Resistance to Isopropyl Alcohol Recommended
Resistance to Lactic Acid Recommended Conditional
Resistance to MEK Recommended Conditional
Resistance to Methanol Recommended
Resistance to Methylene chloride Conditional
Resistance to Mineral Spirits Recommended Conditional
Resistance to Motor Oil Recommended
Resistance to MTEB Conditional
Resistance to Muriatic Acid (10%) Recommended
Resistance to NaCl/H2O (10%) Recommended
Resistance to Nitric Acid (20%) Not Recommended
Resistance to Phosphoric Acid (10%) Recommended
Resistance to Phosphoric Acid (50%) Not Recommended
Resistance to Potassium Hydroxide (10%) Recommended
Resistance to Potassium Hydroxide (20%) Recommended, Discoloration
Resistance to Propylene Carbonate Recommended Conditional
Resistance to Skydrol® Conditional
Resistance to Sodium Bicarbonate Recommended
Resistance to Sodium Hydroxide (25%) Recommended
Resistance to Sodium Hydroxide (50%) Recommended, Discoloration
Resistance to Sodium Hypochlorite (10%) Recommended
Resistance to Stearic Acid Recommended
Resistance to Sugar/H2O Recommended
Resistance to Sulfuric Acid (>50%) Recommended Conditional
Resistance to Sulfuric Acid (10%) Recommended
Resistance to Toluene Recommended
Resistance to Trisodium Phosphate Recommended
Resistance to Vinegar/ H2O (5%) Recommended
Resistance to Xylene Recommended Conditional
Users viewing this material also viewed the following: