Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ACC QM 100 QSI Quantum Silicones Clear 30 Durometer Condensation Cure Material

Category Polymer , Thermoset , Silicone
Manufacturer Amber Chemical Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ACC QM 100 QSI Quantum Silicones Clear 30 Durometer Condensation Cure Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
QM 100 is a two component, room temperature condensation cure silicone material. The cured rubber is a crystal clear material designed specifically for the special effects market. The materials' clarity allows for its' use as fake ice, fake glass or any application where clarity is required. Key Features:Low ViscosityClarityFast demold time Clear, pigment ableApplications: Special effects Fake ice Fake glass Applications where pigment is required. Part of the Amber Chemical Group. Data provided by manufacturer.
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
Uncatalyst QM CAT 100
0.970 g/cc
0.970 g/cc
Uncatalyst QM 100
Viscosity 20 cP
20 cP
Uncatalyst QM CAT 100
600 cP
600 cP
Uncatalyst QM 100
Linear Mold Shrinkage <= 0.0030 cm/cm

@Temperature 25.0 °C,
Time 259000 sec
<= 0.0030 in/in

@Temperature 77.0 °F,
Time 72.0 hour
Cured
Storage Temperature <= 38.0 °C
<= 100 °F
6 months
Mechanical Properties Metric English Comments
Hardness, Shore A 30

@Temperature 25.0 °C,
Time 259000 sec
30

@Temperature 77.0 °F,
Time 72.0 hour
Cured
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Processing Properties Metric English Comments
Dry Time 4 - 6 hour
4 - 6 hour
Demold time, catalyzed
Pot Life >= 35 min
>= 35 min
Snap Time, catalyzed
Descriptive Properties Value Comments
Color Clear
Unccatalyzed, QM 100
Clear
Unccatalyzed, QM CAT 100
Copyright © lookpolymers.com All Rights Reserved