ACC QGel 315 QSI Quantum Silicones General Purpose Silicone Gel

Category Polymer , Thermoset , Silicone
Manufacturer Amber Chemical Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ACC QGel 315 QSI Quantum Silicones General Purpose Silicone Gel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
QGel 315 is a clear, very soft, tough moderately cross-linked silicone polymer. Silicone gels are used to provide protection from vibration and thermal or mechanical shock. Silicone gels also provide excellent moisture protection. Key Features: 24 hour room temperature cure One to one mix ratio Soft but resilient Heat cure requiredPart of the Amber Chemical Group. Data provided by manufacturer.
Physical Properties Metric English Comments
Specific Gravity 0.970 g/cc
0.970 g/cc
"B" component
0.970 g/cc
0.970 g/cc
"A" component
Viscosity 1000 cP
1000 cP
"B" component
1000 cP
1000 cP
"A" component
Storage Temperature <= 38.0 °C
<= 100 °F
12 months
Mechanical Properties Metric English Comments
Penetration 5.0 - 9.0
5.0 - 9.0
mm, 30 mins @ 150°C
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Processing Properties Metric English Comments
Cure Time 15.0 - 30.0 min

@Temperature 150 °C
0.250 - 0.500 hour

@Temperature 302 °F
45.0 - 60.0 min

@Temperature 100 °C
0.750 - 1.00 hour

@Temperature 212 °F
120 - 240 min

@Temperature 25.0 °C
2.00 - 4.00 hour

@Temperature 77.0 °F
Gel Time >= 1440 min
>= 1440 min
Descriptive Properties Value Comments
Color Transparent
"A" component
Transparent
"B" component