ACC EP RAP-1567 EPI Engineered Polymers Aliphatic Polyurea

Category Polymer , Thermoset
Manufacturer Amber Chemical Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ACC EP RAP-1567 EPI Engineered Polymers Aliphatic Polyurea.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
RAP-1567 HX is a two component 100% solids, no VOC’s, aliphatic polyureas “Powered by ReactAmine® Technology” that was developed for UV stable (colorfast) polyurea applications. This new generation polyurea displays fast cure times and excellent adhesion characteristics. RAP-1567 HX is designed to be quick gelling (30 minutes) in order to optimize leveling and wetting properties. RAP-1567 HX can be spray applied at temperatures ranging from 20ºF to 120ºF. This 100% polyurea elastomer displays excellent chemical resistance, water insensitivity and UV resistance (in any color) at a wide range of temperatures. RAP-1567 HX will provide a smooth glossy finish when fully cured. RAP-1567 HX emits virtually no odors and can be applied indoors without any VOC’s. RAP-1567 HX meets USDA and FDA specifications. RAP-1567 HX can be rolled, brushed, or spray applied thru airless or plural equipment.Part of the Amber Chemical Group. Data provided by manufacturer.
Physical Properties Metric English Comments
Viscosity 200 cP
200 cP
A Side
550 cP
550 cP
B Side
Mechanical Properties Metric English Comments
Hardness, Shore D 42
42
ASTM 2240
Tensile Strength, Yield 15.9 MPa
2300 psi
ASTM D412
Elongation at Break 300 %
300 %
ASTM D412
Adhesive Bond Strength >= 1.72 MPa
>= 250 psi
Wood (no primer), Delamination; ASTM D4541 Elcometer
>= 2.07 MPa
>= 300 psi
Concrete (primer), Concrete Failure; ASTM D4541 Elcometer
>= 2.07 MPa
>= 300 psi
Concrete (epoxy), Concrete Failure; ASTM D4541 Elcometer
>= 2.07 MPa
>= 300 psi
Concrete (no primer), Concrete Failure; ASTM D4541 Elcometer
>= 6.21 MPa
>= 900 psi
Steel (no primer), Substrate Failure; ASTM D4541 Elcometer
>= 10.3 MPa
>= 1500 psi
Steel (epoxy primer), Primer Failure; ASTM D4541 Elcometer
Tear Strength 53.5 kN/m
305 pli
ASTM D412
Taber Abrasion, mg/1000 Cycles 40
40
CS17 WHEEL, 1kg per 1000 cycles; ASTM D4060
Thermal Properties Metric English Comments
Flash Point >= 93.3 °C
>= 200 °F
ASTM Pensky-Martin
Processing Properties Metric English Comments
Cure Time >= 30.0 min

@Temperature 75.0 °C
>= 0.500 hour

@Temperature 167 °F
tack free
Pot Life 40.0 min

@Temperature 75.0 °C
40.0 min

@Temperature 167 °F
Descriptive Properties Value Comments
Color All primary colors.
Flexibility Pass
ASTM D1737, 1/8"Mandrel
Resistance to 1,1,1-Trichlorethane Conditional
Resistance to Acetic Acid (100%) Conditional
Resistance to Acetone Conditional
Resistance to Ammonium Hydroxide (50%) Recommended Conditional
Resistance to Benzene Conditional
Resistance to Brine-Saturated H2O Recommended
Resistance to Brine-Saturated H<sub>2</sub>O (310g/l)
Resistance to Chlorinated H2O Recommended
Resistance to Clorox® (10%) H2O Recommended
Resistance to Diesel Fuel Recommended Conditional
Resistance to Gasoline Recommended Conditional
Resistance to Gasoline/ 5% Methanol Recommended Conditional
Resistance to Gasoline/5% MTBE Recommended Conditional
Resistance to H2O Recommended
Resistance to H2O (14 days at 82°C) Recommended Conditional
Resistance to Hydraulic Fluid (oil) Recommended Conditional
Resistance to Hydrochloric Acid (20%) Recommended
Resistance to Hydrofluoric Acid(10%) Not Recommended
Resistance to Isopropyl Alcohol Recommended
Resistance to Lactic Acid Recommended Conditional
Resistance to MEK Recommended Conditional
Resistance to Methanol Recommended
Resistance to Methylene chloride Conditional
Resistance to Mineral Spirits Recommended Conditional
Resistance to Motor Oil Recommended
Resistance to MTEB Conditional
Resistance to Muriatic Acid (10%) Recommended
Resistance to NaCl/H2O (10%) Recommended
Resistance to Nitric Acid (20%) Not Recommended
Resistance to Phosphoric Acid (10%) Recommended
Resistance to Phosphoric Acid (50%) Not Recommended
Resistance to Potassium Hydroxide (10%) Recommended
Resistance to Potassium Hydroxide (20%) Recommended, Discoloration
Resistance to Propylene Carbonate Recommended Conditional
Resistance to Skydrol® Conditional
Resistance to Sodium Bicarbonate Recommended
Resistance to Sodium Hydroxide (25%) Recommended
Resistance to Sodium Hydroxide (50%) Recommended, Discoloration
Resistance to Sodium Hypochlorite (10%) Recommended
Resistance to Stearic Acid Recommended
Resistance to Sugar/H2O Recommended
Resistance to Sulfuric Acid (>50%) Recommended Conditional
Resistance to Sulfuric Acid (10%) Recommended
Resistance to Toluene Recommended
Resistance to Trisodium Phosphate Recommended
Resistance to Vinegar/ H2O (5%) Recommended
Resistance to Xylene Recommended Conditional